# US 2020/0395583 A1 · Separator for electrochemical cells and method of making the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0395583 A1
- Document ID: US20200395583A1
- Status: Published application
- Kind: A1
- Application number: 16/754,487
- Filed: 2018-10-09
- Published: 2020-12-17
- Earliest claimed: 2017-10-09
- Assignees: Optodot Corporation
- Applicants: Optodot Corporation
- Inventors: Steven A. Carlson; David W. Avison; Benjamin Sloan
- Web page: https://patentgrep.com/patent/US20200395583A1

## CPC

- H01M 10/0562: Solid materials
- H01M 50/446: Composite material consisting of a mixture of organic and inorganic materials
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/0569: characterised by the solvents
- H01M 50/426: Fluorocarbon polymers
- H01M 50/434: Ceramics
- H01M 50/451: comprising layers of only organic material and layers containing inorganic material
- H01M 50/489: Separators, membranes, diaphragms or spacing elements inside the cells, characterised by their physical properties, e.g. swelling degree, hydrophilicity or shut down properties
- H01M 50/491: Porosity
- H01M 50/494: Tensile strength
- H01M 50/581: in response to temperature
- H01M 50/403: Manufacturing processes of separators, membranes or diaphragms
- H01M 2300/0028: characterised by the solvent
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A separator for an electrochemical cell having a porous layer with a blend of a first type of boehmite particles and a second type of boehmite particles and an organic polymer binder, where the first type of boehmite particles is different from the second type of boehmite particles with respect to crystallite particle size and/or composition, and the blend ranges from about 50%-50% by weight of the first and second types of boehmite particles to about 60%-40% by weight of the first and second types of boehmite particles. The separator does not include a polymer separator layer; has a shrinkage of less than 1% when heated at 220° C. for 1 hour; and swells by less than 5% when soaked in propylene carbonate for 1 hour.

## Claims

### Claim at position 1

1-17. (canceled)

### Claim 18

A lithium cell comprising:
an anode,
a cathode,
an organic electrolyte comprising a lithium salt, and
a separator interposed between said anode and said cathode, wherein said separator comprises a first porous layer comprising:
(i) 60 to 95% by weight of particles selected from the group consisting of inorganic oxides and inorganic nitrides; and
(ii) a first organic polymer binder;
wherein said separator:
(i) has a tensile stress of at least 1700 psi and an elongation at break of 15%;
(ii) has a Gurley air permeability number of 600 seconds/100 cc or less when the thickness of said separator is normalized to 20 microns; and
(iii) does not include a polymer separator layer.

### Claim 19 (depends on 18)

The lithium cell of claim 18, wherein said lithium cell shuts down at a temperature of at least 110° C.

### Claim 20 (depends on 18)

The lithium cell of claim 18, wherein said lithium cell has a capacity of 5 Ah or higher and has no cell voltage drop until a temperature of at least 190° C. when tested with an accelerating rate calorimeter (ARC) in a “Heat-Wait-Search” mode in an adiabatic environment.

### Claim 21 (depends on 18)

The lithium cell of claim 18, wherein said lithium cell has a capacity of 3.5 Ah or higher and the temperature measured at the surface of the lithium cell at 100% state of charge does not exceed 100° C. when a 3 mm diameter nail penetrates the cell at a speed of about 8 cm/sec.

### Claim 22 (depends on 18)

The lithium cell of claim 18, wherein said lithium cell has a capacity of 3.5 Ah or higher and the temperature measured at the surface of the lithium cell at 100% state of charge does not exceed 70° C. when a 3 mm nail penetrates the cell at a speed of about 8 c/sec.

### Claim 23 (depends on 18)

The lithium cell of claim 18, wherein said lithium cell has a cycle life at 25° C. of 3,000 cycles or longer with at least an 80% capacity retention when cycled at 1 C charge and 1 C discharge rates at 100% Depth of Discharge (DoD).

### Claim 24 (depends on 18)

The lithium cell of claim 18, wherein the first porous layer comprises a cross-linker.

### Claim 25 (depends on 18)

The lithium cell of claim 18, wherein said separator has a shrinkage of less than 1% when heated at 200° C. for 1 hour.

### Claim 26 (depends on 18)

The lithium cell of claim 18, wherein the inorganic oxides in said first porous layer comprise boehmite particles.

### Claim 27 (depends on 26)

The lithium cell of claim 26, wherein said boehmite particles are hydrophobically-modified boehmite particles.

### Claim 28 (depends on 18)

The lithium cell of claim 18, further comprising:
an edge reinforcement lane on one or more edges of said separator,
wherein said edge reinforcement lane is selected from the group consisting of a compression lane, an edge reinforcement coating lane, and a combination of a compression lane and an edge reinforcement coating lane.

### Claim 29 (depends on 18)

The lithium cell of claim 18, wherein the first porous layer comprises a polyvinylidene fluoride polymer.

### Claim 30 (depends on 18)

The lithium cell of claim 18, wherein said separator has less than 5.0% swelling when soaked in propylene carbonate for 1 hour.

### Claim 31 (depends on 1)

The lithium cell of claim 1, wherein said separator has a tensile stress of at least 2000 psi.

### Claim 32 (depends on 1)

The lithium cell of claim 1, wherein said separator has a Gurley air permeability number of less than 300 seconds/100 cc when the thickness of said separator is normalized to 20 microns.

### Claim 33 (depends on 1)

The lithium cell of claim 1, wherein said separator comprises a second porous layer comprising a second organic polymer binder.

### Claim 34 (depends on 16)

The lithium cell of claim 16, wherein said second organic polymer binder comprises thermally fusible particles.

### Claim 35 (depends on 16)

The lithium cell of claim 16, wherein said thermally fusible particles comprise polymer particles.

### Claim 36

A lithium cell comprising:
an anode,
a cathode,
an organic electrolyte comprising a lithium salt and a flammable organic solvent; and
and a porous free-standing inorganic/organic composite separator that does not comprise a porous plastic substrate,
wherein said lithium cell
has a capacity of about 3.5 Ah or higher, and
the temperature measured at the surface of the lithium cell at a 100% state of charge does not exceed 100° C. when a 3 mm diameter nail penetrates the cell at a speed of about 8 cm/sec.

### Claim 37 (depends on 36)

The lithium cell of claim 36, wherein the temperature measured at the surface of the lithium cell at a 100% state of charge does not exceed 70° C. when a 3 mm diameter nail penetrates the cell at a speed of about 8 cm/sec.

### Claim 38 (depends on 36)

The lithium cell of claim 36, wherein said flammable organic solvent is an organic carbonate.

### Claim 39

A lithium cell comprising:
an anode;
a cathode;
an organic electrolyte comprising a lithium salt and a flammable organic solvent; and
a porous free-standing inorganic/organic composite separator that does not comprise a porous plastic substrate,
wherein said lithium cell has a capacity of 5 Ah or higher and has no self-heating onset until a temperature of at least 150° C. when tested with an accelerating rate calorimeter (ARC) in a “Heat-Wait-Search” mode in an adiabatic environment.

### Claim 40 (depends on 39)

The lithium cell of claim 39, wherein said flammable organic solvent is an organic carbonate.

### Claim 41 (depends on 39)

The lithium cell of claim 39, wherein said lithium cell maintains operation at 150° C. over a period of at least 3 hours when heated to that temperature in said accelerating rate calorimeter (ARC) test.

### Claim 42 (depends on 39)

The lithium cell of claim 39, wherein said lithium battery shuts down at a temperature of at least 150° C.