# US 2020/0391485 A1 · Method for reducing bow in laminate structures

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0391485 A1
- Document ID: US20200391485A1
- Status: Published application
- Kind: A1
- Application number: 17/005,458
- Filed: 2020-08-28
- Published: 2020-12-17
- Earliest claimed: 2015-01-06
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: James Gregory Couillard
- Web page: https://patentgrep.com/patent/US20200391485A1

## CPC

- B32B 17/10036: {comprising two outer glass sheets}
- B32B 7/027: Thermal properties
- B32B 17/101: {having a predetermined coefficient of thermal expansion [CTE]}
- B32B 17/10761: {containing vinyl acetal}
- B32B 17/10871: {in combination with particular heat treatment}
- B32B 17/1099: {After-treatment of the layered product, e.g. cooling}
- B32B 37/0015: {to avoid warp or curl}
- B32B 37/06: characterised by the heating method
- B32B 37/144: {using layers with different mechanical or chemical conditions or properties, e.g. layers with different thermal shrinkage, layers under tension during bonding (constructional features for tensioning B32B38/1825)}
- B32B 38/0036: {Heat treatment (for heating or cooling of layers during lamination B32B37/06, B32B37/08)}
- B32B 2038/0048: {Annealing, relaxing}
- B32B 2038/006: {Relieving internal or residual stresses}
- B32B 2315/08: Glass
- B32B 2419/00: Buildings or parts thereof
- B32B 2551/00: Optical elements
- B32B 2605/08: Cars
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM

## Abstract

Disclosed herein are methods for making asymmetric laminate structures and methods for reducing bow in asymmetric laminate structures, the methods comprising subjecting the laminate structures to at least one thermal cycle comprising cooling the laminate structures to a first temperature near or below room temperature and heating the laminate structures to a second temperature near or below the lamination temperature. Also disclosed herein are laminate structures made according to such methods.

## Claims

### Claim 1

A method for making a laminate structure, comprising:
positioning an interlayer between a first substrate and a second substrate to form a stack;
heating the stack to a lamination temperature to form a laminate structure; and
subjecting the laminate structure to at least one thermal cycle,
wherein the thermal cycle comprises cooling the laminate structure to a first temperature ranging from about −20° C. to about 35° C., and heating the laminate structure to a second temperature below the lamination temperature, the second temperature ranging from about 50° C. to about 120° C., and
wherein a coefficient of thermal expansion of the first substrate is different than a coefficient of thermal expansion of the second substrate.

### Claim 2 (depends on 1)

The method of claim 1, wherein the interlayer is chosen from polyvinyl butyral, ethylene-vinyl acetate, thermoplastic polyurethane, and ionomers.

### Claim 3 (depends on 1)

The method of claim 1, wherein the first and second substrates are independently chosen from glass, glass-ceramics, ceramics, polymers, and metals.

### Claim 4 (depends on 1)

The method of claim 1, wherein the lamination temperature ranges from about 120° C. to about 160° C.

### Claim 5 (depends on 4)

The method of claim 4, wherein the stack is heated to the lamination temperature at a pressure ranging from about 0.1 MPa to about 1.5 MPa.

### Claim 6 (depends on 1)

The method of claim 1, further comprising heating the stack to a conditioning temperature ranging from about 75° C. to about 100° C.

### Claim 7 (depends on 1)

The method of claim 1, wherein the thermal cycle comprises a ramp rate between the first and second temperatures ranging from about 0.1° C./min to about 2° C./min.

### Claim 8 (depends on 7)

The method of claim 7, wherein the thermal cycle further comprises holding the laminate structure at the first temperature for a first time period ranging from about 30 minutes to about 4 hours, and holding the laminate structure at the second temperature for a second time period ranging from about 30 minutes to about 4 hours.

### Claim 9 (depends on 8)

The method of claim 8, wherein the thermal cycle further comprises holding the laminate structure at one or more intermediate temperatures between the first and second temperatures.

### Claim 10 (depends on 1)

The method of claim 1, wherein the coefficient of thermal expansion of the first substrate is at least 0.1% greater than the coefficient of thermal expansion of the second substrate.

### Claim 11 (depends on 1)

The method of claim 1, wherein the coefficient of thermal expansion of the first substrate is at least 30% greater than the coefficient of thermal expansion of the second substrate.

### Claim 12 (depends on 1)

The method of claim 1, wherein the stack further comprises an additional layer chosen from polymer layers, additional glass layers, reflective layers, and electrochromic layers.