# US 2020/0402938 A1 · Bump bond structure for enhanced electromigration performance

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0402938 A1
- Document ID: US20200402938A1
- Status: Published application
- Kind: A1
- Application number: 17/009,648
- Filed: 2020-09-01
- Published: 2020-12-24
- Earliest claimed: 2018-07-27
- Assignees: Texas Instruments Incorporated
- Applicants: Texas Instruments Incorporated
- Inventors: Dibyajat Mishra; Ashok Prabhu; Tomoko Noguchi; Luu Thanh Nguyen; Anindya Poddar; Makoto Yoshino; Hau Nguyen
- Web page: https://patentgrep.com/patent/US20200402938A1

## CPC

- H10W 72/072: {of bump connectors}
- H10W 74/131: {the semiconductor body being only partially enclosed}
- H10W 70/457: {of metallic layers on leadframes}
- H10W 70/453: {comprising flexible metallic tapes}
- H10W 72/012: {of bump connectors, dummy bumps or thermal bumps}
- H10W 72/01221: {using local deposition}
- H10W 72/01223: {in liquid form, e.g. by dispensing droplets or by screen printing}
- H10W 72/01235: {by plating, e.g. electroless plating or electroplating}
- H10W 72/01255: {by using masks}
- H10W 72/01257: {by reflowing}
- H10W 72/01261: {Chemical or physical modification, e.g. by sintering or anodisation (patterning H10W72/01251)}
- H10W 72/01271: {Cleaning, e.g. oxide removal or de-smearing}
- H10W 72/07141: {Means for applying energy, e.g. ovens or lasers}
- H10W 72/07236: {Soldering or alloying}
- H10W 72/07255: {changes in materials}
- H10W 72/073: {of die-attach connectors}
- H10W 72/222: {Multilayered bumps, e.g. a coating on top and side surfaces of a bump core}
- H10W 72/223: {characterised by the structure of the outermost layers, e.g. multilayered coatings}
- H10W 72/241: {Dispositions, e.g. layouts}
- H10W 72/245: {of outermost layers of multilayered bumps, e.g. bump coating being only on a part of a bump core}
- H10W 72/252: {comprising solid metals or solid metalloids, e.g. PbSn, Ag or Cu}
- H10W 72/2528: {Intermetallic compounds}
- H10W 72/255: {of outermost layers of multilayered bumps, e.g. material of a coating}
- H10W 72/29: Bond pads specially adapted therefor
- H10W 72/30: Die-attach connectors
- H10W 72/851: {Dispositions of multiple connectors or interconnections}
- H10W 72/923: {Bond pads having multiple stacked layers}
- H10W 72/9415: {relative to the surface, e.g. recessed, protruding}
- H10W 72/952: {comprising metals or metalloids, e.g. PbSn, Ag or Cu}
- H10W 72/953: {not comprising solid metals or solid metalloids, e.g. polymers, ceramics or liquids}
- H10W 72/983: {Reinforcing structures, e.g. collars}
- H10W 74/00: Encapsulations, e.g. protective coatings
- H10W 74/129: {forming a chip-scale package [CSP]}
- H10W 90/724: {between a chip and a stacked insulating package substrate, interposer or RDL}
- H10W 90/726: {between a chip and a stacked lead frame, conducting package substrate or heat sink}
- H10W 90/734: {between a chip and a stacked insulating package substrate, interposer or RDL}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A microelectronic device has a pillar connected to an external terminal by an intermetallic joint. Either the pillar or the external terminal, or both, include copper in direct contact with the intermetallic joint. The intermetallic joint includes at least 90 weight percent of at least one copper-tin intermetallic compound. The intermetallic joint is free of voids having a combined volume greater than 10 percent of a volume of the intermetallic joint; and free of a void having a volume greater than 5 percent of the volume of the intermetallic joint. The microelectronic device may be formed using solder which includes at least 93 weight percent tin, 0.5 weight percent to 5.0 weight percent silver, and 0.4 weight percent to 1.0 weight percent copper, to form a solder joint between the pillar and the external terminal, followed by thermal aging to convert the solder joint to the intermetallic joint.

## Claims

### Claim 1

A method of forming a microelectronic device, comprising:
forming a solder bump including solder directly on a copper-containing pillar, the copper-containing pillar being electrically coupled to a terminal of a die, the solder having at least 93 weight percent tin, 0.5 to 5.0 weight percent silver, and 0.4 to 1.0 weight percent copper;
heating the solder bump to form a solder joint between the copper-containing pillar and an external lead; and
thermally aging the solder joint by heating the solder joint to convert the solder joint to an intermetallic joint, wherein:
the intermetallic joint includes at least 90 weight percent of at least one copper-tin intermetallic compound (IMC) selected from the group consisting of Cu6Sn5 and Cu3Sn;
the intermetallic joint is free of voids having a combined volume greater than 10 percent of a volume of the intermetallic joint; and
the intermetallic joint is free of a void having a volume greater than 5 percent of the volume of the intermetallic joint.

### Claim 2 (depends on 1)

The method of claim 1, wherein thermally aging the solder joint includes heating the solder joint to a temperature higher than a liquidus temperature of the solder, the liquidus temperature of the solder being a temperature at which crystals of tin alloy can co-exist with a liquid state of the solder in thermodynamic equilibrium.

### Claim 3 (depends on 1)

The method of claim 1, wherein thermally aging the solder joint includes heating the solder joint to a temperature of 220° C. to 260° C., and maintaining the temperature for 30 minutes to 90 minutes.

### Claim 4 (depends on 1)

The method of claim 1, wherein thermally aging the solder joint includes heating the solder joint to a temperature of 150° C. to 180° C., and maintaining the temperature for 300 hours to 350 hours.

### Claim 5 (depends on 1)

The method of claim 1, wherein forming the solder bump includes disposing solder paste onto the copper-containing pillar, the solder paste including particles of the solder.

### Claim 6 (depends on 1)

The method of claim 1, wherein the particles of the solder have an average size less than 5 microns.

### Claim 7

A method of forming a microelectronic device, comprising:
disposing solder between a pillar and an external lead, the pillar being electrically coupled to a terminal of a die, the external lead including copper, the solder having at least 93 weight percent tin, 0.5 to 5.0 weight percent silver, and 0.4 to 1.0 weight percent copper;
heating the solder to form a solder joint between the pillar and an external lead; and
thermally aging the solder joint by heating the solder joint to convert the solder joint to an intermetallic joint, wherein:
the intermetallic joint includes at least 90 weight percent of at least one copper-tin intermetallic compound (IMC) selected from the group consisting of Cu6Sn5 and Cu3Sn;
the intermetallic joint is free of voids having a combined volume greater than 10 percent of a volume of the intermetallic joint; and
the intermetallic joint is free of a void having a volume greater than 5 percent of the volume of the intermetallic joint.

### Claim 8 (depends on 7)

The method of claim 7, wherein thermally aging the solder joint includes heating the solder joint to a temperature higher than a liquidus temperature of the solder, the liquidus temperature of the solder being a temperature at which crystals of tin alloy can co-exist with a liquid state of the solder in thermodynamic equilibrium.

### Claim 9 (depends on 7)

The method of claim 7, wherein thermally aging the solder joint includes heating the solder joint to a temperature of 220° C. to 260° C., and maintaining the temperature for 30 minutes to 90 minutes.

### Claim 10 (depends on 7)

The method of claim 7, wherein thermally aging the solder joint includes heating the solder joint to a temperature of 150° C. to 180° C., and maintaining the temperature for 300 hours to 350 hours.

### Claim 11 (depends on 7)

The method of claim 7, wherein disposing the solder between the pillar and the external lead includes disposing solder paste onto the external lead, the solder paste including particles of the solder.

### Claim 12

A method of forming a microelectronic device, comprising:
forming a solder bump including solder directly on a copper-containing pillar, the copper-containing pillar being electrically coupled to a terminal of a die, the solder including tin, silver, and copper;
heating the solder bump to form a solder joint between the copper-containing pillar and an external lead; and
heating the solder joint to convert the solder joint to an intermetallic joint, wherein:
the intermetallic joint includes at least one copper-tin intermetallic compound (IMC) selected from the group consisting of Cu6Sn5 and Cu3Sn;
the intermetallic joint is free of voids having a combined volume greater than 10 percent of a volume of the intermetallic joint; and
the intermetallic joint is free of a void having a volume greater than 5 percent of the volume of the intermetallic joint.

### Claim 13 (depends on 12)

The method of claim 12, wherein heating the solder joint includes heating to a temperature higher than a liquidus temperature of the solder, the liquidus temperature of the solder being a temperature at which crystals of tin alloy can co-exist with a liquid state of the solder in thermodynamic equilibrium.

### Claim 14 (depends on 12)

The method of claim 12, wherein heating the solder joint includes heating the solder joint to a temperature of 220° C. to 260° C., and maintaining the temperature for 30 minutes to 90 minutes.

### Claim 15 (depends on 12)

The method of claim 12, wherein heating the solder joint includes heating the solder joint to a temperature of 150° C. to 180° C., and maintaining the temperature for 300 hours to 350 hours.