# US 2020/0392610 A1 · High-strength cold rolled steel sheet and method for manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0392610 A1
- Document ID: US20200392610A1
- Status: Published application
- Kind: A1
- Application number: 16/957,105
- Filed: 2018-12-13
- Published: 2020-12-17
- Earliest claimed: 2017-12-26
- Assignees: Jfe Steel Corporation
- Applicants: Jfe Steel Corporation
- Inventors: Takaaki TANAKA; Yuki TOJI
- Web page: https://patentgrep.com/patent/US20200392610A1

## CPC

- C22C 38/02: containing silicon
- C22C 38/54: with boron
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 8/0226: {Hot rolling}
- C21D 8/0236: {Cold rolling}
- C21D 8/0263: {following hot rolling}
- C21D 9/46: for sheet metals
- C22C 18/00: Alloys based on zinc
- C22C 18/04: with aluminium as the next major constituent
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/005: {containing rare earths, i.e. Sc, Y, Lanthanides}
- C22C 38/008: {containing tin}
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/42: with copper
- C22C 38/44: with molybdenum or tungsten
- C22C 38/46: with vanadium
- C22C 38/50: with titanium or zirconium
- C23C 2/02: Pretreatment of the material to be coated, e.g. for coating on selected surface areas (C23C2/30 takes precedence)
- C23C 2/0224: {Two or more thermal pretreatments}
- C23C 2/024: {by cleaning or etching}
- C23C 2/06: Zinc or cadmium or alloys based thereon
- C23C 2/28: Thermal after-treatment, e.g. treatment in oil bath
- C23C 2/40: Plates; Strips
- C21D 2211/001: Austenite
- C21D 2211/005: Ferrite
- C21D 2211/008: Martensite
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

Provided are a high-strength cold rolled steel sheet that has a tensile strength of 980 MPa or more, excellent ductility, and a low failure rate in a hole expanding test, and a method for manufacturing the same. A high-strength cold rolled steel sheet comprises a predetermined composition, wherein a total area ratio of ferrite and bainitic ferrite is 20% to 80%, an area ratio of retained austenite (RA) is more than 10% and 40% or less, an area ratio of tempered martensite is more than 0% and 50% or less, a ratio of RA with an aspect ratio of 0.5 or less is 75% or more, a ratio of RA with an aspect ratio of 0.5 or less in ferrite grain boundaries is 50% or more, and an average KAM value of bcc phase is 1° or less.

## Claims

### Claim at position 1

-5. (canceled)

### Claim 6

A high-strength cold rolled steel sheet comprising:
a composition containing, in mass %,
C: more than 0.15% and 0.45% or less,
Si: 0.5% or more and 2.5% or less,
Mn: 1.5% or more and 3.0% or less,
P: 0.05% or less,
S: 0.01% or less,
Al: 0.01% or more and 0.1% or less, and
N: 0.01% or less,
with a balance consisting of Fe and inevitable impurities; and
a microstructure in which:
a total area ratio of ferrite and bainitic ferrite is 20% or more and 80% or less;
an area ratio of retained austenite is more than 10% and 40% or less;
an area ratio of tempered martensite is more than 0% and 50% or less;
a ratio of retained austenite with an aspect ratio of 0.5 or less to the retained austenite is 75% or more in area ratio;
a ratio of retained austenite with an aspect ratio of 0.5 or less existing in ferrite grain boundaries with an orientation difference of 40° or more to the retained austenite with an aspect ratio of 0.5 or less is 50% or more in area ratio; and
an average KAM value of bcc phase is 1° or less.

### Claim 7 (depends on 6)

The high-strength cold rolled steel sheet according to claim 6, wherein the composition further contains, in mass %, at least one selected from the group consisting of
Ti: 0.005% or more and 0.035% or less,
Nb: 0.005% or more and 0.035% or less,
V: 0.005% or more and 0.035% or less,
Mo: 0.005% or more and 0.035% or less,
B: 0.0003% or more and 0.01% or less,
Cr: 0.05% or more and 1.0% or less,
Ni: 0.05% or more and 1.0% or less,
Cu: 0.05% or more and 1.0% or less,
Sb: 0.002% or more and 0.05% or less,
Sn: 0.002% or more and 0.05% or less,
Ca: 0.0005% or more and 0.005% or less,
Mg: 0.0005% or more and 0.005% or less, and
REM: 0.0005% or more and 0.005% or less.

### Claim 8 (depends on 6)

The high-strength cold rolled steel sheet according to claim 6, comprising
a coated or plated layer at a surface thereof.

### Claim 9 (depends on 7)

The high-strength cold rolled steel sheet according to claim 7, comprising
a coated or plated layer at a surface thereof.

### Claim 10 (depends on 6)

A method for manufacturing the high-strength cold rolled steel sheet according to claim 6, the method comprising:
hot rolling a steel material having the composition according to claim 6, to obtain a hot rolled steel sheet;
pickling the hot rolled steel sheet;
cold rolling the hot rolled steel sheet that has been pickled at a rolling reduction of 30% or more, to obtain a cold rolled steel sheet;
heating the cold rolled steel sheet at an annealing temperature T1 of Ac3 point or more and 950° C. or less, cooling the cold rolled steel sheet from the annealing temperature T1 to a cooling stop temperature T2 of 250° C. or more and less than 350° C. at an average cooling rate of more than 10° C./sec, and holding the cold rolled steel sheet at the cooling stop temperature T2 for 10 sec or more, to obtain a first cold rolled and annealed sheet;
heating the first cold rolled and annealed sheet at an annealing temperature T3 of 700° C. or more and 850° C. or less, cooling the first cold rolled and annealed sheet from the annealing temperature T3 to a cooling stop temperature T4 of 300° C. or more and 550° C. or less, holding the first cold rolled and annealed sheet at the cooling stop temperature T4 for 10 sec or more, and cooling the first cold rolled and annealed sheet to a room temperature, to obtain a second cold rolled and annealed sheet; and
heating the second cold rolled and annealed sheet at an annealing temperature T5 of 100° C. or more and 550° C. or less, to obtain a third cold rolled and annealed sheet.

### Claim 11 (depends on 7)

A method for manufacturing the high-strength cold rolled steel sheet according to claim 7, the method comprising:
hot rolling a steel material having the composition according to claim 7, to obtain a hot rolled steel sheet;
pickling the hot rolled steel sheet;
cold rolling the hot rolled steel sheet that has been pickled at a rolling reduction of 30% or more, to obtain a cold rolled steel sheet;
heating the cold rolled steel sheet at an annealing temperature T1 of Ac3 point or more and 950° C. or less, cooling the cold rolled steel sheet from the annealing temperature T1 to a cooling stop temperature T2 of 250° C. or more and less than 350° C. at an average cooling rate of more than 10° C./sec, and holding the cold rolled steel sheet at the cooling stop temperature T2 for 10 sec or more, to obtain a first cold rolled and annealed sheet;
heating the first cold rolled and annealed sheet at an annealing temperature T3 of 700° C. or more and 850° C. or less, cooling the first cold rolled and annealed sheet from the annealing temperature T3 to a cooling stop temperature T4 of 300° C. or more and 550° C. or less, holding the first cold rolled and annealed sheet at the cooling stop temperature T4 for 10 sec or more, and cooling the first cold rolled and annealed sheet to a room temperature, to obtain a second cold rolled and annealed sheet; and
heating the second cold rolled and annealed sheet at an annealing temperature T5 of 100° C. or more and 550° C. or less, to obtain a third cold rolled and annealed sheet.

### Claim 12 (depends on 10)

The method for manufacturing the high-strength cold rolled steel sheet according to claim 10, further comprising
subjecting the second cold rolled and annealed sheet or the third cold rolled and annealed sheet to a coating or plating treatment.

### Claim 13 (depends on 11)

The method for manufacturing the high-strength cold rolled steel sheet according to claim 11, further comprising
subjecting the second cold rolled and annealed sheet or the third cold rolled and annealed sheet to a coating or plating treatment.