# US 2020/0393400 A1 · Electrochemical Sensor for Detection and Quantification of Heavy Metals

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0393400 A1
- Document ID: US20200393400A1
- Status: Published application
- Kind: A1
- Application number: 16/970,897
- Filed: 2019-02-27
- Published: 2020-12-17
- Earliest claimed: 2018-02-27
- Assignees: University of Massachusetts
- Applicants: University of Massachusetts
- Inventors: Pradeep Unnikrishnan Kurup; Susom Dutta
- Web page: https://patentgrep.com/patent/US20200393400A1

## CPC

- G01N 27/308: {at least partially made of carbon}
- G01N 27/3278: {involving nanosized elements, e.g. nanogaps or nanoparticles (nanopores G01N33/48721; magnetic beads G01N27/745)}
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)

## Abstract

Electrochemical sensors useful for detection of heavy metals are described. The electrochemical sensors can be made by forming a layer of graphene oxide on a working electrode, forming a layer of carbon nanotubes (CNTs) on the layer of graphene oxide, and forming a layer of gold nanostars on the layer of CNTs.

## Claims

### Claim 1

An electrochemical sensor comprising:
a) a working electrode, the working electrode comprising:
i) a graphene oxide layer on the working electrode;
ii) carbon nanotubes (CNTs) disposed on the graphene oxide layer; and
iii) gold nanostars disposed on the CNTs;
b) a reference electrode; and
c) a counter electrode.

### Claim 2 (depends on 1)

The electrochemical sensor of claim 1, wherein the electrochemical sensor has a charge transfer resistance from about 0.2 kiloohm (kΩ) to about 1 kiloohm (kΩ).

### Claim 3 (depends on 1)

The electrochemical sensor of claim 1, wherein the electrochemical sensor has a double layer capacitance from about 2 μF to about 5 μF.

### Claim 4 (depends on 1)

The electrochemical sensor of claim 1, where working electrode comprises carbon paste, glassy carbon, gold, platinum, silver, or indium tin oxide (ITO) glass.

### Claim 5 (depends on 1)

The electrochemical sensor of claim 1, wherein the working electrode comprises carbon paste.

### Claim 6 (depends on 1)

The electrochemical sensor of claim 1, wherein about 80% of the gold nanostars have a diameter from about 15 nm to about 55 nm.

### Claim 7 (depends on 1)

The electrochemical sensor of claim 1, wherein the gold nanostars have spike lengths from about 7 nm to about 33 nm.

### Claim 8

A method of making an electrochemical sensor, the method comprising:
a) providing a substrate comprising a working electrode, a reference electrode, and a counter electrode;
b) forming a layer of graphene oxide on the working electrode;
c) forming a layer of carbon nanotubes (CNTs) on the layer of graphene oxide; and
d) forming a layer of gold nanostars on the layer of CNTs.

### Claim 9 (depends on 8)

The method of claim 8, wherein one or more of the layer of graphene oxide, the layer of CNTs, and the layer of gold nanostars is formed by drop casting.

### Claim 10 (depends on 8)

The method of claim 8, wherein one or more of the layer of graphene oxide, the layer of CNTs, and the layer of gold nanostars is formed by electrodeposition.

### Claim 11 (depends on 8)

The method of claim 8, where the working electrode comprises carbon paste, glassy carbon, gold, platinum, silver, or indium tin oxide (ITO) glass.

### Claim 12 (depends on 8)

The method of claim 8, where working electrode comprises carbon paste.

### Claim 13 (depends on 8)

The method of claim 8, wherein about 80% of the gold nanostars have a diameter from about 20 nm to about 45 nm.

### Claim 14 (depends on 8)

The method of claim 8, wherein the gold nanostars have spike lengths from about 7 nm to about 33 nm.

### Claim 15 (depends on 8)

The method of claim 8, further comprising forming gold nanostars by:
a) providing a chloroauric acid solution;
b) heating the chloroauric acid solution;
c) cooling the heated chloroauric acid solution; and
d) combining the cooled chloroauric with a buffered base.

### Claim 16 (depends on 15)

The method of claim 15, further comprising homogenizing the chloroauric acid solution prior to heating the chloroauric acid solution.

### Claim 17 (depends on 15)

The method of claim 15, wherein the buffered base comprises 4-(2-hydroxyethyl)-1-piperazineethanesulfonic acid (HEPES).

### Claim 18 (depends on 15)

The method of claim 15, wherein the buffered base comprises sodium hydroxide (NaOH).

### Claim 19 (depends on 15)

The method of claim 15, wherein the buffered base comprises 4-(2-hydroxyethyl)-1-piperazineethanesulfonic acid (HEPES) and sodium hydroxide (NaOH).

### Claim 20 (depends on 1)

A method for detecting a heavy metal in a sample by square wave anodic stripping voltammetry, the method comprising:
a) depositing an analyte of interest onto a working electrode by applying a reducing potential;
b) stripping the analyte of interest from the working electrode by applying an oxidizing potential;
c) measuring current at the working electrode as a function of time and as a function of the potential between an auxiliary electrode and a reference electrode while stripping the analyte of interest from the working electrode;
d) varying the potential between the auxiliary electrode and the reference electrode in a square wave pattern with an increasing potential;
wherein the working electrode, reference electrode, and counter electrode form an electrochemical sensor of claim 1.

### Claim at position 21

21-34. (canceled)