# US 2020/0395599 A1 · Method of producing amorphous carbon chips and anodes made therefrom for use in electrochemical cells

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0395599 A1
- Document ID: US20200395599A1
- Status: Published application
- Kind: A1
- Application number: 16/773,870
- Filed: 2020-01-27
- Published: 2020-12-17
- Earliest claimed: 2019-01-29
- Assignees: Purdue Research Foundation
- Applicants: Purdue Research Foundation
- Inventors: Vilas Ganpat Pol
- Web page: https://patentgrep.com/patent/US20200395599A1

## CPC

- H01M 4/133: Electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/587: for inserting or intercalating light metals
- C08F 8/36: Sulfonation; Sulfation
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method of producing a sulfonated polymer. The method includes providing a source for a quantity of a polymer having a shape. The quantity of the polymer is heated while immersed in sulfuric acid to 100-200° C. for a period time in a closed reactor containing an atmosphere and capable of holding pressure generated by a reaction between the quantity of the polymer and the sulfuric acid resulting in a sulfonated polymer, wherein substantially all the quantity of the polymer from the source is converted into sulfonated polymer. The sulfonated polymer is then removed from the reactor and dried. An electrode suitable for use as an electrode in an electrochemical energy storage cell is disclosed. The electrode contains amorphous porous carbon sheets made from a sulfonated polymer with a morphology wherein the amorphous porous carbon sheets have the morphology of the sulfonated polymer from which they are made.

## Claims

### Claim 1

A method of producing a sulfonated polymer, the method comprising:
providing a source for a quantity of a polymer, wherein the quantity of the polymer has a shape;
heating the quantity of the polymer immersed in sulfuric acid to a temperature in the range of 100-200° C. for a period time in a closed reactor containing an atmosphere, wherein the reactor is capable of holding pressure generated by a reaction between the quantity of the polymer and the sulfuric acid resulting in a sulfonated polymer, wherein substantially all the quantity of the polymer from the source is converted into sulfonated polymer;
removing the sulfonated polymer from the reactor; and
drying the removed sulfonated polymer.

### Claim 2 (depends on 1)

The method of claim 1, wherein the pressure generated from the reaction is in the range of 10-200 MPa.

### Claim 3 (depends on 1)

The method of claim 1, wherein the time is in the range of 1 minute to 20 hours.

### Claim 4 (depends on 1)

The method of claim 1, further comprising the step of heating the sulfonated polymer to 500-1000° C. in an inert atmosphere, wherein sulfonic groups are converted into gaseous species, resulting in amorphous porous carbon retaining the morphology of the sulfonated polymer.

### Claim 5 (depends on 4)

The method of claim 4, wherein the sulfonated polymer is in a sheet form and the porous carbon is in the form of porous carbon sheets.

### Claim 6 (depends on 5)

The method of claim 5, wherein the porous carbon sheets have a thickness in the range of 1-100 micrometers.

### Claim 7 (depends on 4)

The method of claim 4, wherein the porous carbon sheets have a width in the range of 1-100 micrometers.

### Claim 8 (depends on 5)

The method of claim 5, where in the porous carbon sheets have a surface area in the range of 10 m2/g -1000 m2/g.

### Claim 9 (depends on 4)

The method claim 4, wherein the shape of the quantity of the polymer is retained in the sulfonated polymer and the volume shrinkage of the source of the polymer during conversion to carbon via the sulfonated polymer is in the range of 5-25%.

### Claim 10 (depends on 1)

The method of claim 1, wherein the polymer is a low density polyethylene or high density polyethylene or their mixture.

### Claim 11 (depends on 1)

The method of claim 1, wherein the source is waste polymer bags.

### Claim 12 (depends on 1)

The method of claim 1, wherein the polymer is a low density polyethylene or high density polyethylene.

### Claim 13 (depends on 1)

The method of claim 1, wherein the polymer contains colorants and pigments

### Claim 14 (depends on 4)

The method of claim 4, wherein the source is waste polymer bags.

### Claim 15 (depends on 1)

The method of claim 1, wherein the polymer is a new low density polyethylene or a high density polyethylene fragmented into pieces wherein each piece has a length of one e inch or less in any dimension.

### Claim 16 (depends on 4)

The methods of claim 4, wherein the polymer is a low density polyethylene or a high density polyethylene fragmented into pieces wherein each piece has a length of one inch or less in nay dimension.

### Claim 17

An electrode suitable for use as an electrode in an electrochemical energy storage cell, wherein the electrode contains amorphous porous carbon sheets made from a sulfonated polymer with a morphology wherein the amorphous porous and having the morphology of the sulfonated polymer from which the porous carbon sheets are made.

### Claim 18 (depends on 17)

The electrode of claim 17, wherein the electrode in lithium ion battery has a specific capacity of energy storage in the range of 200-600 mAh/g.

### Claim 19 (depends on 17)

An electrochemical energy storage cell comprising the electrode of claim 17.

### Claim 20 (depends on 18)

An electrochemical energy storage cell comprising the electrode of claim 18.

### Claim 21 (depends on 19)

The electrochemical energy storage cell of claim 19, wherein the electrochemical storage energy cell is a lithium ion battery.