# US 2020/0395569 A1 · Window member for display device, display device, and manufacturing method for display device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0395569 A1
- Document ID: US20200395569A1
- Status: Published application
- Kind: A1
- Application number: 16/835,301
- Filed: 2020-03-31
- Published: 2020-12-17
- Earliest claimed: 2019-06-14
- Assignees: Samsung Display Co., Ltd.
- Applicants: Samsung Display Co., LTD.
- Inventors: KICHEOL SONG; YOUNGMOON KIM; YOUNGSANG PARK; NARI AHN; Hung Kun AHN; Jung-hun JUNG; OJun KWON; Junsu PARK
- Web page: https://patentgrep.com/patent/US20200395569A1

## CPC

- G06F 1/1652: {the display being flexible, e.g. mimicking a sheet of paper, or rollable}
- G06F 1/1616: {with folding flat displays, e.g. laptop computers or notebooks having a clamshell configuration, with body parts pivoting to an open position around an axis parallel to the plane they define in closed position}
- G06F 3/0412: {Digitisers structurally integrated in a display}
- G06F 3/0443: {using a single layer of sensing electrodes}
- H04M 1/0214: {Foldable telephones, i.e. with body parts pivoting to an open position around an axis parallel to the plane they define in closed position (combined with translation movement H04M1/0235)}
- H04M 1/0268: {including a flexible display panel}
- H10K 59/40: OLEDs integrated with touch screens
- H10K 71/70: Testing, e.g. accelerated lifetime tests
- H10K 77/111: {Flexible substrates}
- G06F 2203/04102: Flexible digitiser, i.e. constructional details for allowing the whole digitising part of a device to be flexed or rolled like a sheet of paper
- H10K 59/87: {Passivation; Containers; Encapsulations}
- H10K 59/8791: {Arrangements for improving contrast, e.g. preventing reflection of ambient light}
- H10K 71/00: Manufacture or treatment specially adapted for the organic devices covered by this subclass
- H10K 2102/311: {Flexible OLED}
- Y02E 10/549: Organic PV cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- G06F: ELECTRIC DIGITAL DATA PROCESSING (computer systems based on specific computational models G06N)
- H04M: TELEPHONIC COMMUNICATION (circuits for controlling other apparatus via a telephone cable and not involving telephone switching apparatus G08)
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A display device includes a display module and a window member disposed on the display module, where the window member includes a base layer and a hard coating layer disposed on the base layer. A moisture absorption ratio of the window member is about 2.2% or greater under a first condition including a first temperature and a first humidity. The first temperature is about 60° C. or greater, and the first humidity is about 70% or greater.

## Claims

### Claim 1

A display device comprising:
a display module; and
a window member disposed on the display module, wherein the window member comprises a base layer and a hard coating layer disposed on the base layer,
wherein a moisture absorption ratio of the window member is about 2.2% or less under a first condition including a first temperature and a first humidity,
wherein the first temperature is about 60° C. or greater, and the first humidity is about 70% or greater.

### Claim 2 (depends on 1)

The display device of claim 1, wherein
the first temperature is about 60° C., and
the first humidity is about 93%.

### Claim 3 (depends on 1)

The display device of claim 1, wherein the moisture absorption ratio is a numerical value measured after maintained for about 2 hours under the first condition.

### Claim 4 (depends on 3)

The display device of claim 3, wherein
the moisture absorption ratio is a value in percentage corresponding to a ratio of a difference between a first weight and a second weight to the first weight of the window member,
wherein the first weight represents a weight of the window member before subjected to the first condition, and
the second weight represents a weight of the window member after maintained for about 2 hours under the first condition.

### Claim 5 (depends on 4)

The display device of claim 4, wherein the first weight represents a weight of the window member after dried under a second condition different from the first condition.

### Claim 6 (depends on 5)

The display device of claim 5, wherein
the second condition includes a second temperature and a second humidity,
wherein the second temperature is about 60° C. is greater, and the second humidity is about 0%.

### Claim 7 (depends on 1)

The display device of claim 1, wherein a Young's modulus of the window member measured under the first condition is about 5 GPa or greater.

### Claim 8 (depends on 7)

The display device of claim 7, wherein a test rate of a tensile test for measuring the Young's modulus is about 5 mm/min.

### Claim 9 (depends on 7)

The display device of claim 7, wherein the Young's modulus is measured in a section in which tensile strain of the window member is in a range of about 0.05% to about 0.5%.

### Claim 10 (depends on 1)

The display device of claim 1, wherein a yield point of the base layer under the first condition is present in a section in which tensile strain of the base layer is about 1.09% or greater.

### Claim 11 (depends on 1)

The display device of claim 1, wherein hardness of the window member is about 0.3 GPa or greater.

### Claim 12 (depends on 11)

The display device of claim 11, wherein the hardness is measured on a surface of the hard coating layer by a Berkovich indenter hardness test.

### Claim 13 (depends on 1)

The display device of claim 1, wherein each of the display module and the window member include a folding area.

### Claim 14

A method for manufacturing a display device, the method comprising:
preparing a window member comprising a base layer and a hard coating layer disposed on the base layer;
preparing a first test sample having same physical properties as the window member;
performing a first test of measuring a moisture absorption ratio of the first test sample under a first condition including a first temperature and a first humidity;
preparing a second test sample having the same physical properties as the window member;
performing a second test of measuring a Young's modulus of the second test sample under the first condition;
preparing a third test sample having the same physical properties as the window member;
performing a third test of measuring a hardness of the third test sample under a second condition different from the first condition; and
coupling the window member to a display module when a predetermined condition is satisfied in at least one test selected from the first to third tests.

### Claim 15 (depends on 14)

The method of claim 14, wherein the performing the first test comprises:
drying the first test sample;
measuring a first weight of the dried first test sample;
maintaining the first test sample for about 2 hours under the first condition;
measuring a second weight of the first test sample; and
determining whether or not a value in percentage corresponding to a ratio of a difference between the first weight and the second weight to the first weight is about 2.2% or less.

### Claim 16 (depends on 14)

The method of claim 14, wherein the performing the second test comprises:
elongating the second test sample;
measuring the Young's modulus of the second test sample; and
determining whether or not the Young's modulus is about 5 GPa or greater,
wherein a tensile rate of a tensile test to elongate the second test sample is about 5 mm/min, and
the Young's modulus is measured in a section in which tensile strain is in a range of about 0.05% to about 0.5%.

### Claim 17 (depends on 14)

The method of claim 14, wherein the performing the third test comprises:
disposing the third test sample on a stage;
measuring the hardness of the third test sample using a Berkovich diamond indenter; and
determining whether or not the hardness is about 0.3 GPa or greater.

### Claim 18

A window member for a display device, the window member comprising:
a base layer; and
a hard coating layer disposed on the base layer,
wherein a moisture absorption ratio of an entirety of the base layer and the hard coating layer is about 2.2% or less under a first condition including a first temperature and a first humidity,
wherein the first temperature is about 60° C., and the first humidity is about 93%.

### Claim 19 (depends on 18)

The window member of claim 18, wherein
the moisture absorption ratio is a value in percentage corresponding to a ratio of a difference between a first weight and a second weight to the first weight of the base layer and the hard coating layer,
wherein the first weight represents a weight of the entirety of the base layer and the hard coating layer before subjected to the first condition, and
the second weight represents a weight of the entirety of the base layer and the hard coating layer after maintained for about 2 hours under the first condition.

### Claim 20 (depends on 18)

The window member of claim 18, wherein
a Young's modulus of the entirety of the base layer and the hard coating layer under the first condition is about 5 GPa or greater,
a yield point of the base layer under the first condition is present in a section in which tensile strain of the base layer is about 1.09% or greater, and
a hardness measured on a surface of the hard coating layer by a Berkovich indenter hardness test is about 0.3 GPa or greater.