- Number: US 2020/0395477 A1
- Document ID: US20200395477A1
- Status: Published application
- Kind: A1
- Application number: 16/441,337
- Filed: 2019-06-14
- Published: 2020-12-17
- Earliest claimed: 2019-06-14
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Kun-Mu Li; Heng-Wen Ting; Yen-Ru Lee; Hsueh-Chang Sung
- Web page: https://patentgrep.com/patent/US20200395477A1

## CPC

- H10D 30/62: Fin field-effect transistors [FinFET]
- H10D 30/024: {of fin field-effect transistors [FinFET]}
- H10D 30/0243: {using dummy structures having essentially the same shapes as the semiconductor bodies, e.g. to provide stability}
- H10D 30/797: {being in source or drain regions, e.g. SiGe source or drain}
- H10D 62/151: {of IGFETs (of IGFETs having LDD or DDD structure H10D30/601; of thin film transistors H10D30/6713)}
- H10D 62/822: comprising only Group IV materials heterojunctions, e.g. Si/Ge heterojunctions
- H10D 64/017: {using dummy gates in processes wherein at least parts of the final gates are self-aligned to the dummy gates, i.e. replacement gate processes}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/6923: {the material being boron or phosphorus doped silicon oxides, e.g. BPSG, BSG or PSG}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method includes forming a semiconductor fin over a substrate, etching the semiconductor fin to form a recess, wherein the recess extends into the substrate, and forming a source/drain region in the recess, wherein forming the source/drain region includes epitaxially growing a first semiconductor material on sidewalls of the recess, wherein the first semiconductor material includes silicon germanium, wherein the first semiconductor material has a first germanium concentration from 10 to 40 atomic percent, epitaxially growing a second semiconductor material over the first semiconductor material, the second semiconductor material including silicon germanium, wherein the second semiconductor material has a second germanium concentration that is greater than the first germanium concentration, and epitaxially growing a third semiconductor material over the second semiconductor material, the third semiconductor material including silicon germanium, wherein the third semiconductor material has a third germanium concentration that is smaller than the second germanium concentration.

## Claims

### Claim 1

A method comprising:
forming a semiconductor fin over a semiconductor substrate;
etching the semiconductor fin to form a recess, wherein the recess extends into the semiconductor substrate; and
forming a source/drain region in the recess, wherein forming the source/drain region comprises:
epitaxially growing a first semiconductor material on sidewalls of the recess, wherein the first semiconductor material comprises silicon germanium, wherein the first semiconductor material has a first germanium concentration from 10 to 40 atomic percent;
epitaxially growing a second semiconductor material over the first semiconductor material, the second semiconductor material comprising silicon germanium, wherein the second semiconductor material has a second germanium concentration that is greater than the first germanium concentration; and
epitaxially growing a third semiconductor material over the second semiconductor material, the third semiconductor material comprising silicon germanium, wherein the third semiconductor material has a third germanium concentration that is smaller than the second germanium concentration.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first semiconductor material comprises boron-doped silicon germanium having a boron concentration between 1×1019 atoms/cm3 and 1×1021 atoms/cm3.

### Claim 3 (depends on 1)

The method of claim 1, wherein the second semiconductor material comprises boron-doped silicon germanium having a germanium concentration from 20 to 80 atomic percent.

### Claim 4 (depends on 1)

The method of claim 1, wherein the first semiconductor material is epitaxially grown having a thickness on the sidewalls of the first recess that is between 1 nm and 10 nm.

### Claim 5 (depends on 1)

The method of claim 1, wherein the recess extends into the substrate a distance between 0 nm and 10 nm.

### Claim 6 (depends on 1)

The method of claim 1, wherein the semiconductor fin comprises silicon germanium.

### Claim 7 (depends on 1)

The method of claim 1, wherein the substrate comprises doped silicon having a boron concentration between 1×1017 atoms/cm3 and 1×1020 atoms/cm3.

### Claim 8

A device comprising:
a fin extending from a substrate, the fin having a top surface that is a first height from a top surface of the substrate;
a gate stack over the fin;
a source/drain region in the fin adjacent the gate stack and in the substrate, wherein a bottom surface of the source/drain region is below the top surface of the substrate and wherein a top surface of the source/drain region is above the top surface of the fin, the source/drain region comprising:
a first source/drain material comprising silicon germanium having a first concentration of germanium and a first concentration of boron;
a second source/drain material over the first source/drain material, the second source/drain comprising silicon germanium having a second concentration of germanium and a second concentration of boron, wherein the second concentration of germanium is greater than the first concentration of germanium and wherein the second concentration of boron is greater than the first concentration of boron; and
a third source/drain material over the second source/drain material, the third source/drain material comprising silicon germanium having a third concentration of germanium and a third concentration of boron.

### Claim 9 (depends on 8)

The device of claim 8, wherein the bottom surface of the source/drain region is at a depth of 0 nm to 10 nm below the top surface of the substrate.

### Claim 10 (depends on 8)

The device of claim 8, wherein the top surface of the fin is at a height of 30 nm to 70 nm above the top surface of the substrate.

### Claim 11 (depends on 8)

The device of claim 8, wherein the fin comprises silicon germanium and the substrate comprises silicon.

### Claim 12 (depends on 11)

The device of claim 11, wherein the fin has a concentration of germanium that is between 10 atomic percent and 50 atomic percent.

### Claim 13 (depends on 8)

The device of claim 8, wherein the first concentration of germanium is between 10 atomic percent and 40 atomic percent.

### Claim 14 (depends on 8)

The device of claim 8, wherein the first concentration of boron is between 1×1019 atoms/cm3 and 1×1021 atoms/cm3.

### Claim 15 (depends on 8)

The device of claim 8, wherein the second concentration of boron is 10 times the first concentration of boron.

### Claim 16

A method comprising:
forming a fin extending from a substrate, the fin having a first height above a surface of the substrate;
etching the fin to form an opening, wherein the opening has a depth that is greater than the first height of the fin; and
forming a source/drain region in the opening, wherein forming the source/drain region comprises:
epitaxially growing a first semiconductor material in the opening, wherein a portion of the first semiconductor material extends below the surface of the substrate, wherein the first semiconductor material comprises doped silicon germanium;
epitaxially growing a second semiconductor material over the first semiconductor material, wherein the first semiconductor material comprises doped silicon germanium having a greater dopant concentration and a greater atomic percent of germanium than the first semiconductor material; and
epitaxially growing a third semiconductor material over the second semiconductor, wherein the third semiconductor material comprises doped silicon germanium having a smaller dopant concentration and a smaller atomic percent of germanium than the second semiconductor material.

### Claim 17 (depends on 16)

The method of claim 16, wherein the depth of the opening is between 0 nm and 10 nm greater than the first height of the fin.

### Claim 18 (depends on 16)

The method of claim 16, wherein epitaxially growing the first semiconductor material comprises growing the first semiconductor material to a thickness that is greater than a difference between the depth of the opening and the first height of the fin.

### Claim 19 (depends on 16)

The method of claim 16, wherein the first semiconductor material comprises between 10 atomic percent and 40 atomic percent germanium and wherein the first semiconductor material has a doping concentration that is between 1×1019 atoms/cm3 and 1×1021 atoms/cm3.

### Claim 20 (depends on 16)

The method of claim 16, wherein the first semiconductor material is doped with boron.