# US 2020/0402686 A1 · Superconducting block, superconducting nanocrystal, superconducting device and a process thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0402686 A1
- Document ID: US20200402686A1
- Status: Published application
- Kind: A1
- Application number: 16/979,113
- Filed: 2019-03-11
- Published: 2020-12-24
- Earliest claimed: 2018-03-09
- Assignees: Indian Institute of Science
- Applicants: Indian Institute of Science
- Inventors: Anshu PANDEY; Dev Kumar THAPA; Subham Kumar SAHA
- Web page: https://patentgrep.com/patent/US20200402686A1

## CPC

- H01B 12/00: Superconductive or hyperconductive conductors, cables, or transmission lines
- H10N 60/99: {Alleged superconductivity}
- H10N 60/83: Element shape
- H10N 60/85: Superconducting active materials
- B82Y 10/00: Nanotechnology for information processing, storage or transmission, e.g. quantum computing or single electron logic
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- B82Y 40/00: Manufacture or treatment of nanostructures
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES

## Abstract

The present invention provides a superconducting block, comprising, a pair of cores with materials that are electrically conductive in their normal states. The pair of cores are embedded in the shell with an intervening centroidal distance, with a material that is electrically conductive in its normal state. The embedded pair of cores and the shell are configured to be superconductive. The present invention also provides a superconducting nanocrystal with at least the superconducting block. The present invention also provides a superconductive device with at least the superconducting block and the superconducting nanocrystal. The present invention further provides a process for fabricating the superconducting block and superconducting crystal. The present invention provides superconductors (superconducting block, superconducting nanocrystals) that can be employed to attain superconductivity at high temperatures, corresponding to temperatures existing in the terrestrial ambient and even higher.

## Claims

### Claim 1

A superconducting block, comprising:
a pair of cores with materials that are electrically conductive in their normal states;
a shell with a material that is electrically conductive in its normal state; and
the pair of cores are embedded in the shell, with an intervening centroidal distance (CD), where the embedded pair of cores and the shell are configured to be superconductive.

### Claim 2 (depends on 1)

The superconducting block as claimed in claim 1, wherein each of the cores is with a diameter preferably in the range of 0.3 to 2.7 nanometers.

### Claim 3 (depends on 1)

The superconducting block as claimed in claim 1, wherein magnitude of volta potential difference between the materials of the pair of cores and the shell is greater than or equal to ≥0.4V.

### Claim 4 (depends on 1)

The superconducting block as claimed in claim 1, wherein the intervening centroidal distance (CD) between at least the pair of cores of, is preferably in the range of 0.7 to 20 nm.

### Claim 5 (depends on 1)

The superconducting block as claimed in claim 1, wherein the transition to the superconducting state of the pair of cores and the shell is at a temperature preferably in the range of 1 mK to 104K and at applied pressure preferably in the range of 0-1011 Pa.

### Claim 6 (depends on 1)

The superconducting block as claimed in claim 1, wherein the materials are selected from alkali metals, alkaline earth metals, transitional metals, post transitional metals, metalloids and lanthanoids, preferably Lithium (Li) Sodium (Na), Potassium (K), Caesium (Cs), Magnesium (Mg), Beryllium (Be), Calcium (Ca), Strontium (Sr), Barium (Ba), Gold (Au), Copper (Cu), Nickel (Ni), Molybdenum (Mo), strontium (Sr), silver (Ag), Cobalt (Co), Iron (Fe), Niobium (Nb), Zinc (Zn), Tungsten (W), Platinum (Pt), Palladium (Pd), Titanium (Ti), Chromium (Cr), Scandium (Sc), Manganese (Mn), Vanadium (V), Zirconium (Zr), Hafnium (Hf), Cadmium (Cd), Aluminum (Al), Gallium (Ga), Indium (In), Tin (Sn), Lead (Pb), Neodymium (Nd), Tellurium (Te) Antimony (Sb) Bismuth (Bi) or alloys and compounds thereof.

### Claim 7 (depends on 1)

The superconducting block as claimed in claim 1, wherein the materials are selected from non-elementary conductors, preferably oxides of metals, doped semiconductors, semi-metals, preferably mercury telluride.

### Claim 8 (depends on 1)

The superconducting block as claimed in claim 1, wherein the shell is with multilayers and the pair of cores is with single layer or the pair of cores are with multilayers and the shell is with a single layer, or both shells and the pair of cores are with multilayers.

### Claim 9 (depends on 1)

The superconducting block as claimed in claim 1, wherein a plurality of pairs of cores are embedded in the shell and materials of plurality of pairs of cores are non-identical or identical.

### Claim 10 (depends on 1)

The superconducting block as claimed in claim 1, wherein the superconducting block is a nanospheroid, nanosphere, nanowire, nanotube, nanocube, nanoplate, nanoplatelet and a nanorod.

### Claim 11

A superconducting nanocrystal, comprising:
at least a superconducting block, wherein the superconducting block includes
the pair of cores with materials that are electrically conductive in their normal states;
the shell; and
the pair of cores are embedded in the shell, with an intervening centroidal distance (CD), where the embedded pair of cores and the shell are configured to be superconductive.

### Claim 12 (depends on 11)

The superconducting nanocrystal as claimed in claim 11, wherein magnetic volume susceptibility of the at least superconducting building block is less than −0.001 SI units.

### Claim 13 (depends on 11)

The superconducting nanocrystal as claimed claim 11, wherein a plurality of the superconducting nanocrystals are disposed in a conductive medium with regions and the plurality of the superconducting nanocrystals are not integral to one another.

### Claim 14 (depends on 13)

The superconducting nanocrystal as claimed in claim 13, wherein the resistivity of the plurality of the superconducting nanocrystals disposed in the conductive medium, is less than 1×10-9 Ohm-m.

### Claim 15

A superconductive device, comprising
at least a superconducting block wherein each of the at least superconducting blocks, include a pair of cores with materials that are electrically conductive in their normal states; a shell with a material that is electrically conductive in its normal state; and the pair of cores are embedded in the shell, with an intervening centroidal distance (CD), where the embedded pair of cores and the shell are configured to be superconductive; and a means to extract or induce currents is connected to the at least superconducting block.

### Claim 16 (depends on 15)

The superconductive device as claimed in claim 15, wherein the at least superconducting block is disposed on a substrate.

### Claim 17 (depends on 16)

The superconductive device as claimed in claim 16, wherein the material for the substrate is selected from an electrically conducting material, an insulator or a semiconductor.

### Claim 18 (depends on 16)

The superconductive device as claimed in claim 16, wherein the material for the substrate is selected from polymer, preferably polyethene, polystyrene, bakelite, rubber, preferably a silicone, nitrile, glass, preferably a borosilicate glass, a metal, preferably copper, iron, nickel or aluminum, or an alloy of the metals, or a combination thereof.

### Claim 19 (depends on 15)

The superconductive device as claimed in claim 15, wherein the at least superconducting nanocrystal is used in place of the at least superconducting block.

### Claim 20

A process for the fabrication of a superconducting block, comprising steps of:
(i) selecting a core material and a shell material, with materials that are electrically conductive in their normal states;
(ii) forming at least a pair of cores of the core material with diameter preferably in the range of 0.3 to 2.7 nanometers; and
(iii) embedding the pair of cores into the shell with intervening centroidal distance (CD) between at least the pair of cores of, wherein the intervening centroidal distance (CD) is preferably in the range of 0.7 to 20 nm, to obtain the superconducting block.

### Claim 21 (depends on 20)

The process as claimed in claim 20, wherein a superconducting nanocrystal is prepared from at least a pair of cores and at least a shell.

### Claim 22 (depends on 20)

The process as claimed in claim 20, wherein the materials that are electrically conductive in their normal state for the cores and the shells are selected from alkali metals, alkaline earth metals, transitional metals, post transitional metals, metalloids and lanthanoids, preferably Lithium (Li) Sodium (Na), Potassium (K), Caesium (Cs), Magnesium (Mg), Beryllium (Be), Calcium (Ca), Gold (Au), Copper (Cu), Molybdenum (Mo), strontium (Sr), silver (Ag), Cobalt (Co), Iron (Fe), Copper (Cu), Niobium (Nb), Zinc (Zn), Tungsten (W), Platinum (Pt), Palladium (Pd), Silver (Ag), Manganese (Mn), Zinc (Zn), Vanadium (V), Silver (Ag), Zirconium (Zr), Haufnium (Hf), Cadmium (Cd), Aluminum (Al), Lead (Pb), Neodymium (Nd), Tellurium (Te) or alloys thereof.

### Claim 23 (depends on 20)

The process as claimed in claim 20, wherein the materials are selected from non-elementary conductors, preferably oxides of metals, doped semiconductors, semi-metals, preferably mercury telluride.

### Claim 24 (depends on 20)

The process as claimed in claim 20, wherein magnitude of volta potential difference between the materials of the pair of cores and the shellis greater than or equal to ≥0.4V.

### Claim 25 (depends on 20)

The process as claimed in claim 20, wherein the transition to the superconducting state of the pair of cores and the shell is at a temperature preferably in the range of 1 mK to 104K and at applied pressure preferably in the range of 0-1011 Pa.

### Claim 26 (depends on 20)

The process as claimed in claim 20, wherein the molar ratios of the materials for the shells and the cores are preferably in the range of 1:20 to 20:1.