# US 2020/0392648 A1 · Fibers fabricated with metals incorporated into grain boundaries for high temperature applications

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0392648 A1
- Document ID: US20200392648A1
- Status: Published application
- Kind: A1
- Application number: 17/000,858
- Filed: 2020-08-24
- Published: 2020-12-17
- Earliest claimed: 2017-06-02
- Assignees: Free Form Fibers, LLC
- Inventors: Erik Garth Vaaler; Marvin S. Keshner; Shay Harrison
- Web page: https://patentgrep.com/patent/US20200392648A1

## CPC

- C04B 35/62281: {based on silicon carbide (C04B35/571 takes precedence)}
- D01F 11/127: {Metals (metal depositing by electrolysis D01F11/16; metal alloys with reinforcing carbon fibres C22C49/14)}
- C04B 35/565: based on silicon carbide
- C04B 35/583: based on boron nitride
- C04B 35/6229: {based on boron nitride}
- C04B 35/62847: {with oxide ceramics}
- C04B 35/62849: {Silica or silicates}
- C04B 35/62884: {by gas phase techniques}
- D01F 9/12: Carbon filaments; Apparatus specially adapted for the manufacture thereof
- D01F 11/16: by physicochemical methods
- D06M 11/83: with metals; with metal-generating compounds, e.g. metal carbonyls; Reduction of metal compounds on textiles
- C04B 2235/3418: Silicon oxide, silicic acids or oxide forming salts thereof, e.g. silica sol, fused silica, silica fume, cristobalite, quartz or flint
- C04B 2235/3826: Silicon carbides
- C04B 2235/386: Boron nitrides
- C04B 2235/421: Boron
- C04B 2235/422: Carbon
- C04B 2235/5264: characterised by the diameter of the fibers
- C04B 2235/663: Oxidative annealing
- C04B 2235/85: Intergranular or grain boundary phases
- D06M 2101/40: Fibres of carbon
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- D01F: CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS
- D06M: TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS, FABRICS, FEATHERS OR FIBROUS GOODS MADE FROM SUCH MATERIALS

## Abstract

A fiber comprises a bulk material comprising: one or more of carbon, silicon, boron, silicon carbide, and boron nitride; and a metal or metal alloy whose affinity for oxygen is greater than that of the bulk material. At least a first portion of the metal or metal alloy is present at the entrance to grain boundaries at the surface of the fiber and within the fiber to a depth of at least 1 micron from the fiber surface. A method of improving a fiber comprises heating a fiber in an inert atmosphere to 900-1300 C for sufficient time to allow at least some of a metal or metal alloy, placed on the fiber, to diffuse and/or flow into and along grain boundaries to a depth of at least 1 micron. The metal or metal alloy has a greater affinity for oxygen than that of the fiber bulk material.

## Claims

### Claim 1

A fiber comprising:
a bulk material comprising one or more materials selected from the group consisting of carbon, silicon, boron, silicon carbide, and boron nitride; and
a metal or metal alloy whose affinity for oxygen is greater than the affinity for oxygen of any of the one or more materials;
wherein at least a first portion of the metal or metal alloy is present at the entrance to grain boundaries at the surface of the fiber and within the fiber to a depth of at least 1 micron from the fiber surface.

### Claim 2 (depends on 1)

The fiber of claim 1,
wherein the metal or metal alloy comprises a metal selected from the group consisting of beryllium, titanium, aluminum, hafnium and zirconium.

### Claim 3 (depends on 1)

The fiber of claim 1,
wherein the metal alloy comprises silicon alloyed with one or more of beryllium, titanium, aluminum, hafnium and zirconium.

### Claim 4 (depends on 1)

The fiber of claim 1, wherein at least a second portion of the metal or metal alloy is present at or near a surface of the fiber in an oxidized form, providing a diffusion barrier that blocks oxygen and nitrogen from entering the fiber through the surface.

### Claim 5 (depends on 4)

The fiber of claim 4, wherein the oxidized form of the second portion of the metal or metal alloy is a metal-silicon oxide

### Claim 6 (depends on 4)

The fiber of claim 4, additionally comprising a layer of silicon at the surface of the fiber, the layer of silicon being positioned between the fiber and the second portion of the metal or metal alloy.

### Claim 7 (depends on 1)

The fiber of claim 1 wherein the metal is present in the bulk material as a dilute impurity, at a concentration of less than 5%.

### Claim 8

A method of improving at least one of the strength, creep resistance, and toughness of a fiber, the method comprising:
adding to a fiber, initially comprising a bulk material having a first affinity for oxygen, a first metal or first metal alloy that has a second affinity for oxygen higher than the first affinity;
wherein the adding comprises:
placing the first metal or first metal alloy on a surface of the fiber; and
in a heating step, heating the fiber in an inert atmosphere to 900-1300 C for sufficient time to allow at least some of the first metal or first metal alloy to diffuse and/or flow from the surface into and along grain boundaries to a depth of at least 1 micron from the fiber surface.

### Claim 9 (depends on 8)

The method of claim 8,
wherein the first metal or first metal alloy comprises a metal selected from the group consisting of beryllium, titanium, aluminum, hafnium and zirconium.

### Claim 10 (depends on 8)

The method of claim 8,
wherein, the first metal alloy comprises silicon alloyed with one or more of beryllium, titanium, aluminum, hafnium and zirconium.

### Claim 11 (depends on 8)

The method of claim 8, additionally comprising:
if any portion of the first metal or first metal alloy remains on the surface of the fiber after the heating step, carrying out a first oxidation step comprising heating the fiber to 800-1200 C in an atmosphere containing oxygen to convert the portion of the first metal or first metal alloy remaining on the surface of the fiber to a first metal oxide or a first metal-silicon oxide.

### Claim 12 (depends on 8)

The method of claim 8, wherein the first metal alloy comprises a metal-silicon alloy.

### Claim 13 (depends on 8)

The method of claim 8, additionally comprising:
after the heating step, depositing a second metal or second metal-alloy on the surface of the fiber; and
after the deposition of the second metal or second metal alloy, in a second oxidation step, heating the fiber to 800-1200 C in an atmosphere containing oxygen to convert the second metal or second metal alloy to a second metal or metal alloy oxide;
wherein, if a second metal-alloy is deposited, the alloy comprises silicon alloyed with one or more of beryllium, titanium, aluminum, hafnium and zirconium.

### Claim 14 (depends on 8)

The method of claim 8, wherein a standard gas mixture used to grow the fiber with a chemical vapor deposition (CVD) process, prior to the addition of the first metal, is modified by adding a gaseous precursor of the first metal, such that atoms of the metal are distributed throughout the bulk material of the fiber as a dilute impurity, at a concentration of less than 5% relative to the bulk material of the fiber.

### Claim 15 (depends on 14)

The method of claim 14, wherein the first metal comprises beryllium, and wherein adding the first metal comprises adding a beryllium precursor during the CVD process, such that beryllium is incorporated within the bulk material of the fiber.

### Claim 16 (depends on 15)

The method of claim 15 wherein the beryllium precursor is selected from the group consisting of BeCl2, BeF2 and dimethylberyllium

### Claim 17 (depends on 13)

The method of claim 13,
wherein the fiber is intended to be operated in a temperature range bounded by room temperature and a maximum operating temperature; and
wherein the second oxidation step is carried out at a temperature between room temperature and the maximum operating temperature, selected such that the second metal oxide or second metal alloy oxide produced has a tensile strain at room temperature lower than the tensile yield strength of the second metal oxide or second metal alloy oxide, and has a compressive strain at the maximum operating temperature lower than the compressive yield strength of the second metal oxide or second metal alloy oxide.

### Claim 18 (depends on 11)

The method of claim 11,
wherein the fiber is intended to be operated in a temperature range bounded by room temperature and a maximum operating temperature; and
wherein the second oxidation step is carried out at a temperature between room temperature and the maximum operating temperature, selected such that the first metal oxide or first metal alloy oxide produced has a tensile strain at room temperature lower than the tensile yield strength of the first metal oxide or first metal alloy oxide, and has a compressive strain at the maximum operating temperature lower than the compressive yield strength of the first metal oxide or first metal alloy oxide.

### Claim 19 (depends on 8)

The method of claim 8,
wherein the added metal or metal alloy is a metal-silicon alloy;
wherein the fiber is characterized by a first coefficient of thermal expansion; and
wherein the relative proportions of the metal elements and the silicon in the metal-silicon alloy are adjusted such that the metal-silicon oxide produced after oxidation is characterized by a second coefficient of thermal expansion within 2 ppm/C of the first coefficient of thermal expansion.

### Claim 20

A method of improving at least one of the strength, creep resistance, and toughness of a fiber, the method comprising:
adding to a fiber, initially comprising a bulk material having a first affinity for oxygen, a coating layer of silicon, having an inner surface in contact with the fiber, and an outer surface roughly concentric with the inner surface; and
adding a first metal or first metal alloy that has a second affinity for oxygen higher than the first affinity;
wherein the adding comprises:
placing the first metal or first metal alloy on the outer surface of the silicon coating layer; and
in a heating step, heating the fiber in an inert atmosphere to 900-1300 C for sufficient time to allow at least some of the first metal or first metal alloy to diffuse and/or flow from the outer surface of the silicon coating layer into and along grain boundaries to a depth of at least 1 micron below the inner surface of the silicon coating layer.