# US 2020/0395491 A1 · Graphene-containing membrane, process for producing the same, graphene-containing membrane laminate and photoelectric conversion device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0395491 A1
- Document ID: US20200395491A1
- Status: Published application
- Kind: A1
- Application number: 17/008,706
- Filed: 2020-09-01
- Published: 2020-12-17
- Earliest claimed: 2019-03-05
- Assignees: Kabushiki Kaisha Toshiba; Toshiba Energy Systems & Solutions Corporation
- Applicants: Kabushiki Kaisha Toshiba; Toshiba Energy Systems & Solutions Corporation
- Inventors: Katsuyuki Naito; Naomi Shida; Yutaka Saita
- Web page: https://patentgrep.com/patent/US20200395491A1

## CPC

- H10F 77/244: {made of transparent conductive layers, e.g. transparent conductive oxide [TCO] layers}
- H05B 33/28: of translucent electrodes
- H10F 71/138: {Manufacture of transparent electrodes, e.g. transparent conductive oxides [TCO] or indium tin oxide [ITO] electrodes}
- H10F 77/12: Active materials
- H10F 77/247: {comprising indium tin oxide [ITO]}
- H10K 30/82: Transparent electrodes, e.g. indium tin oxide [ITO] electrodes
- H10K 50/828: Transparent cathodes, e.g. comprising thin metal layers
- H10K 85/1135: {Polyethylene dioxythiophene [PEDOT]; Derivatives thereof}
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- H05B: ELECTRIC HEATING; ELECTRIC LIGHT SOURCES NOT OTHERWISE PROVIDED FOR; CIRCUIT ARRANGEMENTS FOR ELECTRIC LIGHT SOURCES, IN GENERAL
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES

## Abstract

The embodiment provides a graphene-containing membrane producible by wet-coating and excellent in electric properties, a process for producing the membrane, a graphene-containing membrane laminate, and a photoelectric conversion device using the graphene-containing membrane. The graphene-containing membrane contains graphene having a graphene skeleton combined with polyalkyleneimine chains. The membrane has a ratio of the photoelectron intensity at the energy peak position of C1s orbital to that at the bonding energy on an X-ray photoelectron spectrum measured on an ITO film of 288 eV in a range of 5.5 to 20. This membrane can be produced by heating a graphene oxide-containing film in the presence of polyalkyleneimine and further heating the film in the presence of a reducing agent. The graphene-containing membrane can be so installed in a photoelectric conversion device that it is placed between the photoelectric conversion layer and the electrode.

## Claims

### Claim 1

A graphene-containing membrane containing graphene in which polyalkyleneimine chains are connected to the graphene skeleton; which has a ratio of the photoelectron intensity at the energy peak position of C1s orbital to that at the bonding energy on an X-ray photoelectron spectrum measured on an ITO film of 288 eV in a range of 5.5 to 20.

### Claim 2 (depends on 1)

The graphene-containing membrane according to claim 1, wherein said X-ray photoelectron spectrum measured on an ITO film indicates the bonding energy of the peak corresponding to N1s orbital in the range of 399.0 to 399.5 eV.

### Claim 3 (depends on 1)

The graphene-containing membrane according to claim 1, which has a work function of 4 eV or less according to ultraviolet photoelectron spectroscopy measurement.

### Claim 4

A graphene-containing membrane producing process comprising, in this order, the steps of:
(a) adding polyalkyleneimine into an aqueous dispersion of graphene oxide,
(b) adding a reducing agent into the dispersion obtained in the above step (a), and then heating the dispersion, and
(c) coating a substrate with the dispersion obtained in the above step (b).

### Claim 5 (depends on 4)

The process according to claim 4, further comprising the step of:
(b′) washing the dispersed product formed in said step (b) between said steps of (b) and (c).

### Claim 6 (depends on 5)

The process according to claim 5, furthermore comprising the step of:
(b″) dispersing the product obtained in said step (b′) in a low molecular weight alcohol having 1 to 4 carbon atoms, so as to produce a coating solution between said steps of (b′) and (c).

### Claim 7 (depends on 4)

The process according to claim 4, wherein said step (c) is carried out by a bar-coating process comprising the steps of: supplying the dispersion obtained in said step (b) into a gap between said substrate and an applicator, so as to form a meniscus between them; and then sliding said substrate or said applicator.

### Claim 8 (depends on 4)

The process according to claim 4, wherein said reducing agent is hydrazine hydrate.

### Claim 9

A graphene-containing membrane laminate which has a structure comprising a graphene oxide film overlaid on a membrane containing graphene combined with polyalkylene chains.

### Claim 10 (depends on 9)

The graphene-containing membrane laminate according to claim 9, wherein said membrane containing graphene has a ratio of the photoelectron intensity at the energy peak position of C1s orbital to that at the bonding energy on an X-ray photoelectron spectrum measured on an ITO film of 288 eV in a range of 5.5 to 20.

### Claim 11 (depends on 9)

The graphene-containing membrane laminate according to claim 9, which has a work function of 4.5 eV or more according to ultraviolet photoelectron spectroscopy measurement.

### Claim 12

A photoelectric conversion device comprising a negative electrode, a positive electrode, a photoelectric conversion layer provided between said negative electrode and said positive electrode, and a graphene-containing membrane provided between said negative electrode and said photoelectric conversion layer; wherein
said graphene-containing membrane contains graphene in which polyalkyleneimine chains are connected to the graphene skeleton and has a ratio of the photoelectron intensity at the energy peak position of C1s orbital to that at the bonding energy on an X-ray photoelectron spectrum measured on an ITO film of 288 eV in a range of 5.5 to 20.

### Claim 13 (depends on 12)

The device according to claim 12, wherein said X-ray photoelectron spectrum measured on an ITO film indicates the bonding energy corresponding to N1s orbital in the range of 399.0 to 399.5 eV.

### Claim 14 (depends on 12)

The device according to claim 12, wherein said graphene-containing membrane has a work function of 4 eV or less according to ultraviolet photoelectron spectroscopy measurement.

### Claim 15

A photoelectric conversion device comprising a negative electrode, a positive electrode, a photoelectric conversion layer provided between said negative electrodes and said positive electrode, and such a laminate provided between said positive electrode and said photoelectric conversion layer as has a structure comprising a graphene oxide film overlaid on a membrane containing graphene to which polyalkyleneimine chains are connected from the positive electrode side.

### Claim 16 (depends on 15)

The device according to claim 15, wherein said laminate has a work function of 4.5 eV or more according to ultraviolet photoelectron spectroscopy measurement.

### Claim 17 (depends on 15)

The device according to claim 15, wherein said membrane containing graphene has a ratio of the photoelectron intensity at the energy peak position of C1s orbital to that at the bonding energy on an X-ray photoelectron spectrum measured on an ITO film of 288 eV in a range of 5.5 to 20.

### Claim 18 (depends on 12)

The device according to claim 12, wherein at least one of said negative electrode and said positive electrode contains silver.

### Claim 19 (depends on 12)

The device according to claim 12, wherein at least one of said negative electrode and said positive electrode is a transparent electrode containing indium-tin oxide.