# US 2020/0395829 A1 · Method for producing radially anisotropic multipolar solid magnet adapted to different waveform widths

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0395829 A1
- Document ID: US20200395829A1
- Status: Published application
- Kind: A1
- Application number: 16/888,016
- Filed: 2020-05-29
- Published: 2020-12-17
- Earliest claimed: 2019-06-11
- Assignees: Shenzhen Radimag Magnets Co., Ltd
- Applicants: Shenzhen Radimag Magnets Co.,Ltd
- Inventors: Wenhao CHENG
- Web page: https://patentgrep.com/patent/US20200395829A1

## CPC

- H02K 15/03: having permanent magnets
- H02K 1/02: characterised by the magnetic material
- H02K 1/2726: the rotor consisting of a single magnet or two or more axially juxtaposed single magnets
- H02K 1/2733: Annular magnets
- H02K 1/30: using intermediate parts, e.g. spiders
- H02K 2213/03: Machines characterised by numerical values, ranges, mathematical expressions or similar information
- H02K: DYNAMO-ELECTRIC MACHINES (dynamo-electric relays H01H53/00; conversion of DC or AC input power into surge output power {H03K3/53})

## Abstract

A method and device for producing a radially anisotropic multipolar solid magnet adapted to different waveform widths are provided. A mold core is removed from a mold for molding the magnet, and outer oriented poles, the number of which is the same as that of poles of the radially anisotropic multipolar solid cylindrical magnet, are arranged outside the mold. The width of a front end of a single outer oriented pole is determined according to the desired width of a single waveform of the radially anisotropic multipolar solid cylindrical magnet after being magnetized. The sum L of widths or arc lengths of front ends of all the outer oriented poles is less than 0.9πD, particularly less than 0.7πD, where D is the outer diameter of a mold sleeve. Magnetic particles in a mold cavity are rotated with the mold only during magnetization.

## Claims

### Claim 1

A method for molding a radially anisotropic multipolar solid cylindrical magnet adapted to different waveform widths, wherein a mold core is removed from a mold for molding the magnet; outer oriented poles, the number of which is the same as that of poles of the radially anisotropic multipolar solid cylindrical magnet, are arranged outside the mold; the width of a front end of a single outer oriented pole is determined according to the desired width of a single waveform of the radially anisotropic multipolar solid cylindrical magnet after being magnetized; and, when the sum L of widths or arc lengths of front ends of all the outer oriented poles is less than 0.9πD, particularly less than 0.7πD, where D is the outer diameter of a mold sleeve, magnetic particles in a mold cavity are continuously rotated with the mold during magnetization.

### Claim 2

A method for molding a radially anisotropic multipolar solid cylindrical magnet adapted to different waveform widths, comprising following steps of:
(1) preparing a mold without a mold core;
(2) arranging, outside the prepared mold, outer oriented poles, the number of which is the same as that of poles of the radially anisotropic multipolar solid cylindrical magnet, the sum L of widths or arc lengths of front ends of all the outer oriented poles being less than 0.9πD, particularly less than 0.7πD, where D is the outer diameter of a mold sleeve;
(3) filling anisotropic magnetic particles in a mold cavity;
(4) applying a first magnetic field to continuously rotate the mold and the magnetic particles in the mold cavity;
(5) stopping the rotation of the mold and the magnetic particles, applying a second magnetic field, applying an increased stress to the magnetic particles in the mold cavity by an upper ram and a lower ram, and maintaining this stress for a certain period of time to obtain a blank; or, by keeping the lower ram unmoved, moving the upper ram down to apply an increased stress to the magnetic particles in the mold cavity and maintaining this stress for a certain period of time; or, by keeping the upper ram unmoved, moving the lower ram up to apply an increased stress to the magnetic particles in the mold cavity and maintaining this stress for a certain period of time, the stress being preferably 20 MPa to 200 MPa, preferably 50 MPa to 150 MPa;
(6) when the magnetic particles in the mold cavity cannot recover to an out-of-order state before orientation after leaving the oriented magnetic field, applying a third magnetic field, and continuously applying a stress by the rams until the blank has a desired density;
(7) applying a fourth magnetic field to demagnetize the blank; and preferably, applying a reverse magnetic field to the blank in the mold cavity to demagnetize the blank, or applying a forward/reverse alternating magnetic field to demagnetize the blank in the mold cavity; and
(8) stopping the application of stress, and demolding to obtain the blank.

### Claim 3 (depends on 2)

The method according to claim 2, wherein the intensity of the second magnetic field is lower than that of the first magnetic field, the intensity of the first magnetic field being 1.5 to 3 times of that of the second magnetic field; the intensity of the third magnetic field is 1 to 0 times of that of the second magnetic field; and, the intensity of the fourth magnetic field is 0.5 to 1.0 times of that of the second magnetic field.

### Claim 4 (depends on 1)

An application of a radially anisotropic multipolar solid cylindrical magnet molded by the method according to claim 1, wherein the radially anisotropic multipolar solid cylindrical magnet is used for waveforms of magnetic fields of permanent magnetic motors with different widths.

### Claim 5 (depends on 4)

The application according to claim 4, wherein the radially anisotropic multipolar solid cylindrical magnet is directly used as a rotor of a high-precision micro-motor having an inner diameter or diameter less than 3 mm or even less, or mounted, as a component for providing a permanent magnetic field, on a motor shaft by forming a hole with an arbitrarily small inner diameter or diameter in the center of the magnet.

### Claim 6 (depends on 1)

A device using the molding method according to claim 1, comprising a mold, a magnetic field generation device, a rotating mechanism and a stress applying device;
the mold comprises a mold sleeve, a mold cavity, an upper ram and a lower ram, without a mold core;
the magnetic field generation device comprises outer oriented poles, the number of which is the same as that of poles of a radially anisotropic multipolar solid cylindrical magnet and which are arranged outside the mold, wherein the width of the front end of a single outer oriented pole is determined according to the desired width of a single waveform of the radially anisotropic multipolar solid cylindrical magnet after being magnetized; the sum L of widths or arc lengths of front ends of all the outer oriented poles is less than 0.9πD, particularly less than 0.7πD, where D is the outer diameter of the mold sleeve; and the outer orientated poles are symmetrically arranged at equal intervals around the magnet within 360°; and
the rotating mechanism enables anisotropic magnetic particles in the mold cavity to continuously rotate with the mold only during magnetization.

### Claim 7 (depends on 2)

An application of a radially anisotropic multipolar solid cylindrical magnet molded by the method according to claim 2, wherein the radially anisotropic multipolar solid cylindrical magnet is used for waveforms of magnetic fields of permanent magnetic motors with different widths.

### Claim 8 (depends on 3)

An application of a radially anisotropic multipolar solid cylindrical magnet molded by the method according to claim 3, wherein the radially anisotropic multipolar solid cylindrical magnet is used for waveforms of magnetic fields of permanent magnetic motors with different widths.

### Claim 9 (depends on 2)

A device using the molding method according to claim 2, comprising a mold, a magnetic field generation device, a rotating mechanism and a stress applying device;
the mold comprises a mold sleeve, a mold cavity, an upper ram and a lower ram, without a mold core;
the magnetic field generation device comprises outer oriented poles, the number of which is the same as that of poles of a radially anisotropic multipolar solid cylindrical magnet and which are arranged outside the mold, wherein the width of the front end of a single outer oriented pole is determined according to the desired width of a single waveform of the radially anisotropic multipolar solid cylindrical magnet after being magnetized; the sum L of widths or arc lengths of front ends of all the outer oriented poles is less than 0.9πD, particularly less than 0.7πD, where D is the outer diameter of the mold sleeve; and the outer orientated poles are symmetrically arranged at equal intervals around the magnet within 360°; and
the rotating mechanism enables anisotropic magnetic particles in the mold cavity to continuously rotate with the mold only during magnetization.

### Claim 10 (depends on 3)

A device using the molding method according to claim 3, comprising a mold, a magnetic field generation device, a rotating mechanism and a stress applying device;
the mold comprises a mold sleeve, a mold cavity, an upper ram and a lower ram, without a mold core;
the magnetic field generation device comprises outer oriented poles, the number of which is the same as that of poles of a radially anisotropic multipolar solid cylindrical magnet and which are arranged outside the mold, wherein the width of the front end of a single outer oriented pole is determined according to the desired width of a single waveform of the radially anisotropic multipolar solid cylindrical magnet after being magnetized; the sum L of widths or arc lengths of front ends of all the outer oriented poles is less than 0.9πD, particularly less than 0.7πD, where D is the outer diameter of the mold sleeve; and the outer orientated poles are symmetrically arranged at equal intervals around the magnet within 360°; and
the rotating mechanism enables anisotropic magnetic particles in the mold cavity to continuously rotate with the mold only during magnetization.