# US 2020/0392604 A1 · Improved pyrorefining process

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0392604 A1
- Document ID: US20200392604A1
- Status: Published application
- Kind: A1
- Application number: 16/771,404
- Filed: 2018-12-11
- Published: 2020-12-17
- Earliest claimed: 2017-12-14
- Assignees: Metallo Belgium
- Applicants: Metallo Belgium
- Inventors: Bert Coletti; Jan Dirk A. Goris; Yves De Visscher; Charles Geenen; Walter Guns; Niko Mollen; Steven Smets; Andy Breugelmans
- Web page: https://patentgrep.com/patent/US20200392604A1

## CPC

- C22B 25/02: by dry processes
- B23K 35/268: {Pb as the principal constituent}
- C22B 5/02: Dry methods {smelting of sulfides or formation of mattes}
- C22B 7/04: Working-up slag
- C22B 13/025: {Recovery from waste materials}
- C22B 15/0054: {Slag, slime, speiss, or dross treating}
- C22B 15/0056: {Scrap treating}
- C22C 1/06: with the use of special agents for refining or deoxidising
- C22C 3/005: {Separation of the constituents of alloys}
- C22C 9/00: Alloys based on copper
- C22C 11/06: with tin as the next major constituent
- Y02P 10/20: Recycling
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A disclosed process produces at least one concentrated copper product together with at least one crude solder product, starting from a black copper composition with at least 50% of copper together with at least 1.0% wt of tin and at least 1.0% wt of lead The process includes the step of partially oxidizing the black copper thereby forming a first copper refining slag, followed by partially reducing the first copper refining slag to form a first lead-tin based metal composition and a first spent slag. The total feed to the reducing step includes an amount of copper that is at least 1.5 times as high as the sum of the amounts of Sn plus Pb present, and the first spent slag includes at most 20% wt total of copper, tin and lead together.

## Claims

### Claim 1

A process for the production of a first lead-tin based metal composition, comprising the following steps:
a) providing a black copper composition comprising at least 50% wt of copper together with at least 1.0% wt of tin and at least 1.0% wt of lead,
b) partially oxidizing the black copper composition, thereby forming a first enriched copper metal phase and a first copper refining slag, both occurring as liquid molten phases [for support, see Page 30, lines 8-12], followed by separating the first copper refining slag from the first enriched copper metal phase,
c) partially reducing the first copper refining slag thereby forming a first lead-tin based metal composition and a first spent slag, both occurring as liquid molten phases [see Page 30, lines 8-12], followed by separating the first spent slag from the first lead-tin based metal composition, the latter forming the basis for a first liquid bath,
whereby the total feed to step c) comprises an amount of copper that is at least 1.5 times as high as the sum of Sn plus Pb present, and
whereby the first spent slag comprises at most 20% wt total of copper, tin and lead together.

### Claim at position 2

2-13. (canceled)

### Claim 14 (depends on 1)

The process according to claim 1, further comprising the following step:
d) partially oxidizing the first liquid bath, thereby forming a first dilute copper metal composition and a first solder refining slag, followed by separating the first solder refining slag from the first dilute copper metal composition.

### Claim 15 (depends on 14)

The process according to claim 14 further comprising the following step:
e) partially reducing the first solder refining slag, thereby forming a first crude solder metal composition and a second solder refining slag, followed by separating the second solder refining slag from the first crude solder metal composition.

### Claim 16 (depends on 15)

The process according to claim 15 further comprising the following step:
f) partially reducing the second solder refining slag, thereby forming a second lead-tin based metal composition and a second spent slag, followed by separating the second spent slag from the second lead-tin based metal composition.

### Claim at position 6

17-24. (canceled)

### Claim 25 (depends on 1)

The process according to claim 1, further comprising the following step:
h) partially oxidizing the first enriched copper metal phase, thereby forming a second enriched copper metal phase and a second copper refining slag, followed by separating the second copper refining slag from the second enriched copper metal phase.

### Claim 26 (depends on 25)

The process according to claim 25 further comprising the following step:
i) at least one of adding at least a part of the second copper refining slag to the first liquid bath and adding at least a part of the second copper refining slag to step d).

### Claim 27 (depends on 25)

The process according to claim 25 further comprising the following steps:
j) partially oxidizing the second enriched copper metal phase, thereby forming a third enriched copper metal phase and a third copper refining slag, followed by separating the third copper refining slag from the third enriched copper metal phase,
k) at least one of adding at least a part of the third copper refining slag to the first dilute copper metal composition, thereby forming a second liquid bath and adding at least a part of the third copper refining slag to step 1);
l) partially oxidizing (800) the second liquid bath (550), thereby forming a first high-copper metal composition (22) and a third solder refining slag (23), followed by separating the third solder refining slag (23) from the first high-copper metal composition (22).

### Claim 28 (depends on 27)

The process according to claim 27 further comprising the following step:
m) partially reducing the third solder refining slag, thereby forming a second dilute copper metal composition and a fourth solder refining slag, followed by separating the fourth solder refining slag from the second dilute copper metal composition.

### Claim 29 (depends on 28)

The process according to claim 28 further comprising the following step:
n) partially reducing the fourth solder refining slag, thereby forming a second crude solder metal composition and a fifth solder refining slag, followed by separating the second crude solder metal composition from the fifth solder refining slag.

### Claim 30 (depends on 29)

The process according to claim 29 further comprising the following step:
o) partially reducing the fifth solder refining slag, thereby forming a third lead-tin based metal composition and a third spent slag, followed by separating the third spent slag from the third lead-tin based metal composition.

### Claim at position 13

31-44. (canceled)

### Claim 45 (depends on 1)

The process according to claim 1, in which a black copper is added to at least one of steps b), f) and o), wherein the black copper is produced by a smelter step.

### Claim 46 (depends on 15)

The process according to claim 15, wherein at least one of the first crude solder metal composition and the second crude solder metal composition is pre-refined using silicon metal to produce a pre-refined solder metal composition.

### Claim 47 (depends on 1)

The process according to claim 1, further comprising the step of cooling at least one material selected from the first crude solder metal composition, the second crude solder metal composition and the pre-refined solder metal composition down to a temperature of at most 825° C. to produce a bath containing a first supernatant dross which by gravity becomes floating upon a first liquid molten tuned solder phase.

### Claim 48 (depends on 15)

The process according to claim 15, further comprising the step of adding at least one compound selected from an alkali metal, an earth alkali metal, and chemical compounds comprising at least one of an alkali metal and an earth alkali metal, to at least one material selected from the first crude solder metal composition, the second crude solder metal composition to the pre-refined solder metal composition, and the first liquid molten tuned solder phase to form a bath containing a second supernatant dross which by gravity comes floating on top of a second liquid molten tuned solder phase.

### Claim 49 (depends on 48)

The process according to claim 48, further comprising the step of removing the second supernatant dross from the second liquid molten tuned solder phase, thereby forming a second tuned solder.

### Claim 50 (depends on 47)

The process according to claim 47, further comprising the step of removing the first supernatant dross from the first liquid molten tuned solder phase, thereby forming a first tuned solder.

### Claim 51 (depends on 49)

The process according to claim 49, further comprising the step of distilling at least one material selected from the first tuned solder and the second tuned solder, wherein lead (Pb) is removed from the solder by evaporation and a distillation overhead product and a distillation bottom product are obtained.

### Claim at position 21

52-53. (canceled)

### Claim 54 (depends on 47)

The process according to claim 47, further comprising the step of adding at least one compound selected from an alkali metal, an earth alkali metal, and chemical compounds comprising at least one of an alkali metal and an earth alkali metal, to at least one material selected from the first crude solder metal composition, the second crude solder metal composition to the pre-refined solder metal composition, and the first liquid molten tuned solder phase to form a bath containing a second supernatant dross which by gravity comes floating on top of a second liquid molten tuned solder phase.