# US 2020/0395462 A1 · Implantation and Annealing for Semiconductor Device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0395462 A1
- Document ID: US20200395462A1
- Status: Published application
- Kind: A1
- Application number: 16/441,487
- Filed: 2019-06-14
- Published: 2020-12-17
- Earliest claimed: 2019-06-14
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Yu-Chang Lin; Tien-Shun Chang; Szu-Ying Chen; Chun-Feng Nieh; Sen-Hong Syue; Huicheng Chang
- Web page: https://patentgrep.com/patent/US20200395462A1

## CPC

- H10D 64/017: {using dummy gates in processes wherein at least parts of the final gates are self-aligned to the dummy gates, i.e. replacement gate processes}
- H10D 30/024: {of fin field-effect transistors [FinFET]}
- H10D 30/62: Fin field-effect transistors [FinFET]
- H10D 64/01324: {characterised by the sectional shape, e.g. T or inverted-T}
- H10D 84/017: {Manufacturing their source or drain regions, e.g. silicided source or drain regions}
- H10D 84/0172: {Manufacturing their gate conductors}
- H10D 84/0193: {the components including FinFETs}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D 84/853: {comprising FinFETs}
- H10P 14/6518: {by introduction of substances into an already-existing insulating layer}
- H10P 30/20: into semiconductor materials, e.g. for doping
- H10P 30/40: into insulating materials
- H10P 95/90: Thermal treatments, e.g. annealing or sintering
- H10D 30/797: {being in source or drain regions, e.g. SiGe source or drain}
- H10D 62/822: comprising only Group IV materials heterojunctions, e.g. Si/Ge heterojunctions
- H10D 64/01352: {with sacrificial oxide}
- H10D 64/021: {using multiple gate spacer layers, e.g. bilayered sidewall spacers}
- H10D 64/518: {characterised by their lengths or sectional shapes}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A semiconductor device, and a method of manufacturing, is provided. A dummy gate is formed on a semiconductor substrate. An interlayer dielectric (ILD) is formed over the semiconductor fin. A dopant is implanted into the ILD. The dummy gate is removed and an anneal is performed on the ILD. The implantation and the anneal lead to an enhancement of channel resistance by a reduction in gate dielectric thickness and to an enlargement of critical dimensions of a metal gate.

## Claims

### Claim 1

A method of manufacturing a device, the method comprising:
forming a dummy gate on a semiconductor substrate;
forming an interlayer dielectric (ILD) over the semiconductor substrate;
implanting a dopant into the ILD;
after implanting the dopant, removing the dummy gate; and
after removing the dummy gate, performing an anneal on the ILD.

### Claim 2 (depends on 1)

The method of claim 1, wherein the implanting is performed at an energy of between about 5 KeV and about 15 KeV.

### Claim 3 (depends on 1)

The method of claim 1, wherein the anneal is performed using N2 as a flow gas.

### Claim 4 (depends on 1)

The method of claim 1, wherein the anneal is performed at a temperature of between about 600° C. and about 800° C.

### Claim 5 (depends on 1)

The method of claim 1, wherein the anneal is performed for a time period between about 100 minutes and 150 minutes.

### Claim 6 (depends on 1)

The method of claim 1, wherein the dopant comprises nitrogen.

### Claim 7 (depends on 6)

The method of claim 6, wherein the implantation is performed such that the concentration of nitrogen in the ILD is between about 1×1018 cm−3 to about 1×1021 cm−3.

### Claim 8 (depends on 6)

The method of claim 6, wherein the implantation and the anneal are performed such that the nitrogen is distributed in the ILD to a depth of between about 5 nm to about 15 nm.

### Claim 9

A method of manufacturing a device, the method comprising:
forming a fin on a substrate;
forming a dummy gate over the fin;
forming a mask on the dummy gate;
forming an interlayer dielectric (ILD) over the fin and mask with a flowable chemical vapor deposition (FCVD);
performing a UV cure on the ILD;
performing a first anneal on the ILD;
leveling the ILD with a top surface of the mask;
performing a second anneal on the ILD;
removing the mask;
leveling the ILD with a top surface of the dummy gate;
performing a nitrogen implantation on the ILD;
removing the dummy gate;
performing a third anneal on the ILD;
forming a gate dielectric in a recess left by removing the dummy gate; and
depositing a gate electrode over the gate dielectric.

### Claim 10 (depends on 9)

The method of claim 9, wherein the nitrogen implantation is performed at an energy of between about 5 KeV and about 15 KeV.

### Claim 11 (depends on 9)

The method of claim 9, wherein the third anneal is performed with N2 at a temperature of below 900° C.

### Claim 12 (depends on 9)

The method of claim 9, wherein the third anneal is performed with N2 for a time period between about 100 minutes and 150 minutes.

### Claim 13 (depends on 9)

The method of claim 9, wherein the nitrogen implantation is performed such that the concentration of nitrogen in the ILD is between about 1×1018 cm−3 to about 1×1021 cm−3.

### Claim 14 (depends on 9)

The method of claim 9, such that performing the nitrogen implantation and the third anneal cause a vertical thickness of the ILD to contract to between about 80% and about 90% of its original vertical thickness.

### Claim 15 (depends on 9)

The method of claim 9, such that performing the nitrogen implantation and the third anneal cause a top width of the gate electrode to be greater than a bottom width of the gate electrode by a ratio of between about 110% and about 115%.

### Claim 16 (depends on 9)

The method of claim 9, wherein the nitrogen implantation and the third anneal are performed such that the nitrogen is distributed in the ILD to a depth of between about 5 nm to about 15 nm.

### Claim at position 17

17-20. (canceled)

### Claim 21

A method of manufacturing a device, the method comprising:
forming a dummy gate structure over a fin, the fin extending from a semiconductor substrate;
depositing a dielectric layer over the dummy gate structure and the fin;
performing a first anneal on the dielectric layer;
implanting nitrogen into the dielectric layer;
removing the dummy gate structure to form a first recess;
after removing the dummy gate structure, performing a second anneal on the dielectric layer; and
forming a gate electrode in the first recess.

### Claim 22 (depends on 21)

The method of claim 21, wherein the dielectric layer has a vertical thickness in a range of 30 nm to 50 nm after the second anneal.

### Claim 23 (depends on 21)

The method of claim 21, wherein after implanting the nitrogen, the dielectric layer has a nitrogen dopant dose of between about 1×1018 cm−3 to about 1×1021 cm−3.

### Claim 24 (depends on 21)

The method of claim 21, wherein the gate electrode has a first width measured across a top surface of the gate electrode, the gate electrode has a second width measured across a bottom surface of the gate electrode, and a ratio of the second width to the first width is in a range of 88% and 97%.