# US 2020/0402851 A1 · Roughening of a Metallization Layer on a Semiconductor Wafer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0402851 A1
- Document ID: US20200402851A1
- Status: Published application
- Kind: A1
- Application number: 16/906,586
- Filed: 2020-06-19
- Published: 2020-12-24
- Earliest claimed: 2019-06-21
- Assignees: Infineon Technologies AG
- Applicants: Infineon Technologies AG
- Inventors: Carsten von Koblinski; Tobias Polster
- Web page: https://patentgrep.com/patent/US20200402851A1

## CPC

- C25F 3/14: locally
- H10W 20/064: {by modifying the conductivity of conductive parts, e.g. by alloying}
- C25F 3/02: Etching
- C25F 7/00: Constructional parts, or assemblies thereof, of cells for electrolytic removal of material from objects (for both electrolytic coating and removal C25D); Servicing or operating
- H10P 50/667: {by liquid etching only}
- H10P 50/71: {using masks for conductive or resistive materials}
- H10W 20/43: Layouts of interconnections
- H10W 74/131: {the semiconductor body being only partially enclosed}
- C25F: PROCESSES FOR THE ELECTROLYTIC REMOVAL OF MATERIALS FROM OBJECTS; APPARATUS THEREFOR
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method of manufacturing a semiconductor wafer having a roughened metallization layer surface is described. The method includes immersing the semiconductor wafer in an electrolytic bath. Gas bubbles are generated in the electrolytic bath. A surface of a metallization layer on the semiconductor wafer is electrochemically roughened in the presence of the gas bubbles by applying a reversing voltage between the metallization layer and an electrode of the electrolytic bath.

## Claims

### Claim 1

A method of manufacturing a semiconductor wafer having a roughened metallization layer surface, the method comprising:
immersing the semiconductor wafer in an electrolytic bath;
generating gas bubbles in the electrolytic bath; and
electrochemically roughening a surface of a metallization layer on the semiconductor wafer in the presence of the gas bubbles by applying a reversing voltage between the metallization layer and an electrode of the electrolytic bath.

### Claim 2 (depends on 1)

The method of claim 1, wherein the gas bubbles are generated from an inert gas or an oxidizing gas or a reducing gas or a mixture of any of these gases.

### Claim 3 (depends on 1)

The method of claim 1, wherein the gas bubbles are configured to form a temporary and statistically distributed micro-masking of an electrochemical dissolve and deposition process on the surface of the metallization layer.

### Claim 4 (depends on 1)

The method of claim 1, wherein the metallization layer is positioned in a region of the electrolytic bath where the gas bubbles render the electrolytic bath foamy.

### Claim 5 (depends on 1)

The method of claim 1, further comprising:
structuring the metallization layer into separated areas before immersing the semiconductor wafer in the electrolytic bath, wherein the separated areas are electrically connected.

### Claim 6 (depends on 1)

The method of claim 1, further comprising:
masking certain areas of the metallization layer before immersing the semiconductor wafer in the electrolytic bath so as to prevent roughening of the masked areas.

### Claim 7 (depends on 1)

The method of claim 1, wherein the reversing voltage between the metallization layer and the electrode of the electrolytic bath is applied over a number of cycles, wherein the cycle duration is equal to or greater than 5 s, 10 s, 20 s, 30 s, or 40 s and/or the number of cycles is equal to or greater than 5, 10, or 20.

### Claim 8 (depends on 1)

The method of claim 1, wherein a frequency of the reversing voltage is equal to or less than 1 Hz, 0.5 Hz, 0.2 Hz, 0.1 Hz, 0.05 Hz, or 0.02 Hz.

### Claim 9 (depends on 1)

The method of claim 1, wherein the metallization layer is based on copper.

### Claim 10

A semiconductor wafer metallization layer surface roughening equipment, comprising:
an electrolytic bath;
a first electrode and a second electrode, the first electrode and the second electrode are configured to be connected to a reversing voltage, wherein at least one of the first electrode and the second electrode is a metallization layer on a semiconductor wafer; and
a first gas bubble generator configured to treat the metallization layer with gas bubbles during electrochemical roughening.

### Claim 11 (depends on 10)

The semiconductor wafer metallization layer surface roughening equipment of claim 10, wherein the semiconductor wafer is held inclined relative to a direction of movement of the gas bubbles in the electrolytic bath.

### Claim 12 (depends on 10)

The semiconductor wafer metallization layer surface roughening equipment of claim 10, wherein the first electrode and the second electrode are each metallization layers on different semiconductor wafers, further comprising:
a second gas bubble generator configured to treat the metallization layer on the further semiconductor wafer with gas bubbles during electrochemical roughening.

### Claim 13

A semiconductor package, comprising:
a semiconductor die having a metallization layer, the metallization layer comprising a roughened surface; and
an encapsulation embedding at least partially the semiconductor die and the roughened surface of the metallization layer, wherein the roughened surface has a roughness of a root mean square height of equal to or greater than 300 nm, 400 nm, 500 nm, 600 nm, 700 nm, or 800 nm.

### Claim 14 (depends on 13)

The semiconductor package of claim 13, wherein the metallization layer further comprises a smooth surface, and wherein the roughness of the roughened surface is equal to or greater than 5, 7, 9, or 11 times the roughness of the smooth surface in terms of the root mean square height of the respective surfaces.

### Claim 15 (depends on 13)

The semiconductor package of claim 13, wherein the semiconductor die is a power die, and wherein the metallization layer comprises a power die backside metallization layer and/or a load electrode metallization layer of the power die.