# US 2020/0392601 A1 · Treated Geothermal Brine Compositions With Reduced Concentrations Of Silica, Iron and Manganese

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0392601 A1
- Document ID: US20200392601A1
- Status: Published application
- Kind: A1
- Application number: 16/880,266
- Filed: 2020-05-21
- Published: 2020-12-17
- Earliest claimed: 2009-06-24
- Assignees: Terralithium LLC
- Applicants: Terralithium LLC
- Inventors: Stephen Harrison; John Burba, III
- Web page: https://patentgrep.com/patent/US20200392601A1

## CPC

- C22B 3/20: Treatment or purification of solutions, e.g. obtained by leaching (C22B3/18 takes precedence)
- C02F 9/00: Multistage treatment of water, waste water or sewage
- C09K 8/00: Compositions for drilling of boreholes or wells; Compositions for treating boreholes or wells, e.g. for completion or for remedial operations
- C22B 7/006: {Wet processes}
- C22B 13/04: {by wet processes}
- C22B 19/20: Obtaining zinc otherwise than by distilling
- C22B 26/10: Obtaining alkali metals
- C22B 26/12: Obtaining lithium
- C02F 1/26: by extraction
- C02F 1/281: {using inorganic sorbents}
- C02F 1/42: by ion-exchange (ion-exchange in general B01J)
- C02F 1/5245: {using basic salts, e.g. of aluminium and iron}
- C02F 1/56: Macromolecular compounds
- C02F 1/66: by neutralisation; pH adjustment (for degassing C02F1/20; using ion-exchange C02F1/42; for flocculation or precipitation of suspended impurities C02F1/52; for removing dissolved compounds C02F1/58)
- C02F 1/74: with air (aeration of stretches of water C02F7/00)
- C02F 5/00: Softening water; Preventing scale; Adding scale preventatives or scale removers to water, e.g. adding sequestering agents (softening using ion-exchange C02F1/42)
- C02F 2001/5218: {Crystallization}
- C02F 2101/10: Inorganic compounds
- C02F 2101/203: {Iron or iron compound}
- C02F 2103/06: Contaminated groundwater or leachate
- C02F 2103/08: Seawater, e.g. for desalination
- C02F 2103/10: from quarries or from mining activities
- C02F 2209/02: Temperature
- C02F 2209/06: pH
- Y02P 10/20: Recycling
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- C02F: TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE (separation in general B01D; special arrangements on waterborne vessels of installations for treating water, waste water or sewage, e.g. for producing fresh water, B63J; adding materials to water to prevent corrosion C23F; treating radioactively-contaminated liquids G21F9/04; regeneration of reactants for recirculation into processes, see the relevant places for the processes)
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

This invention relates to treated geothermal brine compositions containing reduced concentrations of iron, silica, and manganese compared to the untreated brines. Exemplary compositions contain a concentration of manganese less than 10 mg/kg, a concentration of silica ranging from less than 10 mg/kg, and a concentration of iron less than 10 mg/kg, and the treated geothermal brine is derived from a Salton Sea geothermal reservoir.

## Claims

### Claim at position 1

1-20. (canceled)

### Claim 21

An aqueous treated geothermal brine composition, the composition comprising dissolved manganese, dissolved silica, and dissolved iron, wherein the dissolved manganese has a concentration greater than zero and no more than 200 mg/kg, the dissolved silica has a concentration of 0 mg/kg to 80 mg/kg, and the dissolved iron has a concentration of 0 mg/kg to 300 mg/kg.

### Claim 22 (depends on 21)

The aqueous treated geothermal brine composition of claim 21, wherein the concentration of the dissolved manganese is no more than 200 mg/kg, the concentration of the dissolved silica is no more than 30 mg/kg, and the concentration of the dissolved iron is no more than 300 mg/kg.

### Claim 23 (depends on 21)

The aqueous treated geothermal brine composition of claim 21, wherein the concentration of the dissolved manganese is less than 100 mg/kg, the concentration of the dissolved silica is less than 30 mg/kg, and the concentration of the dissolved iron is less than 300 mg/kg.

### Claim 24 (depends on 21)

The aqueous treated geothermal brine composition of claim 21, wherein the concentration of the dissolved manganese is less than 50 mg/kg, the concentration of the dissolved silica is less than 30 mg/kg, and the concentration of the dissolved iron is less than 300 mg/kg.

### Claim 25 (depends on 21)

The aqueous treated geothermal brine composition of claim 21, wherein the concentration of the dissolved manganese is less than 20 mg/kg, the concentration of the dissolved silica is less than 20 mg/kg, and the concentration of the dissolved iron is less than 100 mg/kg.

### Claim 26 (depends on 21)

The aqueous treated geothermal brine composition of claim 21, wherein the concentration of the dissolved manganese is less than 20 mg/kg, the concentration of the dissolved silica is less than 20 mg/kg, and the concentration of the dissolved iron is less than 50 mg/kg.

### Claim 27 (depends on 21)

The aqueous treated geothermal brine composition of claim 21, wherein the concentration of the dissolved manganese is less than 10 mg/kg, the concentration of the dissolved silica is less than 10 mg/kg, and the concentration of the dissolved iron is less than 100 mg/kg.

### Claim 28 (depends on 21)

The aqueous treated geothermal brine composition of claim 21, wherein the concentration of the dissolved manganese is less than 10 mg/kg, the concentration of the dissolved silica is less than 10 mg/kg, and the concentration of the dissolved iron is less than 10 mg/kg.

### Claim 29 (depends on 21)

The aqueous treated geothermal brine composition of claim 21, wherein the concentration of the dissolved manganese is less than 5 mg/kg, the concentration of the dissolved silica is less than 5 mg/kg, and the concentration of the dissolved iron is less than 5 mg/kg.

### Claim 30 (depends on 21)

The aqueous treated geothermal brine composition of claim 21, wherein the aqueous treated geothermal brine is a Salton Sea brine.

### Claim 31 (depends on 21)

The aqueous treated geothermal brine composition of claim 21, further comprising sodium in a concentration of at least 50,000 mg/kg and potassium in a concentration of at least 9,000 mg/kg.

### Claim 32

A treated geothermal brine composition comprising dissolved manganese, dissolved silica, and dissolved iron, wherein the dissolved manganese has a concentration greater than zero and no more than 100 mg/kg, the dissolved silica has a concentration of 0 mg/kg to 30 mg/kg, and the dissolved iron has a concentration of 0 mg/kg to 300 mg/kg, and wherein the treated geothermal brine is a treated Salton Sea geothermal brine.

### Claim 33 (depends on 32)

The treated geothermal brine composition of claim 32, wherein the concentration of the dissolved manganese is less than 20 mg/kg, the concentration of the dissolved silica is less than 20 mg/kg, and the concentration of the dissolved iron is less than 200 mg/kg.

### Claim 34 (depends on 32)

The treated geothermal brine composition of claim 32, wherein the dissolved manganese has a concentration of less than 10 mg/kg, the dissolved silica has a concentration of less than 10 mg/kg, and the dissolved iron has a concentration of less than 10 mg/kg.

### Claim 35 (depends on 32)

The treated geothermal brine composition of claim 32, further comprising sodium in a concentration of at least 50,000 mg/kg and potassium in a concentration of at least 9,000 mg/kg.

### Claim 36

A method of using an aqueous treated geothermal brine composition, the method comprising:
providing an aqueous treated geothermal brine comprising a concentration of dissolved manganese greater than zero and no more than 200 mg/kg, a concentration of dissolved silica of 0 mg/kg to 80 mg/kg, and a concentration of dissolved iron of 0 mg/kg to 300 mg/kg; and
at least one of: (i) providing the aqueous treated geothermal brine composition to a process for mineral extraction or (ii) injecting the aqueous treated geothermal brine composition into a geothermal reservoir.

### Claim 37 (depends on 36)

The method of claim 36, wherein the concentration of dissolved manganese is less than 100 mg/kg, the concentration of dissolved silica is less than 30 mg/kg, and the concentration of dissolved iron is less than 300 mg/kg.

### Claim 38 (depends on 36)

The method of claim 36, wherein the concentration of dissolved manganese is less than 100 mg/kg, the concentration of dissolved silica is less than 30 mg/kg, and the concentration of dissolved iron is less than 100 mg/kg.

### Claim 39 (depends on 36)

The method of claim 36, wherein the process for mineral extraction comprises extracting at least one of lithium, zinc, lead, potassium, rubidium, cesium, or a phosphate from the aqueous treated geothermal brine.

### Claim 40 (depends on 36)

The method of claim 36, wherein the treated geothermal brine is a treated Salton Sea geothermal brine.