# US 2020/0402808 A1 · Highly selective silicon oxide/silicon nitride etching by selective boron nitride or aluminum nitride deposition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0402808 A1
- Document ID: US20200402808A1
- Status: Published application
- Kind: A1
- Application number: 16/902,582
- Filed: 2020-06-16
- Published: 2020-12-24
- Earliest claimed: 2019-06-20
- Assignees: Tokyo Electron Limited
- Applicants: Tokyo Electron Limited
- Inventors: Yu-Hao Tsai; Du Zhang; Mingmei Wang
- Web page: https://patentgrep.com/patent/US20200402808A1

## CPC

- H10P 50/246: {of Group III-V materials}
- H10P 50/73: {using masks for insulating materials}
- H10P 14/6319: {Formation by plasma treatments, e.g. plasma oxidation of the substrate}
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10P 14/6939: {characterised by the metal}
- H10P 14/69391: {the material containing aluminium, e.g. Al2O3}
- H10P 50/283: {by chemical means}
- H10P 95/064: {the removal being chemical etching}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method for selective etching of silicon oxide relative to silicon nitride includes exposing a substrate to a first gas that forms a first layer on the silicon oxide film and a second layer on the silicon nitride film, where the first gas contains boron, aluminum, or both boron and aluminum, exposing the substrate to a nitrogen-containing gas that reacts with the first layer to form a first nitride layer on the silicon oxide film and reacts with the second layer to form a second nitride layer on the silicon nitride film, where a thickness of the second nitride layer is greater than a thickness of the first nitride layer. The method further includes exposing the substrate to an etching gas that etches the first nitride layer and silicon oxide film, where the second nitride layer protects the silicon nitride film from etching by the etching gas.

## Claims

### Claim 1

A substrate processing method, comprising:
providing a substrate containing a silicon oxide film and a silicon nitride film;
a1) exposing the substrate to a first gas that forms a first layer on the silicon oxide film and a second layer on the silicon nitride film, wherein the first gas contains boron, aluminum, or both boron and aluminum;
a2) exposing the substrate to a nitrogen-containing gas that reacts with the first layer to form a first nitride layer on the silicon oxide film and reacts with the second layer to form a second nitride layer on the silicon nitride film, wherein a thickness of the second nitride layer is greater than a thickness of the first nitride layer; and
a3) exposing the substrate to an etching gas that etches the first nitride layer and the silicon oxide film, wherein the second nitride layer protects the silicon nitride film from etching by the etching gas.

### Claim 2 (depends on 1)

The method of claim 1, further comprising:
repeating steps a1) and a2) at least once before performing step a3).

### Claim 3 (depends on 1)

The method of claim 1, further comprising:
repeating steps a1), a2), and a3) at least once to further etch the silicon oxide film.

### Claim 4 (depends on 1)

The method of claim 1, further comprising:
a0) exposing the substrate to a H2-containing gas that terminates the silicon oxide film with —OH surface species and terminates the silicon nitride film with —NHx surface species.

### Claim 5 (depends on 4)

The method of claim 4, further comprising:
repeating a0), a1), a2), and a3) at least once to further etch the silicon oxide film.

### Claim 6 (depends on 4)

The method of claim 4, further comprising:
repeating a1), a2), and a3) at least once to further etch the silicon oxide film.

### Claim 7 (depends on 1)

The method of claim 1, wherein the first gas contains a boron hydride, a boron halide, an organoaluminum compound, an aluminum hydride, an aluminum chloride, or a combination thereof.

### Claim 8 (depends on 1)

The method of claim 1, wherein the first gas is selected from the group consisting of BH3, BCl3, BF3, Al(CH3)3, AlH3, AlCl3, and a combination thereof.

### Claim 9 (depends on 1)

The method of claim 1, wherein the nitrogen-containing gas is selected from the group consisting of a nitrogen hydride, a nitrogen halide, N2, and a combination thereof.

### Claim 10 (depends on 1)

The method of claim 1, wherein the nitrogen-containing gas is selected from the group consisting of NH3, N2H4, NCl3, N2, and a combination thereof

### Claim 11 (depends on 1)

The method of claim 1, wherein the etching gas contains a fluorocarbon gas, a hydrofluorocarbon gas, a hydrochlorocarbon gas, a hydrochlorofluorocarbon gas, or a combination thereof.

### Claim 12 (depends on 1)

The method of claim 1, wherein the etching gas is selected from the group consisting of CF4, CF2Cl2, CH2F2, CH4, CH3F, CHF3, C4H6, C2H4, C3H6, CH2Cl2, CH3Cl, CHCl2, CH2ClF, CHCl2F, and a combination thereof.

### Claim 13

A substrate processing method, comprising:
providing a substrate containing a silicon oxide film and a silicon nitride film;
a1) exposing the substrate to a BCl3 gas that forms a first BCl3 layer on the silicon oxide film and a second BCl3 layer on the silicon nitride film;
a2) exposing the substrate to NH3 gas that reacts with the first BCl3 layer to form a first boron nitride layer on the silicon oxide film and reacts with the second BCl3 layer to form a second boron nitride layer on the silicon nitride film, wherein a thickness of the second boron nitride layer is greater than a thickness of the first boron nitride layer; and
a3) exposing the substrate to plasma-excited CF4 gas that etches the first boron nitride layer and the silicon oxide film, wherein the second boron nitride layer protects the silicon nitride film from etching by the plasma-excited CF4 gas.

### Claim 14 (depends on 13)

The method of claim 13, further comprising:
repeating steps a1) and a2) at least once before performing step a3).

### Claim 15 (depends on 13)

The method of claim 13, further comprising:
repeating a1), a2), and a3) at least once to further etch the silicon oxide film.

### Claim 16 (depends on 13)

The method of claim 13, further comprising:
a0) exposing the substrate to a H2-containing gas that terminates the silicon oxide film with —OH surface species and terminates the silicon nitride film with —NHx surface species.

### Claim 17 (depends on 16)

The method of claim 16, further comprising:
repeating a0), a1), a2), and a3) at least once to further etch the silicon oxide film.

### Claim 18 (depends on 16)

The method of claim 16, further comprising:
repeating a1), a2), and a3) at least once to further etch the silicon oxide film.

### Claim 19

A substrate processing method, comprising:
providing a substrate containing a silicon oxide film and a silicon nitride film;
a1) exposing the substrate to a boron-containing gas that forms a boron-containing layer that is thicker on the silicon nitride film than on the silicon oxide film;
a2) exposing the substrate to a nitrogen-containing gas that reacts with the boron-containing layer to form a boron nitride layer that is thicker on the silicon nitride film than on the silicon oxide film; and
a3) exposing the substrate to an etching gas that etches the boron nitride layer on the silicon oxide film and the silicon oxide film, wherein the boron nitride layer protects the silicon nitride film from etching by the etching gas.

### Claim 20 (depends on 19)

The method of claim 19, wherein the boron-containing gas is selected from the group consisting of BH3, BCl3, BF3, and a combination thereof, the nitrogen-containing gas is selected from the group consisting of NH3, N2H4, NCl3, N2, and a combination thereof, and the etching gas is selected from the group consisting of CF4, CF2Cl2, CH2F2, CH4, CH3F, CHF3, C4H6, C2H4, C3H6, CH2Cl2, CH3Cl, CH3Cl, CH2ClF, CHCl2F, and a combination thereof.