# US 2020/0395608 A1 · Method for producing silicon-based anodes for secondary batteries

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0395608 A1
- Document ID: US20200395608A1
- Status: Published application
- Kind: A1
- Application number: 16/077,963
- Filed: 2017-02-10
- Published: 2020-12-17
- Earliest claimed: 2016-02-15
- Assignees: Helmholtz-Zentrum Dresdenrossendorf E.V.; Technische Universitaet Bergakademie Freiberg
- Applicants: Helmholtz-Zentrum Dresdenrossendorf E.V.; Technische Universitaet Bergakademie Freiberg
- Inventors: Charaf CHERKOUK; Dirk C. MEYER; Tilmann LEISEGANG; Teresa Orellana PEREZ; Slawomir PRUCNAL; Wolfgang SKORUPA
- Web page: https://patentgrep.com/patent/US20200395608A1

## CPC

- H01M 4/386: {Silicon or alloys based on silicon}
- H01M 10/052: Li-accumulators
- H01M 4/0409: {by a doctor blade method, slip-casting or roller coating}
- H01M 4/0421: {involving vapour deposition}
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY

## Abstract

A method for producing silicon-based anodes for secondary batteries carries out the following steps for producing an anode: —depositing a silicon layer on a metal substrate having grain boundaries, wherein the silicon layer has a first boundary surface directed towards the metal substrate, —heating the metal substrate using a heating unit to a temperature between 200° C. and 1000° C., —conditioning the region of the second boundary surface of the silicon layer that is facing away from the metal substrate using an energy-intensive irradiation during the heating, —generating polyphases in the region of the silicon layer and the metal substrate, made up of amorphous silicon and/or crystalline silicon of the silicon of the silicon layer and of crystalline metal of the metal substrate and of silicide and—generating crystalline metal of the metal substrate.

## Claims

### Claim 1

A method for the manufacture of silicon-based anodes for secondary batteries (30), wherein the secondary batteries (30) comprise at least of the anode, at least one electrolyte (31a, 31b) and a counter-electrode (33), comprising the following steps:
depositing a silicon layer (3) on a metal substrate (1), wherein the silicon layer (3) has a first interface (14) directed toward the metal substrate (1),
heating the metal substrate (1) by means of a heating unit (22) to a temperature between 200° C. and 1000° C.,
tempering the region of the second interface (15) of the silicon layer (3) turned away from the metal substrate (1) by means of an energy-intensive irradiation during the heating,
generating multiple phases (10, 11) in the region of the silicon layer (3) and of the metal substrate (1), comprising amorphous silicon and/or crystalline silicon of the silicon of the silicon layer (3) and crystalline metal of the metal substrate (1) and
generating crystalline metal (8) of the metal substrate (1).

### Claim 2 (depends on 1)

The method according to claim 1, wherein a buffer layer (4a, 4b) in the form of a metallic, oxidic, carbon-containing or polymer-containing layer is respectively introduced at the first Si-layer interface (14) to the metal substrate (1) and/or at the second Si-layer interface (15) directed toward the electrolyte (31b).

### Claim 3 (depends on 1)

The method according to claim 1, wherein the tempering is performed by means of an arrangement (21) for rapid energy-intensive thermal treatment and annealing.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the metal substrate (1) functions as an integrated current lead.

### Claim 5 (depends on 4)

The method according to claim 4, wherein nickel or copper is used as the metal of the metal substrate (1).

### Claim 6 (depends on 1)

The method according to claim 1, wherein the irradiation and the process for annealing are performed at least with an energy source in the form of an energy-intensive flash lamp (6), which has a flash duration between 0.2 ms and 20 ms and an energy density of 0.6 J/cm2 and 160 J/cm2.

### Claim 7 (depends on 1)

The method according to claim 1, wherein, by means of a roll-to-roll technology, both the deposition of the silicon layer on the metal substrate and the buffer layers and/or as well as the thermal treatment and annealing are performed on a metal substrate, which is situated on a roll, unrolled, coated, heated and processed as well as finally rolled up in the roll once again.

### Claim 8 (depends on 1)

A silicon-based anode (20), manufactured according to the method of claim 1 for secondary batteries (30), wherein the anode (20) at least comprises
a metal substrate (1), functioning as carrier material and as current lead,
a silicon layer (3) deposited on the metal substrate (1), with a formation of a first interface (14) to the metal substrate (1),
multiple phases (10, 11) of amorphous silicon,
crystalline silicon and crystalline metal in the region of the metal substrate (1) and of the silicon layer (3).

### Claim 9 (depends on 8)

The anode according to claim 8, wherein at least one buffer layer (4b) is situated in the region of the first interface (14) between metal substrate (1) and the silicon layer (3).

### Claim 10 (depends on 8)

The anode according to claim 8, wherein at least one buffer layer (4a) is applied on a second interface (15) of the silicon layer (3) turned away from the metal substrate (1).

### Claim 11 (depends on 8)

An arrangement (21) for energy-intensive thermal treatment and annealing of the anode (20) according to claim 8, wherein the arrangement (21) at least comprises
at least one energy-intensive energy source (6), which is directed with its energy flow toward the silicon layer (3) of the anode (20),
a heating unit (22), which is associated with the metal substrate (1) and is directed toward the metal substrate (1) and at least heats the metal substrate (1) and the silicon layer (3) to a temperature between 200° C. and 1000° C.,
wherein, during the heating, the energy source (6) is directed toward the second interface (15) of the silicon layer (3) turned away from the metal substrate (1) for the transmission of short-time high energy (7).

### Claim 12 (depends on 11)

The arrangement according to claim 11, wherein the energy-intensive energy source (6) at least comprises
at least one flash lamp (6), which is directed toward the second interface (15) of the silicon layer (3) of the anode (20),
at least one reflector (5) associated with the flash lamp (6),
wherein, during the heating, the flash-lamp light (7) is directed toward the second interface (15) of the silicon layer (3) turned away from the metal substrate (1) for the transmission of short-time high energy.

### Claim 13 (depends on 8)

A secondary battery (30) with an anode (20) according to claim 8, comprising at least the components:
a cathode (33),
a first electrolyte (31a),
a separator (32),
a second electrolyte (31b), wherein the anode (20) is arranged after the second electrolyte (31b), wherein the components: cathode (33), first electrolyte (31a), separator (32), second electrolyte (31b) and anode (20) are combined in layered manner in the said order within the secondary battery (30).