# US 2020/0400613 A1 · Methods of characterizing ion-exchanged chemically strengthened glasses containing lithium

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0400613 A1
- Document ID: US20200400613A1
- Status: Published application
- Kind: A1
- Application number: 17/010,942
- Filed: 2020-09-03
- Published: 2020-12-24
- Earliest claimed: 2015-09-17
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Ryan Claude Andrews; Rostislav Vatchev Roussev; Vitor Marino Schneider
- Web page: https://patentgrep.com/patent/US20200400613A1

## CPC

- G01N 27/60: by investigating electrostatic variables {, e.g. electrographic flaw testing (G01N27/007 takes precedence)}
- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- G01N 27/72: by investigating magnetic variables
- G01N 33/386: {Glass}
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

Methods of characterizing ion-exchanged chemically strengthened glass containing lithium are disclosed. The methods allow for performing quality control of the stress profile in chemically strengthened Li-containing glasses having a surface stress spike produced in a potassium-containing salt, especially in a salt having both potassium and sodium. The method allows the measurement of the surface compression and the depth of the spike, and its contribution to the center tension, as well as the compression at the bottom of the spike, and the total center tension and calculation of the stress at the knee where the spike and the deep region of the stress profile intersect. The measurements are for a commercially important profile that is near-parabolic in shape in most of the interior of the substrate apart from the spike.

## Claims

### Claim at position 1

1-21. (canceled)

### Claim 22

A method of characterizing a stress profile of a chemically strengthened glass substrate formed by the in-diffusion of alkali ions and having an upper surface and a body, a shallow spike region of stress immediately adjacent the upper surface and a deep region of slowly varying stress within the body and that intersects the spike region at a knee, wherein the method comprises:
measuring a TM mode spectrum and a TE mode spectrum of the glass substrate, wherein the TM mode spectrum and the TE mode spectrum each include mode lines and a transition associated with a critical angle;
calculating the knee stress CSknee utilizing the TE mode spectrum, TM mode spectrum, and the stress-optic coefficient SOC.

### Claim 23 (depends on 22)

The method of claim 22, further comprising determining a surface compressive stress CSsp of the spike.

### Claim 24 (depends on 23)

The method of claim 23, wherein determining the surface compressive stress CSsp of the spike utilizes the TM and TE mode spectra.

### Claim 25 (depends on 23)

The method of claim 23, wherein determining the surface compressive stress CSsp of the spike utilizes a measurement of a surface concentration of at least one type of the alkali ions.

### Claim 26 (depends on 22)

The method of claim 22, further comprising determining an amount of birefringence BR.

### Claim 27 (depends on 26)

The method of claim 26, wherein determining the amount of birefringence BR comprises measuring a difference between the TE and TM transition locations.

### Claim 28 (depends on 27)

The method of claim 27, wherein calculating the knee stress CSknee utilizes the amount of birefringence BR.

### Claim 29 (depends on 28)

The method of claim 28, wherein the knee stress CSknee is calculated as CSknee=(CFD)(BR)/SOC, where CFD is a calibration factor.

### Claim 30 (depends on 29)

The method of claim 29, wherein CFD is between 0.5 and 1.5.

### Claim 31 (depends on 28)

The method of claim 28, wherein the knee stress CSknee is calculated as CSknee=K3×BR/SOC, where K3 is a calibration factor.

### Claim 32 (depends on 31)

The method of claim 31, wherein K3 is between 0.2 and 2.

### Claim 33 (depends on 26)

The method of claim 26, wherein the amount of birefringence BR is given by:
BR=nLMTE−nLMTM
where nLMTE is the effective index of a highest-common-order TE spike mode, and nLMTM is the effective index of a highest-common-order TM spike mode.

### Claim 34 (depends on 33)

The method of claim 33, wherein calculating the knee stress CSknee utilizes the amount of birefringence BR.

### Claim 35 (depends on 34)

The method of claim 34, wherein the knee stress CSknee is calculated as CSknee=(CFD)(BR)/SOC, where CFD is a calibration factor.

### Claim 36 (depends on 35)

The method of claim 35, wherein CFD is between 0.5 and 1.5.

### Claim 37 (depends on 34)

The method of claim 34, wherein the knee stress CSknee is calculated as CSknee=K3×BR/SOC, where K3 is a calibration factor.

### Claim 38 (depends on 37)

The method of claim 37, wherein K3 is between 0.2 and 2.

### Claim 39 (depends on 22)

A prism-coupling system, wherein the prism-coupling system is configured to perform the method of claim 22.