# US 2020/0395631 A1 · Solid electrolyte composite having superior flexibility and strength and method of manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0395631 A1
- Document ID: US20200395631A1
- Status: Published application
- Kind: A1
- Application number: 16/741,174
- Filed: 2020-01-13
- Published: 2020-12-17
- Earliest claimed: 2019-06-11
- Assignees: Hyundai Motor Company; Kia Motors Corporation; Ulsan National Institute of Science and Technology
- Applicants: Hyundai Motor Company; Kia Motors Corporation; Ulsan National Institute of Science and Technology
- Inventors: Sang Mo Kim; Hong Seok Min; Sang Heon Lee; Jae Min Lim; Ju Yeong Seong; Yun Sung Kim; Sang Young Lee; Jung Hwan Kim; Sang Ho Hong
- Web page: https://patentgrep.com/patent/US20200395631A1

## CPC

- H01M 10/0565: Polymeric materials, e.g. gel-type or solid-type
- H01M 10/0585: of accumulators having only flat construction elements, i.e. flat positive electrodes, flat negative electrodes and flat separators
- H01M 10/056: characterised by the materials used as electrolytes, e.g. mixed inorganic/organic electrolytes
- H01M 50/403: Manufacturing processes of separators, membranes or diaphragms
- H01M 50/411: Organic material
- H01M 50/417: Polyolefins
- H01M 50/423: Polyamide resins
- H01M 50/426: Fluorocarbon polymers
- H01M 50/44: Fibrous material
- H01M 50/446: Composite material consisting of a mixture of organic and inorganic materials
- H01M 2300/0068: inorganic
- H01M 2300/0071: Oxides
- H01M 2300/0082: Organic polymers
- H01M 2300/0091: in the form of mixtures
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Disclosed are a solid electrolyte composite having high flexibility and strength, a method of manufacturing the same and an electrochemical device including the same. The solid electrolyte composite includes a matrix including a solid electrolyte, and fibrous polymers located in the same layer as the matrix and distributed in the matrix, and is manufactured by preparing a first solution including a polymer material, preparing a second solution including a solid electrolyte, producing fibrous polymers by electrospinning the first solution and simultaneously obtaining a structure configured such that the solid electrolyte is loaded between the fibrous polymers by electrospraying the second solution, and pressing the structure.

## Claims

### Claim 1

A solid electrolyte composite, comprising:
a matrix comprising a solid electrolyte; and
fibrous polymers located in the same layer as the matrix and distributed in the matrix.

### Claim 2 (depends on 1)

The solid electrolyte composite of claim 1, wherein the solid electrolyte comprises a sulfide-based solid electrolyte, an oxide-based solid electrolyte, or combinations thereof.

### Claim 3 (depends on 1)

The solid electrolyte composite of claim 1, wherein the fibrous polymers comprises one or more selected from the group consisting of polyethylene terephthalate, polyimide, polyamide, polysulfone, polyvinylidene fluoride, polyacrylonitrile, polyethylene, and polypropylene.

### Claim 4 (depends on 1)

The solid electrolyte composite of claim 1, wherein the fibrous polymers have an average diameter of about 0.001 μm to about 10 μm and an average length of about 150 μm to 10,000 μm.

### Claim 5 (depends on 1)

The solid electrolyte composite of claim 1, wherein the solid electrolyte composite has a thickness of about 1 μm to 100 μm.

### Claim 6 (depends on 1)

The solid electrolyte composite of claim 1, wherein the solid electrolyte composite is a free-standing thin film.

### Claim 7 (depends on 1)

The solid electrolyte composite of claim 1, wherein the solid electrolyte composite has a density variation of about 15% or less.

### Claim 8 (depends on 1)

The solid electrolyte composite of claim 1, wherein the solid electrolyte composite has a density of about 1.3 g/cm3 to 4.6 g/cm3.

### Claim 9

A method of manufacturing a solid electrolyte composite, comprising:
preparing a first solution comprising a polymer material;
preparing a second solution comprising a solid electrolyte;
producing fibrous polymers by electrospinning the first solution and simultaneously obtaining a structure configured such that the solid electrolyte is loaded between the fibrous polymers by electrospraying the second solution; and
pressing the structure.

### Claim 10 (depends on 9)

The method of claim 9, further comprising drying the pressed structure.

### Claim 11 (depends on 9)

The method of claim 9, wherein the polymer material comprises one or more selected from the group consisting of polyethylene terephthalate, polyimide, polyamide, polysulfone, polyvinylidene fluoride, polyacrylonitrile, polyethylene, and polypropylene.

### Claim 12 (depends on 9)

The method of claim 9, wherein the first solution comprises an amount of about 5 wt % to 30 wt % of the polymer material based on the total weight of the first solution.

### Claim 13 (depends on 9)

The method of claim 9, wherein the solid electrolyte comprises a sulfide-based solid electrolyte, an oxide-based solid electrolyte, or combinations thereof.

### Claim 14 (depends on 9)

The method of claim 9, wherein the solid electrolyte has an average particle diameter of about 0.001 μm to 10 μm.

### Claim 15 (depends on 9)

The method of claim 9, wherein the second solution comprises an amount of about 5 wt % to 50 wt % of the solid electrolyte based on the total weight of the second solution.

### Claim 16 (depends on 9)

The method of claim 9, wherein the electrospinning is performed using a first unit including a first tank for storing the first solution and a pin-shaped first nozzle for jetting the first solution stored in the first tank.

### Claim 17 (depends on 9)

The method of claim 9, wherein the electrospinning is performed under conditions of an applied voltage of about 1 kV to 30 kV, a jetting distance of about 5 cm to 20 cm and a jetting speed of about 5 μl/min to 20 μl/min.

### Claim 18 (depends on 9)

The method of claim 9, wherein the electro spraying is performed using a second unit including a second tank for storing the second solution and a pin-shaped second nozzle for jetting the second solution stored in the second tank.

### Claim 19 (depends on 9)

The method of claim 9, wherein the electrospraying is performed under conditions of an applied voltage of about 1 kV to 30 kV, a jetting distance of about 5 cm to 20 cm and a jetting speed of about 50 μl/min to 1,000 μl/min.

### Claim 20 (depends on 1)

An all-solid-state battery, comprising:
a cathode;
an anode; and
a solid electrolyte composite of claim 1 disposed between the cathode and the anode.