# US 2020/0393603 A1 · Polarizing Plate, Polarizing Plate-Carrier Film Laminate, Method for Preparing Polarizing Plate-Carrier Film Laminate, Method for Preparing Polarizing Plate, and Active Energy Ray Curable Composition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0393603 A1
- Document ID: US20200393603A1
- Status: Published application
- Kind: A1
- Application number: 16/770,813
- Filed: 2018-12-14
- Published: 2020-12-17
- Earliest claimed: 2017-12-15
- Assignees: LG Chem, Ltd.
- Applicants: LG Chem, Ltd.
- Inventors: Mi So Lee; Yoonkyung Kwon; Jin Woo Kim; Dong Uk Kim
- Web page: https://patentgrep.com/patent/US20200393603A1

## CPC

- G02B 5/305: {including organic materials, e.g. polymeric layers}
- B32B 7/023: Optical properties
- B32B 7/12: using interposed adhesives or interposed materials with bonding properties
- B32B 27/08: of synthetic resin
- B32B 27/18: characterised by the use of special additives
- B32B 27/306: {comprising vinyl acetate or vinyl alcohol (co)polymers}
- B32B 27/36: comprising polyesters
- B32B 27/38: comprising epoxy resins
- B32B 37/10: characterised by the pressing technique, e.g. using action of vacuum or fluid pressure
- B32B 37/12: characterised by using adhesives
- B32B 37/1284: {Application of adhesive}
- B32B 38/10: Removing layers, or parts of layers, mechanically or chemically
- G02B 1/18: Coatings for keeping optical surfaces clean, e.g. hydrophobic or photo-catalytic films (G02B1/16 takes precedence)
- G02B 5/30: Polarising elements (light-modulating devices with active elements G02F1/00)
- G02F 1/133528: {Polarisers}
- B32B 2037/243: {Coating}
- B32B 2255/10: on synthetic resin layer or on natural or synthetic rubber layer
- B32B 2255/24: Organic non-macromolecular coating
- B32B 2255/26: Polymeric coating
- B32B 2305/72: Cured, e.g. vulcanised, cross-linked
- B32B 2307/30: having particular thermal properties
- B32B 2307/40: having particular optical properties
- B32B 2307/42: Polarizing, birefringent, filtering
- B32B 2307/732: Dimensional properties
- B32B 2307/748: Releasability
- B32B 2457/20: Displays, e.g. liquid crystal displays, plasma displays
- B32B 2551/00: Optical elements
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS

## Abstract

A polarizing plate and a polarizing plate-carrier film laminate are provided. A method for manufacturing a polarizing plate-carrier film laminate and a method for manufacturing a polarizing plate using the same polarizing plate-carrier film laminate are also provided. An active energy ray curable composition for a polarizing plate protective layer is also provided.

## Claims

### Claim 1

A polarizing plate comprising:
a polarizer;
a bonding agent layer and a protective film sequentially provided on one surface of the polarizer; and
a protective layer which is directly attached to the other surface of the polarizer,
wherein the protective layer is a resin layer comprising an active energy ray curable composition comprising a bisphenol F-type epoxy compound, an oxetane compound, a polyol compound, and an epoxy compound which does not contain an aromatic ring, or a cured product thereof; and
wherein the active energy ray curable composition includes 15 to 40 parts by weight of the bisphenol F-type epoxy compound, 30 to 80 parts by weight of the oxetane compound, and 1 to 20 parts by weight of the polyol compound based on 100 parts by weight of the epoxy compound which does not contain an aromatic ring.

### Claim 2 (depends on 1)

The polarizing plate of claim 1, wherein a bonding strength (X1) of the protective layer with respect to the polarizer is 4B or more when measured by an ASTM standard cross-cut tape test in accordance with D3359-87.

### Claim 3 (depends on 1)

The polarizing plate of claim 1, wherein an epoxy equivalent weight of the bisphenol F-type epoxy compound is 120 g/eq or more.

### Claim 4 (depends on 1)

The polarizing plate of claim 1, wherein the bisphenol F-type epoxy compound has a viscosity of 2,000 cps to 5,000 cps at 25° C.

### Claim 5 (depends on 1)

The polarizing plate of claim 1, wherein the protective layer has a thickness of 4 μm to 11 μm.

### Claim 6 (depends on 1)

The polarizing plate of claim 1, wherein the active energy ray curable composition has a glass transition temperature of 90° C. or more after curing.

### Claim 7 (depends on 1)

The polarizing plate of claim 1, wherein the polarizer is a polyvinyl alcohol-based film.

### Claim 8 (depends on 1)

A polarizing plate-carrier film laminate comprising:
the polarizing plate according to claim 1; and
a carrier film on a surface opposite to a surface of the protective layer of the polarizing plate which is in contact with the polarizer.

### Claim 9 (depends on 8)

The polarizing plate-carrier film laminate of claim 8, wherein X2 calculated according to the following General Equation 1 is 0.95 to 1:
X2=(Area of the remaining protective layer after the ASTM standard cross-cut tape test)/(Area of the entire peeled surface) [General Equation 1]

### Claim 10 (depends on 8)

The polarizing plate-carrier film laminate of claim 8, wherein a peel strength (X3) of the protective layer with respect to the carrier film is 40 gf/5 cm or less.

### Claim 11

A method for manufacturing a polarizing plate-carrier film laminate, comprising:
supplying a carrier film to a first surface of a polarizer;
supplying a protective film to a second surface of the polarizer;
forming a protective layer by supplying an active energy ray curable composition between the polarizer and the carrier film;
forming a bonding agent layer by supplying a photocurable bonding agent composition between the polarizer and the protective film;
pressurizing a laminate in which the carrier film, the protective layer, the polarizer, the bonding agent layer, and the protective film are sequentially laminated by disposing a pair of pressurization means on each surface of the carrier film and the protective film; and
curing the protective layer and the bonding agent layer by irradiating the protective layer and the bonding agent layer with an active energy ray.

### Claim 12 (depends on 11)

The method of claim 11, wherein the active energy ray curable composition has a viscosity of 50 cps to 200 cps at room temperature.

### Claim 13 (depends on 8)

A method for manufacturing a polarizing plate, comprising: peeling off the carrier film from the protective layer of the polarizing plate-carrier film laminate according to claim 8.

### Claim 14

An active energy ray curable composition for a polarizing plate protective layer, comprising, a bisphenol F-type epoxy compound, an oxetane compound, a polyol compound, and an epoxy compound which does not contain an aromatic ring, and
wherein the active ray curable composition includes 15 to 40 parts by weight of the bisphenol F-type epoxy compound, 30 to 80 parts by weight of the oxetane compound, and 1 to 20 parts by weight of the polyol compound based on 100 parts by weight of the epoxy compound which does not contain an aromatic ring.

### Claim 15 (depends on 1)

The polarizing plate of claim 1, wherein a bonding strength (X1) of the protective layer with respect to the polarizer is 4B to 5B when measured by an ASTM standard cross-cut tape test in accordance with D3359-87.

### Claim 16 (depends on 1)

The polarizing plate of claim 1, wherein an epoxy equivalent weight of the bisphenol F-type epoxy compound is 120 g/eq to 500 g/eq.

### Claim 17 (depends on 1)

The polarizing plate of claim 1, wherein the active energy ray curable composition has a glass transition temperature from 100° C. to 150° C. after curing.