# US 2020/0392299 A1 · Super-hydrophobic electrothermal epoxy resin composite material and preparation and self-repairing method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0392299 A1
- Document ID: US20200392299A1
- Status: Published application
- Kind: A1
- Application number: 17/003,569
- Filed: 2020-08-26
- Published: 2020-12-17
- Earliest claimed: 2018-02-27
- Assignees: Soochow University
- Applicants: Soochow University
- Inventors: Guozheng LIANG; Youhao ZHANG; Aijuan GU; Li YUAN
- Web page: https://patentgrep.com/patent/US20200392299A1

## CPC

- C07D 327/00: Heterocyclic compounds containing rings having oxygen and sulfur atoms as the only ring hetero atoms
- C08G 59/4064: {sulfur containing compounds (C08G59/4021, C08G59/4028 take precedence)}
- C08G 59/4215: {cycloaliphatic}
- C08J 7/0423: {with at least one layer of inorganic material and at least one layer of a composition containing a polymer binder}
- C08J 7/0427: {with only one layer of a composition containing a polymer binder (with more layers C08J7/042)}
- C08L 63/00: Compositions of epoxy resins; Compositions of derivatives of epoxy resins
- C08J 2363/00: Characterised by the use of epoxy resins; Derivatives of epoxy resins
- C08J 2463/00: Characterised by the use of epoxy resins; Derivatives of epoxy resins
- C07D: HETEROCYCLIC COMPOUNDS (macromolecular compounds C08)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

Superhydrophobic electrothermal epoxy composites, their preparation and a self-healing method are disclosed. 1,4,5-oxadithiepane-2,7-dione and methylhexahydrophthalic anhydride were mixed and cured with epoxides to get self-healable epoxy resins; carbon nanotube/self-healable epoxy resin prepolymers were coated on self-healable epoxy resins and cured to get electrothermal epoxy composites; modified superhydrophobic copper powders were adhered on electrothermal epoxy composites and cured to get a kind of superhydrophobic electrothermal epoxy composites. The thermal resistance of superhydrophobic electrothermal epoxy composites is superior to existed technical solutions and they can simultaneously repair cracking and delamination and the healed samples still exhibit excellent superhydrophobicity. These merits of superhydrophobic electrothermal epoxy composites provided in this invention can meet the harsh requirements of self-healing and removing ice on surfaces of wind turbine blades, suggesting good abilities of guaranteeing service safety and lifespan of wind turbine blades.

## Claims

### Claim 1

A method of preparing superhydrophobic electrothermal epoxy composites, comprising:
(1) mixing 100 parts of an epoxy resin, 42 to 84 parts of 1,4,5-oxadithiepane-2,7-dione and 0 to 43 parts of methylhexahydrophthalic anhydride, by weight, homogeneously at 50 to 70° C., and curing to obtain self-healable epoxy resins;
(2) mixing 10 parts of the epoxy resin, 4.2 to 8.4 parts of 1,4,5-oxadithiepane-2,7-dione, and 0 to 4.3 parts of methylhexahydrophthalic anhydride, by weight, homogeneously at 50 to 70° C. to obtain a first prepolymer, adding 0.1 to 4 parts of a carbon nanotube by weight and a ester solvent to the first prepolymer and mixing homogeneously to to obtain a paste, coating the self-healable epoxy resins obtained in the step (1) with the paste, evaporating the ester solvent and curing to obtain electrothermal epoxy composites;
(3) dispersing 4 parts of copper nanopowders and 0.1 to 2 parts of perfluorocarboxylic acid, by weight, in water, mixing homogeneously, filtering and drying to obtain modified superhydrophobic copper powders;
(4) mixing at 50 to 70° C., 10 parts of epoxy resin, 4.2 to 8.4 parts of 1,4,5-oxadithiepane-2,7-dione and 0 to 4.3 parts of methylhexahydrophthalic anhydride, by weight, homogeneously to obtain a second prepolymer, dispersing the second prepolymer and the modified superhydrophobic copper powders sequentially on the electrothermal epoxy composites obtained in the step (2), and curing to obtain the superhydrophobic electrothermal epoxy composites.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the 1,4,5-oxadithiepane-2,7-dione is prepared by a method comprising:
(1) mixing 120 parts of 2-mercaptoacetic acid, 500 to 700 parts of the ester solvent and 0.6 to 1.2 parts of potassium iodide, by ewight, homogeneously at 20 to 30° C. to obtain a solution, adding 80 to 90 parts of 30 wt % H2O2, by weight, dropwise to the solution, and continuing to react for 2 to 4 hour to get 2,2′-dithiodiacetic acid;
(2) mixing 100 parts of 2,2′-dithiodiacetic acid and 120 to 150 parts of an acid anhydride, by weight, homogeneously at 20 to 30° C., and continuing to react for 2 to 4 hours to obtain the 1,4,5-oxadithiepane-2,7-dione.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the ester solvent is selected from the group consisting of methyl acetate, ethyl acetate, propyl acetate, methyl propionate, ethyl propionate, and a combination thereof

### Claim 4 (depends on 1)

The method according to claim 1, wherein the perfluorocarboxylic acid is selected from the group consisting of perfluorooctanoic acid, perfluorononanoic acid, perfluorodecanoic acid, and a combination thereof.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the epoxy resin is selected from the group consisting of a glycidyl ether type epoxy resin, a glycidyl ester type epoxy resin, a glycidyl amine type epoxy resin, aliphatic epoxides, alicyclic epoxides, and a combination thereof.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the carbon nanotube is selected from the group consisting of an unprocessed single-walled carbon nanotube, a multi-walled carbon nanotube, and a combination thereof.

### Claim 7 (depends on 2)

The method according to claim 2, wherein the acid anhydride is selected from the group consisting of acetic anhydride, trifluoroacetic anhydride, and a combination thereof.

### Claim 8 (depends on 1)

The method according to claim 1, further comprising:
heating the superhydrophobic electrothermal epoxy composites at 160 to 200° C. for 1 to 3 hours to complete a self-healing process.