# US 2020/0403143 A1 · Minimal Thickness, Low Switching Voltage Magnetic Free Layers Using an Oxidation Control Layer and Magnetic Moment Tuning Layer for Spintronic Applications

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0403143 A1
- Document ID: US20200403143A1
- Status: Published application
- Kind: A1
- Application number: 16/448,362
- Filed: 2019-06-21
- Published: 2020-12-24
- Earliest claimed: 2019-06-21
- Assignees: Headway Technologies, Inc.
- Applicants: Headway Technologies, Inc.
- Inventors: Jodi Mari Iwata; Guenole Jan; Santiago Serrano Guisan; Luc Thomas; Ru-Ying Tong
- Web page: https://patentgrep.com/patent/US20200403143A1

## CPC

- H10N 50/80: Constructional details
- H01F 10/3254: {the spacer being semiconducting or insulating, e.g. for spin tunnel junction [STJ]}
- H01F 10/3268: {the exchange coupling being asymmetric, e.g. by use of additional pinning, by using antiferromagnetic or ferromagnetic coupling interface, i.e. so-called spin-valve [SV] structure, e.g. NiFe/Cu/NiFe/FeMn}
- H01F 10/329: {Spin-exchange coupled multilayers wherein the magnetisation of the free layer is switched by a spin-polarised current, e.g. spin torque effect}
- H01F 41/303: {with exchange coupling adjustment of magnetic film pairs, e.g. interface modifications by reduction, oxidation}
- H10B 61/00: Magnetic memory devices, e.g. magnetoresistive RAM [MRAM] devices
- H10N 50/01: Manufacture or treatment
- H10N 50/10: Magnetoresistive devices
- H10N 50/85: Materials of the active region
- H10N 52/00: Hall-effect devices (integrated devices or assemblies of multiple devices H10N59/00)
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

A perpendicular magnetic tunnel junction is disclosed wherein first and second interfaces of a free layer (FL) with a first metal oxide (Hk enhancing layer) and second metal oxide (tunnel barrier), respectively, produce perpendicular magnetic anisotropy (PMA) to provide thermal stability to 400° C. Insertion of an oxidation control layer (OCL) such as Mg and a magnetic moment tuning layer (MMTL) like Mo or W enables FL thickness to be reduced below 10 Angstroms while providing sufficient PMA for a switching voltage substantially less than 500 mV at a 10 ns pulse width and 1 ppm defect rate. Magnetoresistive ratio is ≥1, and resistance x area (RA) product is below 5 ohm-μm2. Embodiments are provided where MMTL and OCL materials interface with each other, or do not contact each other. Each of the MMTL and OCL materials may be deposited separately, or at least one is co-deposited with the FL.

## Claims

### Claim 1

A perpendicular magnetic tunnel junction (p-MTJ), comprising:
(a) a tunnel barrier layer that is a first metal oxide layer;
(b) a Hk enhancing layer that is a second metal oxide layer or a metal oxynitride layer;
(c) a free layer (FL) with a first surface that forms a first interface with the tunnel barrier layer, a second surface that forms a second interface with the Hk enhancing layer, and comprised of an oxidation control layer (OCL) material that getters oxygen and a magnetic moment tuning layer (MMTL) material where the OCL and MMTL materials form a third interface with each other; and
(d) a capping layer.

### Claim 2 (depends on 1)

The p-MTJ of claim 1 wherein the OCL material is one of Mg, a Mg alloy, Ba, or Ca, and has a thickness up to about 6 Angstroms.

### Claim 3 (depends on 1)

The p-MTJ of claim 1 wherein each of the OCL material and MMTL material form a continuous layer, a discontinuous layer, metal particles, or metal clusters.

### Claim 4 (depends on 1)

The p-MTJ of claim 1 wherein the MMTL material is one or more of Nb, Mo, W, Re, Zr, Ru, Rh, Os, Ir, Zn, Pt, Pd, Ga, and Ge, and has a thickness from 0.25 Angstrom to 1.0 Angstrom.

### Claim 5 (depends on 1)

The p-MTJ of claim 1 wherein the free layer is a single layer or a multilayer of one or more of Co, Fe, CoFe, CoFeB, CoB, FeB, CoFeNi, and CoFeNiB.

### Claim 6 (depends on 1)

The p-MTJ of claim 1 wherein the free layer is comprised of a high Ku material having inherent PMA, which is a Heusler alloy that is Ni2MnZ, Pd2MnZ, Co2MnZ, Fe2MnZ, Co2FeZ, Mn3Ge, or Mn2Ga where Z is one of Si, Ge, Al, Ga, In, Sn, and Sb, or an ordered L10 or L11 material with a composition that is one of MnAl, MnGa, or RT wherein R is Rh, Pd, Pt, Ir, or an alloy thereof, and T is Fe, Co, Ni, or an alloy thereof, or a rare-earth alloy with a TbFeCo, GdCoFe, FeNdB, or SmCo composition.

### Claim 7 (depends on 1)

The p-MTJ of claim 1 wherein the free layer has a first sub-layer (FL1) with a thickness t1 that forms the first interface, and a second sub-layer (FL2) with a thickness t2 that forms the second interface, and where a sum (t1+t2) is from 5 Angstroms to 12 Angstroms.

### Claim 8 (depends on 1)

The p-MTJ of claim 1 further comprising a seed layer formed on a substrate, and a pinned layer (PL) on the seed layer to yield a seed layer/PL/tunnel barrier layer/FL/Hk enhancing layer/capping layer configuration.

### Claim 9 (depends on 1)

The p-MTJ of claim 1 further comprising a seed layer formed on a substrate, and a pinned layer (PL) on the tunnel barrier layer to yield a seed layer/Hk enhancing layer/FL/tunnel barrier layer/PL/capping layer configuration.

### Claim 10 (depends on 1)

The p-MTJ of claim 1 wherein the Hk enhancing layer is a single layer or a laminate comprised of an oxide or oxynitride of one or more of Si, Sr, Ti, Ba, Ca, La, Al, Mn, V, and Hf, and has a resistance x area (RA) product less than a RA product of the tunnel barrier layer.

### Claim 11 (depends on 1)

The p-MTJ of claim 1 wherein the capping layer is comprised of a metal nitride (MN) or metal oxynitride (MON) where M is one or more of Ti, V, Cr, Zr, Nb, Mo, Hf, Ta, W, and Si.

### Claim 12 (depends on 7)

The p-MTJ of claim 7 wherein the OCL material and MMTL material form a stack of layers having an OCL1/MMTL/OCL2 configuration on the FL1 where the first OCL (OCL1) contacts a top surface of the FL1, and the second OCL (OCL2) adjoins a bottom surface of the FL2.

### Claim 13 (depends on 7)

The p-MTJ of claim 7 wherein the OCL material and MMTL material form a stack of layers having an OCL/MMTL or MMTL/OCL configuration on the FL1 where one of the OCL and MMTL materials contacts a top surface of the FL1, and the other of the OCL and MMTL materials adjoins a bottom surface of the FL2.

### Claim 14 (depends on 7)

The p-MTJ of claim 7 wherein the OCL material is formed within each of the FL1 and FL2, and the MMTL material is formed between the FL1 and FL2.

### Claim 15 (depends on 7)

The p-MTJ of claim 7 wherein both of the OCL and MMTL materials are formed within each of the FL1 and FL2, and the OCL material is also formed between the FL1 and FL2.

### Claim 16 (depends on 7)

The p-MTJ of claim 7 wherein the OCL material is formed between the FL1 and FL2, and the MMTL material is formed within each of the FL2 and the OCL material.

### Claim 17 (depends on 1)

The p-MTJ of claim 1 wherein the p-MTJ is incorporated in a magnetic random access memory (MRAM), spin transfer torque (STT)-MRAM, spin orbit torque (SOT)-MRAM, spin torque oscillator, Spin Hall Effect device, magnetic sensor, or a biosensor.

### Claim 18

A perpendicular magnetic tunnel junction (p-MTJ), comprising:
(a) a tunnel barrier layer that is a first metal oxide layer;
(b) a Hk enhancing layer that is a second metal oxide layer or a metal oxynitride layer;
(c) a free layer (FL) with a first surface that forms a first interface with the tunnel barrier layer, a second surface that forms a second interface with the Hk enhancing layer, and comprised of an oxidation control layer (OCL) material that getters oxygen, and a magnetic moment tuning layer (MMTL) material wherein the OCL and MMTL materials are separated by at least a portion of the FL; and
(d) a capping layer.

### Claim 19 (depends on 18)

The p-MTJ of claim 18 wherein the OCL material is one of Mg, a Mg alloy, Ba, or Ca, and has a thickness up to about 6 Angstroms.

### Claim 20 (depends on 18)

The p-MTJ of claim 18 wherein each of the OCL material and MMTL material form a continuous layer, a discontinuous layer, metal particles, or metal clusters.

### Claim 21 (depends on 18)

The p-MTJ of claim 18 wherein the MMTL material is one or more of Nb, Mo, Ta, W, Re, Ti, V, Cr, Zr, Hf, Ru, Rh, Os, Ir, Cu, Zn, Pt, Au, Ag, Pd, Al, B, Ga, Si, and Ge, and has a thickness from 0.25 Angstrom to 1.0 Angstrom.

### Claim 22 (depends on 18)

The p-MTJ of claim 18 wherein the free layer is a single layer or a multilayer of one or more of Co, Fe, CoFe, CoFeB, CoB, FeB, CoFeNi, and CoFeNiB.

### Claim 23 (depends on 18)

The p-MTJ of claim 18 wherein the free layer is comprised of a high Ku material having inherent PMA which is a Heusler alloy that is Ni2MnZ, Pd2MnZ, Co2MnZ, Fe2MnZ, Co2FeZ, Mn3Ge, or Mn2Ga where Z is one of Si, Ge, Al, Ga, In, Sn, and Sb, or an ordered L10 or L11 material with a composition that is one of MnAl, MnGa, or RT wherein R is Rh, Pd, Pt, Ir, or an alloy thereof, and T is Fe, Co, Ni, or an alloy thereof, or a rare-earth alloy with a TbFeCo, GdCoFe, FeNdB, or SmCo composition.

### Claim 24 (depends on 18)

The p-MTJ of claim 18 wherein the free layer has a first sub-layer (FL1) with a thickness t1 that forms the first interface, and a second sub-layer (FL2) with a thickness t2 that forms the second interface, and where a sum (t1+t2) is from 5 Angstroms to 12 Angstroms.

### Claim 25 (depends on 18)

The p-MTJ of claim 18 further comprising a seed layer formed on a substrate, and a pinned layer (PL) on the seed layer to yield a seed layer/PL/tunnel barrier layer/FL/Hk enhancing layer/capping layer configuration.

### Claim 26 (depends on 18)

The p-MTJ of claim 18 further comprising a seed layer formed on a substrate, and a pinned layer (PL) on the tunnel barrier layer to yield a seed layer/Hk enhancing layer/FL/tunnel barrier layer/PL/capping layer configuration.

### Claim 27 (depends on 18)

The p-MTJ of claim 18 wherein the Hk enhancing layer is a single layer or a laminate comprised of an oxide or oxynitride of one or more of Si, Sr, Ti, Ba, Ca, La, Al, Mn, V, and Hf, and has a resistance x area (RA) product less than a RA product of the tunnel barrier layer.

### Claim 28 (depends on 18)

The p-MTJ of claim 18 wherein the capping layer is comprised of a metal nitride (MN) or metal oxynitride (MON) where M is one or more of Ti, V, Cr, Zr, Nb, Mo, Hf, Ta, W, and Si.

### Claim 29 (depends on 24)

The p-MTJ of claim 24 wherein the FL2 has a first sub-layer (FL2a) with a thickness t21, and a second sub-layer (FL2b) having a thickness t22 that forms the second interface, and wherein the MMTL material is formed between the FL1 and FL2a, and the OCL material is formed between the FL2a and FL2b to give a FL1/MMTL/FL2a/OCL/FL2b configuration for the FL, and where a sum (t1+t21+t22) is from 5 to 12 Angstroms.

### Claim 30 (depends on 24)

The p-MTJ of claim 24 wherein the FL2 has a first sub-layer (FL2a) with a thickness t21, and a second sub-layer (FL2b) having a thickness t22 that forms the second interface, and wherein the OCL material is formed between the FL1 and FL2a, and the MMTL material is formed between the FL2a and FL2b to give a FL1/OCL/FL2a/MMTL/FL2b configuration for the FL, and where a sum (t1+t21+t22) is from 5 to 12 Angstroms.

### Claim 31 (depends on 24)

The p-MTJ of claim 24 wherein the FL1 has a first sub-layer (FL1a) with a thickness t11 that forms the first interface, and a second sub-layer (FL1b) having a thickness t12, and wherein the MMTL material is formed between the FL1b and FL2, and the OCL material is formed between the FL1a and FL1b to give a FL1a/OCL/FL1b/MMTL/FL2 configuration for the FL, and where a sum (t11+t12+t2) is from 5 to 12 Angstroms.

### Claim 32 (depends on 24)

The p-MTJ of claim 24 wherein the FL1 has a first sub-layer (FL1a) with a thickness t11 that forms the first interface, and a second sub-layer (FL1b) having a thickness t12, and wherein the OCL material is formed between the FL1b and FL2, and the MMTL material is formed between the FL1a and FL1b to give a FL1a/MMTL/FL1b/OCL/FL2 configuration for the FL, and where a sum (t11+t12+t2) is from 5 to 12 Angstroms.

### Claim 33 (depends on 18)

The p-MTJ of claim 18 wherein the p-MTJ is incorporated in a MRAM, STT-MRAM, SOT-MRAM, spin torque oscillator, Spin Hall Effect device, magnetic sensor, or a biosensor.

### Claim 34

A method of forming a perpendicular magnetic tunnel junction (p-MTJ) having a first interface between a free layer (FL) and a first oxide layer that is a tunnel barrier layer, and a second interface between the FL and a Hk enhancing layer that is a second metal oxide layer or a metal oxynitride layer, comprising:
(a) forming the FL on the tunnel barrier layer with a sputter deposition sequence, comprising;
(1) depositing a first FL sub-layer (FL1) on the tunnel barrier layer;
(2) depositing one of an oxidation control layer (OCL) material that getters oxygen, and a magnetic moment tuning layer (MMTL) material on the FL1;
(3) depositing the other of the OCL material and the MMTL material; and
(4) depositing an uppermost FL sub-layer on the other of the OCL material and the MMTL material;
(b) depositing a metal layer on the uppermost FL sub-layer; and
(c) performing an oxidation or oxynitridation of the metal layer to yield the Hk enhancing layer.

### Claim 35 (depends on 34)

The method of claim 34 wherein the FL1 has a thickness t1, and the uppermost FL sub-layer is FL2 with a thickness t2 where (t1+t2) is from about 5 to 12 Angstroms.

### Claim 36 (depends on 34)

The method of claim 34 wherein the Hk enhancing layer has a lower resistance x area (RA) product than a RA product of the tunnel barrier layer.

### Claim 37 (depends on 34)

The method of claim 34 wherein the free layer is a single layer or multilayer of one or more of Co, Fe, CoFe, CoFeB, CoB, FeB, CoFeNi, and CoFeNiB.

### Claim 38 (depends on 34)

The method of claim 34 wherein the free layer is comprised of a high Ku material having inherent PMA which is a Heusler alloy that is Ni2MnZ, Pd2MnZ, Co2MnZ, Fe2MnZ, Co2FeZ, Mn3Ge, or Mn2Ga where Z is one of Si, Ge, Al, Ga, In, Sn, and Sb, or an ordered L10 or L11 material with a composition that is one of MnAl, MnGa, or RT wherein R is Rh, Pd, Pt, Ir, or an alloy thereof, and T is Fe, Co, Ni or an alloy thereof, or a rare-earth alloy with a TbFeCo, GdCoFe, FeNdB, or SmCo composition.

### Claim 39 (depends on 34)

The method of claim 34 wherein the OCL material is one of Mg, a Mg alloy, Ba, or Ca.

### Claim 40 (depends on 34)

The method of claim 34 wherein each of the OCL material and MMTL material form a continuous layer, a discontinuous layer, metal particles, or metal clusters.

### Claim 41 (depends on 34)

The method of claim 34 wherein the MMTL material is one or more of Nb, Mo, W, Re, Zr, Ru, Rh, Os, Ir, Zn, Pt, Pd, Ga, and Ge.

### Claim 42 (depends on 35)

The method of claim 35 wherein the OCL material and then the MMTL material is deposited on the FL1, and further comprised of depositing a second OCL material on the MMTL material to give a FL1/OCL/MMTL/OCL/FL2 configuration for the FL.

### Claim 43 (depends on 34)

The method of claim 34 further comprised of depositing a second FL sub-layer that is FL1b on the one of the OCL material and the MMTL material before depositing the other of the OCL material and MMTL material, and wherein the uppermost FL sub-layer is FL2 to give a FL1/OCL/FL1b/MMTL/FL2 or FL1/MMTL/FL1b/OCL/FL2 configuration for the FL.

### Claim 44 (depends on 34)

The method of claim 34 further comprised of depositing a second FL sub-layer that is FL2a on the one of the OCL material and MMTL material before depositing the other of the OCL material and MMTL material, and wherein the uppermost FL sub-layer is FL2b to give a FL1/OCL/FL2a/MMTL/FL2b or FL1/MMTL/FL2a/OCL/FL2b configuration for the FL.

### Claim 45

A method of forming a perpendicular magnetic tunnel junction (p-MTJ) having a first interface between a free layer (FL) and a first oxide layer that is a tunnel barrier layer, and a second interface between the FL and a Hk enhancing layer that is a second metal oxide layer or a metal oxynitride layer, comprising:
(a) forming the FL on the tunnel barrier layer with a sputter deposition sequence, comprising;
(1) co-depositing an oxidation control layer (OCL) material that getters oxygen, and a first FL sub-layer (FL1) on the tunnel barrier layer;
(2) depositing a magnetic moment tuning layer (MMTL) material on the co-deposited FL1 and OCL material; and
(3) co-depositing the OCL material and a second FL sub-layer (FL2) on the MMTL material;
(b) depositing a metal layer on the co-deposited FL2 and OCL material; and
(c) performing an oxidation or oxynitridation of the metal layer to yield the Hk enhancing layer.

### Claim 46 (depends on 45)

The method of claim 45 wherein the OCL material is one of Mg, a Mg alloy, Ba, or Ca.

### Claim 47 (depends on 45)

The method of claim 45 wherein the OCL material forms metal particles or clusters within each of the FL1 and FL2, and wherein the MMTL material forms a continuous layer, a discontinuous layer, metal particles, or metal clusters.

### Claim 48 (depends on 45)

The method of claim 45 wherein the MMTL material is one or more of Nb, Mo, W, Re, Zr, Ru, Rh, Os, Ir, Zn, Pt, Pd, Ga, and Ge.

### Claim 49

A method of forming a perpendicular magnetic tunnel junction (p-MTJ) having a first interface between a free layer (FL) and a first oxide layer that is a tunnel barrier layer, and a second interface between the FL and a Hk enhancing layer that is a second metal oxide layer or a metal oxynitride layer, comprising:
(a) forming the FL on the tunnel barrier layer with a sputter deposition sequence, comprising;
(1) co-depositing an oxidation control layer (OCL) material that getters oxygen, and a magnetic moment tuning layer (MMTL) material with a first FL sub-layer (FL1) on the tunnel barrier layer;
(2) depositing the OCL material on the co-deposited FL1 and OCL and MMTL materials; and
(3) co-depositing the OCL and MMTL materials with a second FL sub-layer (FL2) on the OCL material;
(b) depositing a metal layer on the co-deposited FL2 and OCL and MMTL materials; and
(c) performing an oxidation or oxynitridation of the metal layer to yield the Hk enhancing layer.

### Claim 50 (depends on 49)

The method of claim 49 wherein the OCL material is one of Mg, a Mg alloy, Ba, or Ca.

### Claim 51 (depends on 49)

The method of claim 49 wherein the OCL and MMTL materials form metal particles or clusters within each of the FL1 and FL2, and wherein the OCL material forms a continuous layer, a discontinuous layer, metal particles, or metal clusters between the co-deposited FL1, OCL, and MMTL materials and the co-deposited FL2, OCL, and MMTL materials.

### Claim 52 (depends on 49)

The method of claim 49 wherein the MMTL material is one or more of Nb, Mo, W, Re, Zr, Ru, Rh, Os, Ir, Zn, Pt, Pd, Ga, and Ge.

### Claim 53

A method of forming a perpendicular magnetic tunnel junction (p-MTJ) having a first interface between a free layer (FL) and a first oxide layer that is a tunnel barrier layer, and a second interface between the FL and a Hk enhancing layer that is a second metal oxide layer or a metal oxynitride layer, comprising:
(a) forming the FL on the tunnel barrier layer with a sputter deposition sequence, comprising;
(1) depositing a first FL sub-layer (FL1) on the tunnel barrier layer;
(2) depositing an oxidation control layer (OCL) material that getters oxygen, on the FL1; and
(3) forming a second FL sub-layer (FL2) on the OCL material wherein the FL2 comprises a magnetic moment tuning layer (MMTL) material; and
(b) depositing a metal layer on the FL2; and
(c) performing an oxidation or oxynitridation of the metal layer to yield the Hk enhancing layer.

### Claim 54 (depends on 53)

The method of claim 53 wherein the MMTL is formed within the FL2 using an ion implant process.

### Claim 55 (depends on 53)

The method of claim 53 wherein the MMTL is formed within the FL2 with a process comprising:
(a) depositing the FL2 on the OCL;
(b) depositing the MMTL on the FL2; and
(c) performing an anneal process to drive the MMTL into the FL2.