# US 2020/0392318 A1 · Filled polypropylene (pp) compositions with improved thermo-mechanical properties

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0392318 A1
- Document ID: US20200392318A1
- Status: Published application
- Kind: A1
- Application number: 16/754,504
- Filed: 2018-10-22
- Published: 2020-12-17
- Earliest claimed: 2017-10-25
- Assignees: Borealis AG
- Applicants: Borealis AG
- Inventors: Jingbo Wang; Simon Schwarzenberger; Klaus Bernreitner; Markus Gahleitner; Ville Vurkkunen
- Web page: https://patentgrep.com/patent/US20200392318A1

## CPC

- C08K 3/34: Silicon-containing compounds
- C08L 23/12: Polypropene
- C08K 3/22: of metals
- C08K 3/30: Sulfur-, selenium- or tellurium-containing compounds
- C08K 3/346: {Clay}
- C08K 5/523: with hydroxyaryl compounds
- C08K 5/526: with hydroxyaryl compounds
- C08K 2003/2224: {Magnesium hydroxide}
- C08K 2003/3063: {Magnesium sulfate}
- C08K 2201/003: Additives being defined by their diameter
- C08K 2201/006: Additives being defined by their surface area
- C08L 2205/24: Crystallisation aids
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

The present application relates to a polypropylene (PP) composition comprising a) 50.0 to 95.0 wt.-%, based on the total weight of the polypropylene (PP) composition, of a polypropylene (PP) homopolymer being polymerized in the presence of a single-site catalyst and b) 5.0 to 50.0 wt.-%, based on the total weight of the polypropylene (PP) composition, of a mineral filler, to an article comprising the polypropylene (PP) composition as well as the use of the polypropylene (PP) composition for improving the thermo-mechanical properties.

## Claims

### Claim 1

Polypropylene (PP) composition comprising
a) 50.0 to 95.0 wt.-%, based on the total weight of the polypropylene (PP) composition, of a polypropylene (PP) homopolymer being polymerized in the presence of a single-site catalyst and having
i) a melt flow rate MFR2 (230° C.) measured according to ISO 1133 in the range of 1 to 200 g/10 min, and
ii) a melting temperature (Tm) measured by differential scanning calorimetry (DSC) of ≥153° C., and
b) 5.0 to 50.0 wt.-%, based on the total weight of the polypropylene (PP) composition, of a mineral filler.

### Claim 2 (depends on 1)

The polypropylene (PP) composition according to claim 1, wherein the polypropylene (PP) homopolymer is unimodal and/or has a molecular weight distribution Mw/Mn measured according to ISO 16014 in the range of 1.5 to 4.5, preferably in the range from 2.0 to 4.0, and more preferably in the range from 2.5 to 4.0.

### Claim 3 (depends on 1, 2)

The polypropylene (PP) composition according to claim 1 or 2, wherein the polypropylene (PP) homopolymer has
a) a melt flow rate MFR2 (230° C.) measured according to ISO 1133 in the range of 2 to 100 g/10 min, preferably from 2.2 to 50 g/10 min, and/or
b) a melting temperature (Tm) measured by differential scanning calorimetry (DSC) in the range from 153 to 165° C., preferably in the range from 153 to 163° C., and/or
c) a heat deflection temperature HDT B measured in accordance with ISO 75 at a load of 0.46 MPa of at least 90° C., preferably in the range from 90 to 100° C.

### Claim 4

The polypropylene (PP) composition according to any one of the preceding claims, wherein the polypropylene (PP) homopolymer has
a) a xylene cold soluble fraction (XCS) determined at 23° C. according ISO 16152 of equal or below 2.0 wt.-%, and/or
b) a weight average molecular weight (Mw) measured according to ISO 16014 in the range from 80 to 500 kg/mol, and/or
c) an isotactic triad fraction (mm) determined from 13C-NMR spectroscopy of at least 98.0%, and/or
d) a content of <2,1> erythro regiodefects as determined from 13C-NMR spectroscopy in the range from 0.10 to 1.00 mol.-%.

### Claim 5

The polypropylene (PP) composition according to any one of the preceding claims, wherein the polypropylene (PP) homopolymer has a flexural modulus measured according to ISO 178 of at least 1300 MPa, preferably in the range from 1300 to 2200 MPa.

### Claim 6

The polypropylene (PP) composition according to any one of the preceding claims, wherein the mineral filler is an anisotropic mineral filler, preferably a mineral filler selected from the group comprising talc, wollastonite, mica, montmorillonite, magnesium sulfate, magnesium hydroxide, halloysite and mixtures thereof.

### Claim 7

The polypropylene (PP) composition according to any one of the preceding claims, wherein the mineral filler has a particle size d50 in the range from 0.1 to 10 μm, preferably in the range from 0.2 to 6.0 μm, more preferably in the range from 0.3 to 4.0 μm.

### Claim 8

The polypropylene (PP) composition according to any one of the preceding claims, wherein the polypropylene (PP) composition further comprises a nucleating agent in an amount in the range from 0.002 to 1.5 wt.-%, based on the total weight of the polypropylene (PP) composition.

### Claim 9 (depends on 8)

The polypropylene (PP) composition according to claim 8, wherein the nucleating agent is a α-nucleating agent, preferably a phosphate-based α-nucleating agent.

### Claim 10

The polypropylene (PP) composition according to any one of the preceding claims, wherein the polypropylene (PP) composition has
a) a melt flow rate MFR2 (230° C., 2.16 kg) measured according to ISO 1133 in the range from 0.5 to 175 g/10 min, more preferably in the range from 1.0 to 90 g/10 min, like in the range from 2.0 to 45 g/10 min, and/or
b) a melting temperature (Tm) measured by differential scanning calorimetry (DSC) in the range from 154 to 165° C., preferably in the range from 155 to 163° C., and/or
c) a crystallization temperature (Tc) measured by differential scanning calorimetry (DSC) in the range from 120 to 135° C., preferably in the range from 122 to 132° C., and/or
d) a flexural modulus measured according to ISO 178 in the range from 2700 to 6500 MPa, preferably in the range from 2750 to 6000 MPa, and/or
e) a heat deflection temperature (HDT) measured according to ISO 75 A at a load of 1.8 MPa in the range of 76 to 95° C., more preferably in the range from 77 to 92° C.

### Claim 11

The polypropylene (PP) composition according to any one of the preceding claims, wherein the polypropylene (PP) composition has a ratio of melting temperature (Tm) measured by differential scanning calorimetry (DSC) to heat deflection temperature (HDT) measured according to ISO 75 A [Tm/HDT] of ≤2.0.

### Claim 12

Article comprising the polypropylene (PP) composition according to any one of the preceding claims.

### Claim 13 (depends on 12)

The article according to claim 12, wherein the article is an automotive interior article.

### Claim 14 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11)

Use of a polypropylene (PP) composition as defined in any one of claims 1 to 11 for improving the thermo-mechanical properties, wherein the improvement is achieved if the polypropylene (PP) composition has a ratio of melting temperature (Tm) measured by differential scanning calorimetry (DSC) to heat deflection temperature (HDT) measured according to ISO 75 A [Tm/HDT] of ≤2.0.