# US 2020/0392031 A1 · Basalt fibers produced from high temperature melt

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0392031 A1
- Document ID: US20200392031A1
- Status: Published application
- Kind: A1
- Application number: 16/828,211
- Filed: 2020-03-24
- Published: 2020-12-17
- Earliest claimed: 2016-04-21
- Assignees: Americas Basalt Technology, LLC
- Applicants: Americas Basalt Technology, LLC
- Inventors: Yevgeniy Zubko; Yurii Zubko
- Web page: https://patentgrep.com/patent/US20200392031A1

## CPC

- C03B 5/021: {by induction heating}
- C03B 5/1672: {Use of materials therefor}
- C03B 5/23: Cooling the molten glass (C03B5/18, C03B5/225 take precedence)
- C03B 19/102: {by blowing a gas onto a stream of molten glass or onto particulate materials, e.g. pulverising}
- C03B 37/02: by drawing or extruding, {e.g. direct drawing of molten glass from nozzles; Cooling fins therefor (C03B37/04 takes precedence; sizing of the fibres C03C25/00)}
- C03B 37/06: by blasting or blowing molten glass, e.g. for making staple fibres
- C03B 37/065: starting from tubes, rods, fibres or filaments
- H05B 6/24: Crucible furnaces (H05B6/30 takes precedence)
- C03B 5/26: Outlets {, e.g. drains, siphons}; Overflows {, e.g. for supplying the float tank, tweels}
- Y02P 40/57: Improving the yield, e-g- reduction of reject rates
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- H05B: ELECTRIC HEATING; ELECTRIC LIGHT SOURCES NOT OTHERWISE PROVIDED FOR; CIRCUIT ARRANGEMENTS FOR ELECTRIC LIGHT SOURCES, IN GENERAL
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Methods, systems and apparatus for producing continuous basalt fibers, microfibers, and microspheres from high temperature melts are disclosed. A cold crucible induction furnace is used to super heat crushed basalt rock to form a melt. The melt is cooled prior to forming a fiber. The fiber produced from the superheated melt possesses superior properties not found with conventional basalt fibers produced in gas furnaces. In some implementations, the superheated melt is spun into continuous basalt fibers. In some implementations, the superheated melt is blown into microfibers and microspheres.

## Claims

### Claim 1

A method of producing basalt microspheres, comprising:
charging a quantity of basalt into an induction furnace, the induction furnace having an interior comprising copper plates and containing substantially no refractory lining;
inductively superheating at least about 100 kilograms of basalt in the induction furnace to form a superheated melt;
cooling the superheated melt by passing the melt through a water cooled tray to form a cooled melt; and
forming the basalt microspheres from the cooled melt, wherein 1 kilogram of microspheres is produced using less than 2.2 kilowatts of electrical power.

### Claim 2 (depends on 1)

The method of claim 1, wherein the basalt microspheres have an average diameter from about 0.5 microns to about 215 microns.

### Claim 3 (depends on 2)

The method of claim 2, wherein the basalt microspheres have an average diameter from about 0.5 microns to about 3 microns.

### Claim 4 (depends on 1)

The method of claim 1, the basalt microspheres are in the shapes of rods or dumbbells.

### Claim 5 (depends on 2)

The method of claim 2, the basalt microspheres are solid balls without any entrapped air.

### Claim 6 (depends on 2)

The method of claim 2, wherein the induction furnace is a cold crucible induction furnace.

### Claim 7 (depends on 1)

The method of claim 1, wherein the superheated melt is substantially homogeneous at a temperature of at least about 2500° C., and the cooled melt is at a temperature below 1500° C.

### Claim 8 (depends on 1)

The method of claim 1, wherein forming the basalt microspheres from the cooled melt includes passing the cooled melt through a blowing device.

### Claim 9 (depends on 8)

The method of claim 8, wherein the blowing device produces a high speed jet of air and creates an ultrasonic vibration.

### Claim 10 (depends on 1)

The method of claim 1, further comprising:
classifying the basalt microspheres by size.

### Claim 11

A method of producing microspheres, comprising:
charging a quantity of a rock into an induction furnace, the induction furnace having an interior comprising copper plates and containing substantially no refractory lining, the rock comprising plagioclase having a plagioclase melting point and a component having a component melting point, wherein the plagioclase melting point is less than the component melting point;
inductively heating the quantity of the rock in the induction furnace to a furnace temperature above the component melting point to form a superheated melt,
cooling the superheated melt to a temperature between the plagioclase melting point and the component melting point by passing the superheated melt though a water cooled tray to form a cooled melt; and
forming microspheres from the cooled melt.

### Claim 12 (depends on 11)

The method of claim 11, wherein the rock is basalt.

### Claim 13 (depends on 12)

The method of claim 12, wherein the plagioclase melting point is from about 950° C. to about 1200° C.

### Claim 14 (depends on 13)

The method of claim 13, wherein the component melting point is from about 1400° C. to about 1600° C.

### Claim 15 (depends on 14)

The method of claim 14, wherein the superheated melt is at least about 98% amorphous at the furnace temperature of at least about 2500° C.

### Claim 16 (depends on 11)

The method of claim 11, wherein the component is quartz or iron oxide.

### Claim 17 (depends on 11)

The method of claim 11, wherein forming microspheres from the cooled melt includes passing the cooled melt through a blowing device.

### Claim 18

A method of producing a microspheres, comprising:
charging a quantity of basalt into a cold crucible induction furnace wherein the induction furnace has an interior comprising copper plates and containing substantially no refractory lining;
inductively heating the quantity of the basalt in the cold crucible induction furnace to a temperature of at least about 2500° C. to form a homogenous melt, wherein the cold crucible induction furnace heats about 1 kilogram of basalt per less than 2.2 kilowatts of electrical power;
cooling the homogenous melt to a temperature less than about 1500° C. by passing the melt through a water cooled tray to form a cooled homogenous melt; and
forming the microspheres by passing the cooled homogenous melt through a blowing device.

### Claim 19 (depends on 18)

The method of claim 18, wherein the cold crucible induction furnace heats about 1 kilogram of basalt per less than 2.0 kilowatts of electrical power.

### Claim 20 (depends on 18)

The method of claim 18, wherein the cold crucible induction furnace operates at a frequency of about 0.22 megahertz, 0.32 megahertz, 0.44 megahertz, or 1.76 megahertz.

### Claim 21

A method of producing microspheres from a homogeneous melt, comprising:
charging a quantity of basalt rock into a cold crucible induction furnace; inductively heating the quantity of the basalt in the cold crucible induction furnace to a temperature of at least about 2500° C. to form a homogenous melt having a viscosity of less than about 500 cP, wherein the cold crucible induction furnace includes an interior comprising copper plates and containing substantially no refractory lining;
wherein the cold crucible induction furnace heats about 1 kilogram of basalt per less than 2.2 kilowatts of electrical power;
cooling the homogenous melt to a temperature less than about 1500° C. by passing the homogenous melt through a water cooled tray; and
forming the microspheres by passing the cooled homogenous melt through a blowing device.

### Claim 22 (depends on 21)

The method of claim 21, wherein the cold crucible induction furnace operates at a frequency of about 0.22 megahertz, 0.32 megahertz, 0.44 megahertz, or 1.76 megahertz.