# US 2020/0395593 A1 · Anode pre-lithiation for high energy li-ion battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0395593 A1
- Document ID: US20200395593A1
- Status: Published application
- Kind: A1
- Application number: 16/900,352
- Filed: 2020-06-12
- Published: 2020-12-17
- Earliest claimed: 2019-06-12
- Assignees: A123 Systems, Inc.
- Applicants: A123 Systems LLC
- Inventors: Xiangyang Zhu; Weidong Zhou; Jun Wang; Hong Yan; Derek C. Johnson
- Web page: https://patentgrep.com/patent/US20200395593A1

## CPC

- H01M 4/0459: {Electrochemical doping, intercalation, occlusion or alloying}
- H01M 4/364: {as mixtures}
- H01M 4/386: {Silicon or alloys based on silicon}
- H01M 4/483: {for non-aqueous cells (H01M4/485 takes precedence)}
- H01M 4/587: for inserting or intercalating light metals
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/058: Construction or manufacture
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Methods and systems are provided for fabricating a large format lithium ion electrochemical cell that includes an anode and a cathode. In one example, the anode is prepared via loading the anode to a predetermined anode loading amount, followed by electrochemical pre-lithiation of the anode via electrically coupling an auxiliary electrode to the anode where lithium is transferred to the anode through an electrolyte solution from the auxiliary electrode. In this way, pre-lithiation of the anode may be improved, which may in turn increase a capacity of the large format lithium ion electrochemical cell.

## Claims

### Claim 1

A method for improving a capacity of a lithium ion battery, the method comprising:
providing a three-electrode system including a cathode, an anode, and an auxiliary electrode;
determining an anode loading amount and loading the anode to the determined anode loading amount; and
pre-lithiating the anode with lithium from the auxiliary electrode, where a pre-lithiation efficiency is based on the anode loading amount.

### Claim 2 (depends on 1)

The method of claim 1, wherein the auxiliary electrode is a lithium metal electrode.

### Claim 3 (depends on 1)

The method of claim 1, wherein the auxiliary electrode is a lithium iron phosphate electrode.

### Claim 4 (depends on 1)

The method of claim 1, wherein the anode is a silicon oxide/graphite anode.

### Claim 5 (depends on 1)

The method of claim 1, wherein the anode is a silicon/graphite anode or a graphite anode.

### Claim 6 (depends on 1)

The method of claim 1, wherein the pre-lithiation efficiency increases as the anode loading amount decreases.

### Claim 7 (depends on 1)

The method of claim 1, further comprising controlling a rate at which the anode is pre-lithiated.

### Claim 8 (depends on 7)

The method of claim 7, wherein controlling the rate includes adjusting a current density for pre-lithiating the anode.

### Claim 9 (depends on 1)

The method of claim 1, further comprising controlling a degree to which the anode is pre-lithiated.

### Claim 10 (depends on 9)

The method of claim 9, wherein controlling the degree includes controlling a duration over which the anode is pre-lithiated.

### Claim 11 (depends on 1)

The method of claim 1, wherein the anode loading amount comprises a loading on opposing sides of a current collector of the anode of greater than or equal to 100 g/m2 or an areal capacity of greater than or equal to 7 mAh/cm2.

### Claim 12 (depends on 1)

The method of claim 1, wherein the anode loading amount comprises a loading on opposing sides of a current collector of the anode of less than or equal to 190 g/m2 or an areal capacity of less than or equal to 13 mAh/cm2.

### Claim 13 (depends on 1)

The method of claim 1, wherein pre-lithiating the anode includes pre-lithiating the anode to a predetermined pre-lithiation percentage, the predetermined pre-lithiation percentage being from 5% to 30%.

### Claim 14 (depends on 1)

The method of claim 1, wherein improving the capacity includes the lithium ion battery having an initial coulombic efficiency of approximately 90%.

### Claim 15 (depends on 1)

The method of claim 1, wherein improving the capacity includes the lithium ion battery having a first discharge capacity under 0.1C greater than 83 ampere hours.

### Claim 16 (depends on 1)

The method of claim 1, wherein improving the capacity includes the lithium ion battery having a second discharge capacity under 0.3C greater than 82 ampere hours.

### Claim 17 (depends on 1)

The method of claim 1, further comprising removing the auxiliary electrode after pre-lithiating the anode.

### Claim 18 (depends on 1)

The method of claim 1, wherein pre-lithiating the anode includes electrochemically pre-lithiating the anode, where lithium ions from the auxiliary electrode migrate through an electrolyte solution to intercalate or alloy with the anode.

### Claim 19

A method for manufacturing a large format electrochemical cell, the method comprising:
providing a three-electrode system including a cathode, an anode, and an auxiliary electrode;
determining an anode loading amount based on a desired design and application of the large format electrochemical cell;
loading the anode to the anode loading amount;
including the cathode, the anode, and the auxiliary electrode in the large format electrochemical cell;
filling the large format electrochemical cell with an electrolyte solution;
electrochemically pre-lithiating the anode to a desired pre-lithiation amount based on the anode loading amount; and
removing the auxiliary electrode and vacuum sealing the large format electrochemical cell including the anode and the cathode.

### Claim 20 (depends on 19)

The method of claim 19, wherein the auxiliary electrode is a lithium metal electrode or a lithium iron phosphate electrode.

### Claim 21 (depends on 19)

The method of claim 19, wherein the anode is a silicon oxide/graphite anode or a silicon/graphite anode.

### Claim 22 (depends on 19)

The method of claim 19, wherein removing the auxiliary electrode includes forming a heat seal to seal the anode and the cathode from the auxiliary electrode, and then cutting the large format electrochemical cell along the heat seal.

### Claim 23 (depends on 19)

The method of claim 19, wherein subsequent to electrochemically pre-lithiating the anode and removing the auxiliary electrode, the anode is not exposed to oxygen or moisture.

### Claim 24 (depends on 19)

The method of claim 19, wherein the anode loading amount is for two opposite sides of a current collector of the anode and the anode loading amount is determined from a range of 100 g/m2 to 190 g/m2 or an areal capacity of 7 mAh/cm2 to 13 mAh/cm2.

### Claim 25 (depends on 19)

The method of claim 19, wherein the desired pre-lithiation amount of the anode is between 5% and 30% pre-lithiation.

### Claim 26 (depends on 19)

The method of claim 19, further comprising controlling a rate and a degree at which the anode is pre-lithiated by controlling a current density and a duration for electrochemically pre-lithiating the anode.

### Claim 27 (depends on 19)

The method of claim 19, wherein electrochemically pre-lithiating the anode includes electrically connecting the anode to the auxiliary electrode.

### Claim 28

A large format electrochemical cell fabricated by a process comprising the steps of:
(a) preparing an anode in a process comprising the steps of:
(i) determining a total anode loading weight for two opposite sides of a current collector of the anode based on a desired design and application of the large format electrochemical cell, wherein determining the total anode loading weight includes selecting an anode weight from a range of 100 g/m2 to 190 g/m2 or an areal capacity of 7 mAh/cm2 to 13 mAh/cm2; and
(ii) loading the anode to the determined total anode loading weight;
(b) providing a cathode and an auxiliary electrode and including the anode, the cathode, and the auxiliary electrode in the large format electrochemical cell;
(c) bathing the cathode, the anode, and the auxiliary electrode in an electrolyte solution;
(d) electrically connecting the anode and the auxiliary electrode to pre-lithiate the anode to a desired level, wherein the desired level of pre-lithiation of the anode is between 5% and 30% pre-lithiation; and
(e) removing the auxiliary electrode and sealing the large format electrochemical cell.

### Claim 29 (depends on 28)

The large format electrochemical cell of claim 28, wherein a rate at which the anode is pre-lithiated to the desired level is controlled by adjusting a current density at which the anode is pre-lithiated.

### Claim 30 (depends on 28)

The large format electrochemical cell of claim 28, wherein removing the auxiliary electrode includes forming a heat seal to melt opposite sides of the large format electrochemical cell together, and then cutting the large format electrochemical cell along the heat seal.

### Claim 31 (depends on 28)

The large format electrochemical cell of claim 28, wherein the desired level of anode pre-lithiation is a function of the determined total anode loading weight.

### Claim 32 (depends on 28)

The large format electrochemical cell of claim 28, wherein the large format electrochemical cell has an energy density of 300 watt-hours/kilogram.

### Claim 33 (depends on 28)

The large format electrochemical cell of claim 28, wherein the large format electrochemical cell has an initial coulombic efficiency of greater than 90%.

### Claim 34 (depends on 28)

The large format electrochemical cell of claim 28, wherein the large format electrochemical cell has a first discharge capacity under 0.1C of greater than 83 ampere hours.

### Claim 35 (depends on 28)

The large format electrochemical cell of claim 28, wherein the large format electrochemical cell has a second discharge capacity under 0.3C of greater than 82 ampere hours.

### Claim 36 (depends on 28)

The large format electrochemical cell of claim 28, wherein the anode is a silicon oxide/graphite anode or a silicon/graphite anode.

### Claim 37 (depends on 28)

The large format electrochemical cell of claim 28, wherein the auxiliary electrode is lithium metal or lithium iron phosphate.