# US 2020/0395220 A1 · Methods of enhancing surface topography on a substrate for inspection

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0395220 A1
- Document ID: US20200395220A1
- Status: Published application
- Kind: A1
- Application number: 17/000,173
- Filed: 2020-08-21
- Published: 2020-12-17
- Earliest claimed: 2017-05-30
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Co., Ltd.
- Inventors: Han-Wen LIAO; Jun-Xiu LIU; Chun-Chih LIN
- Web page: https://patentgrep.com/patent/US20200395220A1

## CPC

- H10P 52/402: {of semiconductor materials}
- H10P 72/0616: {Monitoring of warpages, curvatures, damages, defects or the like}
- H10P 74/203: {Structural properties, e.g. testing or measuring thicknesses, line widths, warpage, bond strengths or physical defects}
- H10P 74/23: {characterised by multiple measurements, corrections, marking or sorting processes}
- H10P 74/235: {comprising optical enhancement of defects or not-directly-visible states}
- H10P 95/062: {involving a dielectric removal step}
- H10W 10/00: Isolation regions in semiconductor bodies between components of integrated devices
- H10W 10/01: {Manufacture or treatment}
- H10W 10/014: {using trench refilling with dielectric materials, e.g. shallow trench isolations}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10P 50/283: {by chemical means}
- H10P 50/644: {Anisotropic liquid etching (H10P50/61 takes precedence)}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

Methods for enhancing a surface topography of a structure formed on a substrate are provided. In one example, the method includes performing a polishing process on a substrate having a shallow trench isolation structure and a diffusion region, performing a surface topography enhancing process to enlarge a defect in at least one of the shallow trench isolation structure and the diffusion region, inspecting at least one of the shallow trench isolation structure and the diffusion region to detect the enlarged defect, and adjusting a parameter of the polishing process in response to detecting the enlarged defect.

## Claims

### Claim 1

A method of manufacturing a structure on a substrate, comprising:
polishing a substrate having a shallow trench isolation structure and a diffusion region;
treating a surface of the substrate to deepen a defect in at least one of the shallow trench isolation structure and the diffusion region;
detecting the deepened defect in at least one of the shallow trench isolation structure and the diffusion region; and
adjusting a polishing process in response to detecting the deepened defect.

### Claim 2 (depends on 1)

The method of claim 1, wherein the treating a surface of the substrate to deepen a defect comprises:
altering a surface profile of a structure on the substrate by immersing the substrate in a liquid solution.

### Claim 3 (depends on 2)

The method of claim 2, wherein the altering a surface profile of a structure on the substrate further comprises treating a surface of the substrate with a plasma.

### Claim 4 (depends on 2)

The method of claim 2, wherein the altering a surface profile of a structure on the substrate includes immersing the substrate in an acid solution comprising at least one of HF, NH4F, buffered HF, ammonium fluoride or ammonium bifluoride in deionized water.

### Claim 5 (depends on 4)

The method of claim 4, wherein the altering a surface profile of a structure on the substrate further comprises immersing the substrate in an alkaline solution comprising at least one of tetramethyl ammonium hydroxide, aqueous potassium hydroxide, sodium hydroxide or aqueous ammonia in deionized water.

### Claim 6 (depends on 5)

The method of claim 5, wherein the defect in at least one of the shallow trench isolation and the diffusion region is a defect in both the shallow trench isolation and the diffusion region.

### Claim 7 (depends on 6)

The method of claim 6, wherein the treating a surface of the substrate to deepen a defect further comprises treating a surface of the substrate with a plasma.

### Claim 8 (depends on 2)

The method of claim 2, wherein the liquid solution is an acid solution comprising at least one of HF, NH4F, buffered HF, ammonium fluoride or ammonium bifluoride in deionized water.

### Claim 9 (depends on 1)

The method of claim 1, wherein the defect in at least one of the shallow trench isolation and the diffusion region is a defect at an interface between the shallow trench isolation and the diffusion region.

### Claim 10 (depends on 1)

The method of claim 1, wherein the defect comprises at least one of micro-scratches, dishing and residuals from the polishing step.

### Claim 11 (depends on 9)

The method of claim 9, wherein the defect is deepened to a shape selected from the group consisting of polygon, pyramids, cylinder, notch, cubic, and angled sidewalls.

### Claim 12 (depends on 1)

The method of claim 1, further comprising:
forming a gate structure or fin structures on the diffusion region of the substrate.

### Claim 13 (depends on 9)

The method of claim 9, wherein the deepened defect has a depth between about 800 Å and about 1600 Å.

### Claim 14

A method of manufacturing a structure on a substrate, comprising:
processing a surface of a substrate having a shallow trench isolation structure and a diffusion region;
deepening a defect caused by the processing a surface of the substrate by a combination of treating the surface with a plasma and altering a surface profile of a structure on the substrate by immersing the substrate in an alkaline or acid solution;
inspecting the structure to detect the deepened defect.

### Claim 15 (depends on 14)

The method of claim 14, wherein the deepening step includes deepening a defect located in the diffusion region, the diffusion region fabricated from a silicon containing material.

### Claim 16 (depends on 15)

The method of claim 15, wherein the silicon containing material is a crystalline silicon material or doped silicon material.

### Claim 17 (depends on 14)

The method of claim 14, wherein the deepening step includes deepening a defect located in the shallow trench isolation structure, the shallow trench isolation structure fabricated from a dielectric material.

### Claim 18

A method for manufacturing a structure on a substrate, comprising:
performing a CMP process on a surface of a substrate having a shallow trench isolation structure and a diffusion region;
dry treating the surface of the substrate to deepen a structure selected from the group consisting of scratches, convex regions, concave regions, dishing defects and erosion defects in at least one of the shallow trench isolation structure or the diffusion region, wherein the structure is deepened between about 20 percent and 60 percent from its original depth; and
inspecting the shallow trench isolation structure or the diffusion region including the deepened structure to detect the deepened structure, the deepened structure having a shape selected from the group consisting of polygon, pyramids, cylinder, notch, cubic, and angled sidewalls.

### Claim 19 (depends on 18)

The method of claim 18, wherein the shallow trench isolation structure is in the substrate.

### Claim 20 (depends on 1)

The method of claim 1, wherein the shallow trench isolation structure is in the substrate.