# US 2020/0392035 A1 · Non-iox glasses with high coefficient of thermal expansion and preferential fracture behavior for thermal tempering

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0392035 A1
- Document ID: US20200392035A1
- Status: Published application
- Kind: A1
- Application number: 16/767,191
- Filed: 2018-11-30
- Published: 2020-12-17
- Earliest claimed: 2017-11-30
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Timothy Michael Gross; Peter Joseph Lezzi
- Web page: https://patentgrep.com/patent/US20200392035A1

## CPC

- C03C 3/097: containing phosphorus, niobium or tantalum
- C03B 25/025: {Glass sheets}
- C03B 27/012: by heat treatment, e.g. for crystallisation; Heat treatment of glass products before tempering by cooling (C03B27/008, C03B27/016 take precedence)
- C03B 27/0413: {Stresses, e.g. patterns, values or formulae for flat or bent glass sheets}
- C03B 27/044: for flat or bent glass sheets being in a horizontal position
- C03C 3/091: containing aluminium
- C03C 23/007: {by thermal treatment}
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES

## Abstract

The disclosure relates to glass compositions with high coefficients of thermal expansion and low fracture toughness designed for thermal tempering. These glasses are ideally suited to produce a “dicing” pattern when thermally tempered, even when thin (<3 mm). Disclosed glasses have high thermal expansions at low and high temperatures to produce increased temper stresses once quenched, coupled with low fracture toughness which promotes crack bifurcation and enhanced frangibility. Methods of making such glasses are also provided.

## Claims

### Claim 1

A glass comprising:
from 75 to 90 mol % SiO2
from 5 to 20 mol % Al2O3
greater than 0 to 20 mol % of at least one alkaline earth oxide from the group consisting of MgO, CaO, BaO, or SrO
from 8 to 20 mol % K2O; and
>0-10 mol % B2O3 in composition of the glass.

### Claim 2 (depends on 1)

The glass of claim 1, comprising from 75 to 85 mol % SiO2 in composition of the glass.

### Claim 3 (depends on 1)

The glass of claim 1, further comprising:
0-16 mol % Na2O; and
3-22 mol % Na2O+K2O in composition of the glass.

### Claim 4 (depends on 1)

The glass of claim 1, wherein the low temperature coefficient of thermal expansion from 25-300° C. is greater than 75×10−7 ppm/° C.

### Claim 5 (depends on 1)

The glass of claim 1, wherein the high temperature coefficient of thermal expansion is greater than 250×10−7 ppm/° C.

### Claim 6 (depends on 1)

The glass of claim 1, wherein the fracture toughness, KIC is less than 0.65 MPa-m1/2.

### Claim 7 (depends on 1)

The glass of claim 1, wherein the glass has a viscosity of 200 kP at a temperature of from 1000-1200° C.

### Claim 8 (depends on 1)

The glass of claim 1, wherein the glass has a viscosity of 35 kP at a temperature of from 1100-1300° C.

### Claim 9 (depends on 1)

The glass of claim 1, comprising from 75 to 80 and 0.5 to 8 mol % B2O3 in composition of the glass.

### Claim 10 (depends on 1)

The glass of claim 1, comprising from 7 to 20 mol % Al2O3 in composition of the glass.

### Claim 11 (depends on 1)

The glass of claim 1, comprising 2 to 20 mol % MgO in composition of the glass.

### Claim 12 (depends on 1)

The glass of claim 1, comprising 8-16 mol % Na2O+K2O in of the glass.

### Claim 13 (depends on 1)

The glass of claim 1, comprising from 11 to 20 mol % K2O in of the glass.

### Claim 14

A glass, comprising:
from 75 to 90 mol % SiO2;
from 5 to 20 mol % Al2O3;
greater than 0 to 20 mol % of at least one alkaline earth oxide from the group consisting of MgO, CaO, BaO, or SrO;
from 11 to 20 mol % K2O; and
greater than 0 to 10 mol % B2O3 in of the glass,
wherein the glass is thermally tempered and has a depth of compression of at least about 10 microns, and
wherein the depth of compression extends up to about 25% into the glass as measured by thickness from surface to center of the glass.

### Claim 15 (depends on 14)

The glass of claim 14, wherein the glass is thermally tempered and has a surface compressive stress of at least 250 MPa.

### Claim 16 (depends on 14)

The glass of claim 14, wherein the glass meets the dicing standard ASTM C1048.

### Claim 17 (depends on 1)

A method of making the glass of claim 1, the method comprising mixing SiO2, Al2O3, at least one alkaline earth oxide from the group consisting of MgO, CaO, BaO, or SrO, K2O; and B2O3 to create a homogenous melt.

### Claim 18 (depends on 17)

The method of claim 17, wherein the melt is formed into glass sheets and the glass sheets are subsequently thermally tempered.

### Claim 19 (depends on 17)

The method of claim 17, wherein the glass meets the dicing standard ASTM C1048.

### Claim 20 (depends on 17)

The method of claim 17, wherein the glass is melted and maintained at temperatures ranging from 1100-1650° C. for times ranging from about 6-16 hours, and annealed at about 500-650° C., where the glass is held at temperature for about 1 hour and subsequently cooled for at least 6 hours.