# US 2020/0392331 A1 · Polycarbonate copolymer blends, articles formed therefrom, and methods of manufacture

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0392331 A1
- Document ID: US20200392331A1
- Status: Published application
- Kind: A1
- Application number: 16/971,398
- Filed: 2019-02-21
- Published: 2020-12-17
- Earliest claimed: 2018-02-21
- Assignees: Sabic Global Technologies B.V.
- Applicants: Sabic Global Technologies B.V.
- Inventors: Paul Dean Sybert; Norimitsu Yamaguchi; Jacob Lee Oberholtzer; James Alan Mahood
- Web page: https://patentgrep.com/patent/US20200392331A1

## CPC

- C08L 69/005: {Polyester-carbonates}
- C08G 73/1053: {with oxygen only in the tetracarboxylic moiety}
- C08G 73/1071: {Wholly aromatic polyimides containing oxygen in the form of ether bonds in the main chain}
- C08K 5/0066: {Flame-proofing or flame-retarding additives}
- C08K 5/3417: condensed with carbocyclic rings
- C08K 5/42: Sulfonic acids; Derivatives thereof
- C08L 79/08: Polyimides; Polyester-imides; Polyamide-imides; Polyamide acids or similar polyimide precursors
- C08L 2201/10: Transparent films; Clear coatings; Transparent materials
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08L 2205/03: containing three or more polymers in a blend
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

A polymer blend including 5 to 95 weight percent of a poly(ester-carbonate-carbonate) comprising 40 to 95 mole percent of ester units comprising low heat bisphenol groups and high heat bisphenol groups, wherein the ester units comprise 20 to 80 mole percent of the low heat bisphenol groups and 20 to 80 mole percent of the high heat bisphenol groups, based on the total moles of ester units in the poly(ester-carbonate-carbonate), and 5 to 60 mole percent of carbonate units comprising the low heat bisphenol groups and the high heat bisphenol groups, wherein the carbonate units comprise 20 to 80 mole percent of the low heat bisphenol groups and 20 to 80 mole percent of the high heat bisphenol groups, based on the total moles of carbonate units in the poly(ester-carbonate-carbonate); and 5 to 95 weight percent of a poly(etherimide), wherein the weight percent of each polymer is based on the total weight of the polymers in the blend, and a molded 0.125-inch thick ASTM tensile bar comprising the polymer blend has a haze value of less than 25% as determined according to ASTM D1003 using the color space CIE1931 with Illuminant C and a 2° observer.

## Claims

### Claim 1

A polymer blend, comprising
5 to 95 weight percent of a poly(ester-carbonate-carbonate) comprising
40 to 95 mole percent of ester units comprising low heat bisphenol groups and high heat bisphenol groups, wherein the ester units comprise 20 to 80 mole percent of the low heat bisphenol groups and 20 to 80 mole percent of the high heat bisphenol groups, based on the total moles of ester units in the poly(ester-carbonate-carbonate), and
5 to 60 mole percent of carbonate units comprising the low heat bisphenol groups and the high heat bisphenol groups,
wherein the carbonate units comprise 20 to 80 mole percent of the low heat bisphenol groups and 20 to 80 mole percent of the high heat bisphenol groups, based on the total moles of carbonate units in the poly(ester-carbonate-carbonate); and
5 to 95 weight percent of a poly(etherimide),
wherein
the weight percent of each polymer is based on the total weight of the polymers in the blend, and
a molded 0.125-inch thick ASTM tensile bar comprising the polymer blend has a haze value of less than 25% as determined according to ASTM D1003 using the color space CIE1931 with illuminant C and a 2° observer.

### Claim 2 (depends on 1)

The polymer blend of claim 1, wherein
compared to the poly(ester-carbonate-carbonate) alone, a composition comprising the polymer blend has at least one of
an improved heat deflection temperature,
a higher glass transition temperature,
an improved strength, or
an improved modulus; and
compared to the polyetherimide alone, a composition comprising the polymer blend has at least one of
a higher melt flow, or
a higher impact strength.

### Claim 3 (depends on 1)

The polymer blend of claim 1, having at least one of
a single glass transition temperature of 200 to 240° C. determined using scanning calorimetry according to ASTM D3418 with a 20° C./min heating rate;
a melt volume rate of 15 to 20 cm3/10 minutes determined according to ASTM D1238 at 337° C. and a 6.7 kilogram load with an equilibration time of 360 seconds;
a heat deflection temperature of 180 to 195° C. determined using a 0.125 inch thick unannealed bar according to ASTM D648 at a pressure of 1.82 MPa; or
a flexural modulus of greater than or equal to 2500 MPa determined using a 0.125 inch thick unannealed bar according to ASTM D790.

### Claim 4 (depends on 1)

The polymer blend of claim 1, wherein a molded sample comprising the polymer blend has at least one of
a coefficient of thermal expansion determined according to ASTM E-831 of 49 to 62 measured cross flow over a temperature of 23 to 150° C.;
a haze of less than 10, or less than 3 determined on a measured according to ASTM D1003 using the color space CIE1931 with Illuminant C and a 2° observer at a 0.125 inch thickness; or
greater than or equal to 70% transmission determined according to ASTM D1003 using the color space CIE1931 with Illuminant C and a 2° observer at a 0.125 inch thickness.

### Claim 5 (depends on 1)

The polymer blend of claim 1, wherein
a multiplication product of the mole percent of the ester units and the mole percent of the high heat monomer groups in the poly(ester-carbonate-carbonate) is greater than 1800, or greater than 2000, or
a composition comprising the polymer blend has a haze of less than 3 and greater than or equal to 70% transmission each determined according to ASTM D1003 using the color space CIE1931 with illuminant C and a 2° observer at a 0.125 mm thickness.

### Claim 6 (depends on 1)

The polymer blend of claim 1, wherein a molded sample comprising the polymer blend retains 70% to 100% of its weight average molecular weight after heating in an air circulating oven at 190° C. for 1992 hours.

### Claim 7 (depends on 1)

The polymer blend of claim 1, wherein
the ester units are of the formula
wherein T is a C2-20 alkylene, a C6-20 cycloalkylene, or a C6-20 arylene, and each R1 is independently the low heat bisphenol group or the high heat monomer group; and
the carbonate units are of the formula,
wherein each R1 is independently the low heat bisphenol group or the high heat monomer group.

### Claim 8 (depends on 7)

The polymer blend of claim 7,
wherein T comprises isophthaloyl groups, terephthaloyl groups, or a combination comprising at least one of the foregoing, and
wherein R1 comprises bisphenol A, bisphenol AF, bisphenol B, bisphenol C, bisphenol C2, bisphenol E, bisphenol F, bisphenol G, or bisphenol S groups and phthalimidine groups of the formula
wherein Rc and Rd are each independently a C1-12 alkyl, C2-12 alkenyl, C3-8 cycloalkyl, or C1-12 alkoxy, m and n are each independently 0 to 4, and R4 is hydrogen, C2-6 alkyl, or phenyl optionally substituted with 1 to 5 C1-6 alkyl groups.

### Claim 9 (depends on 1)

The polymer blend of claim 1, wherein the low heat groups are bisphenol A groups and the high heat groups are phthalimidine groups of the formula

### Claim 10 (depends on 1)

The polymer blend of claim 1, wherein the polyetherimide comprise 2 to 1000 or 5 to 500 structural units of the formula
wherein T is a group of the formula —O—Z—O—, and
each Z is independently a divalent group of the formula
wherein Q is —O—, —S—, —C(O)—, —SO2—, —SO—, —P(Ra)(═O)— wherein Ra is a C1-8 alkyl or C6-12 aryl, or —CyH2y— wherein y is an integer from 1 to 5; and
each R is independently
wherein Q1 is —O—, —S—, —C(O)—, —SO2—, —SO—, —P(Rd)(═O)— wherein Rd is a C1-8 alkyl or C6-12 aryl, —CyH2y— wherein y is an integer from 1 to 5, or —(C6H10)z— wherein z is an integer of 1 to 4.

### Claim 11 (depends on 10)

The polymer blend of claim 10, wherein Z comprises bisphenol A groups and R comprises m-phenylene, p-phenylene, bis(4,4′-phenylene)sulfone, bis(3,4′-phenylene)sulfone, bis(3,3′-phenylene)sulfone, or a combination comprising at least one of the foregoing.

### Claim 12 (depends on 1)

The polymer blend of claim 1,
further comprising a filler, flame retardant, heat stabilizer, ultraviolet light stabilizer, mold release agent, lubricant, processing aid, dye, pigment, or a combination thereof.

### Claim 13 (depends on 1)

The polymer blend of claim 1, further comprising potassium perfluorobutane sulfonate.

### Claim 14 (depends on 1)

An article comprising the polymer blend of claim 1.

### Claim 15 (depends on 14)

The article of claim 14, wherein the article is a heat reflector, light reflector, component of a medical device, food tray, food dish, or optical connector.

### Claim 16 (depends on 1)

The polymer blend of claim 1, wherein the phthalimidine groups are of the formula
wherein R4 is hydrogen, methyl, or phenyl.

### Claim 17 (depends on 1)

The polymer blend of claim 1, wherein the phthalimidine groups are of the formula

### Claim 18 (depends on 1)

The polymer blend of claim 1 further comprising a flame retardant, wherein a composition comprising the polymer blend a V0 rating determined according to UL 94 at a thickness of 1.5 millimeters.

### Claim 19 (depends on 14)

The article of claim 14, wherein the article is a metallized article, injection-molded article, or extruded article.