# US 2020/0402846 A1 · Self-limiting growth

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0402846 A1
- Document ID: US20200402846A1
- Status: Published application
- Kind: A1
- Application number: 16/764,812
- Filed: 2018-11-19
- Published: 2020-12-24
- Earliest claimed: 2017-11-20
- Assignees: Lam Research Corporation
- Applicants: Lam Research Corporation
- Inventors: Joshua Collins; Griffin John Kennedy; Hanna Bamnolker; Michal Danek; Shruti Vivek Thombare; Patrick van Cleemput; Gorun Butail
- Web page: https://patentgrep.com/patent/US20200402846A1

## CPC

- H10P 72/0468: {comprising a chamber adapted to a particular process}
- H10W 20/045: {for deposition from the gaseous phase, e.g. for chemical vapour deposition [CVD]}
- C23C 16/045: {Coating cavities or hollow spaces, e.g. interior of tubes; Infiltration of porous substrates}
- C23C 16/14: Deposition of only one other metal element
- C23C 16/44: characterised by the method of coating (C23C16/04 takes precedence)
- H10D 64/01318: {the conductor comprising a layer of alloy material, compound material or organic material contacting the insulator, e.g. TiN (comprising a layer of alloys of Si, Ge or C H10D64/01314)}
- H10P 14/418: {the conductive layers comprising transition metals}
- H10P 14/432: {using selective deposition}
- H10P 72/0462: {characterised by the construction of the processing chambers, e.g. modular processing chambers}
- H10W 20/056: {by filling conductive material into holes, grooves or trenches}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

Provided herein are methods and apparatuses for forming metal films such as tungsten (W) and molybdenum (Mo) films on semiconductor substrates. The methods involve forming a reducing agent layer, then exposing the reducing agent layer to a metal precursor to convert the reducing agent layer to a layer of the metal. In some embodiments, the reducing agent layer is a silicon- (Si-) and boron- (B-) containing layer. The methods may involve forming the reducing agent layer at a first substrate temperature, raising the substrate temperature to a second substrate temperature, and then exposing the reducing agent layer to the metal precursor at the second substrate temperature. The methods may be used to form fluorine-free tungsten or molybdenum films in certain embodiments. Apparatuses to perform the methods are also provided.

## Claims

### Claim 1

A method comprising:
providing a substrate including a structure;
exposing the substrate to a reducing agent gas at a first substrate temperature of no more than 400° C. to form a conformal reducing agent layer on the structure;
raising the temperature of the substrate to a second substrate temperature of at least 500° C.; and
at the second substrate temperature, exposing the conformal reducing agent layer to a metal precursor to convert the conformal reducing agent layer to the metal.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first substrate temperature is no more than 350° C.

### Claim 3 (depends on 1)

The method of claim 1, wherein the first substrate temperature is no more than 300° C.

### Claim 4 (depends on 1)

The method of claim 1, wherein the reducing agent gas is a silicon-containing gas.

### Claim 5 (depends on 1)

The method of claim 1, wherein the reducing agent gas is a boron-containing gas.

### Claim 6 (depends on 1)

The method of claim 1, wherein the reducing agent gas is a mixture of a silicon-containing gas and a boron-containing gas.

### Claim 7 (depends on 6)

The method of claim 6, wherein the reducing agent gas is a mixture of silane (SiH4) and diborane (B2H6).

### Claim 8 (depends on 1)

The method of claim 1, wherein exposing the conformal reducing agent layer to a metal precursor comprises exposing the conformal reducing agent layer to hydrogen (H2) gas.

### Claim 9 (depends on 1)

The method of claim 1, wherein the metal precursor is provided with H2.

### Claim 10 (depends on 1)

The method of claim 1, wherein exposing the conformal reducing agent layer to a metal precursor to convert the reducing agent layer to metal comprises exposing the conformal reducing agent layer to alternating pulses of H2 and the metal precursor.

### Claim 11 (depends on 1)

The method of claim 1, wherein the metal precursor is a tungsten chloride compound and the metal is tungsten.

### Claim 12 (depends on 1)

The method of claim 1, wherein the metal precursor is a molybdenum-containing compound and the metal is molybdenum.

### Claim 13 (depends on 1)

The method of claim 1, wherein the conformal reducing agent layer is formed directly on an oxide surface.

### Claim 14 (depends on 1)

The method of claim 1, wherein the conformal reducing agent layer is formed directly on a nitride surface.

### Claim 15 (depends on 1)

The method of claim 1, wherein the conformal reducing agent layer is between about 10 and 50 Angstroms thick.

### Claim 16 (depends on 6)

The method of claim 6, wherein the concentration of boron in the reducing agent layer decreases with increasing thickness.

### Claim 17 (depends on 6)

The method of claim 6, wherein the silicon:boron ratio in the mixture is at least 10:1.

### Claim 18

A method comprising:
providing a substrate including a structure;
exposing the substrate to a mixture of a silicon-containing gas and a boron-containing gas at a first substrate temperature of no more than 400° C. to form a conformal reducing agent layer on the structure;
raising the temperature of the substrate to a second substrate temperature of at least 500° C.; and
at the second substrate temperature, exposing the conformal reducing agent layer to a tungsten-containing or molybdenum-containing precursor to convert the reducing agent layer to tungsten or molybdenum.

### Claim 19 (depends on 18)

The method of claim 18, wherein the silicon:boron ratio in the mixture is at least 10:1.

### Claim 20

A method comprising:
providing a substrate including a structure;
exposing the substrate to a mixture of a silicon-containing gas and a boron-containing gas to form a conformal reducing agent layer on the structure; and
exposing the conformal reducing agent layer to a molybdenum-containing precursor to convert the reducing agent layer to molybdenum.

### Claim 21

(canceled)