# US 2020/0391350 A1 · Peening media and processes for producing and using peening media

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0391350 A1
- Document ID: US20200391350A1
- Status: Published application
- Kind: A1
- Application number: 16/902,880
- Filed: 2020-06-16
- Published: 2020-12-17
- Earliest claimed: 2019-06-17
- Assignees: Purdue Research Foundation
- Applicants: Purdue Research Foundation
- Inventors: David F. Bahr; David A. Brice
- Web page: https://patentgrep.com/patent/US20200391350A1

## CPC

- B24C 11/00: Selection of abrasive materials {or additives} for abrasive blasts (polishing compositions C09G)
- B24C 1/10: for compacting surfaces, e.g. shot-peening (for deforming sheet metal, tubes or profiles B21D31/06; as a metallurgical treatment C21D7/00, C22F1/00)
- C22F 1/183: {of titanium or alloys based thereon}
- C22F 1/186: {of zirconium or alloys based thereon}
- B24C: ABRASIVE OR RELATED BLASTING WITH PARTICULATE MATERIAL
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)

## Abstract

Processes for producing peening media, the peening media produced from such processes, and methods of using such media. Particles are provided having surfaces that are formed of or contain a metal that exhibits solubility for oxygen in a metallic phase so as to increase in surface hardness as a result of solid solution strengthening due to oxidizing of the surfaces of the particles. The particles are subjected to a thermal process in an oxygen-containing atmosphere at a process temperature and for a process duration sufficient to oxidize the surfaces of the particles to increase the surface hardness of the particles while not forming an oxide layer that encases the particles.

## Claims

### Claim 1

A process of producing shot peening media, the process comprising:
providing particles wherein at least surfaces of the particles consist of or containing a metal that exhibits solubility for oxygen in a metallic phase so as to increase in surface hardness as a result of solid solution strengthening due to oxidizing of the surfaces of the particles; and
subjecting the particles to a thermal process in an oxygen-containing atmosphere at a process temperature and for a process duration sufficient to oxidize the surfaces of the particles to increase the surface hardness of the particles while not forming an oxide layer that encases the particles.

### Claim 2 (depends on 1)

The process of claim 1, wherein the surface hardness of the particles is increased by a factor of about three.

### Claim 3 (depends on 1)

The process of claim 1, wherein the metal is a valve metal.

### Claim 4 (depends on 1)

The process of claim 1, wherein the metal is chosen from the group consisting of titanium, tantalum, vanadium, and zirconium.

### Claim 5 (depends on 1)

The process of claim 1, wherein the process temperature of the thermal process is below an oxidation start temperature of the metal.

### Claim 6 (depends on 1)

The process of claim 1, wherein the oxygen-containing atmosphere of the thermal process is ambient atmosphere.

### Claim 7 (depends on 1)

The process of claim 1, wherein the thermal process is performed with no mechanical agitation of the particles.

### Claim 8 (depends on 1)

The process of claim 1, wherein the thermal process is performed without sintering the particles.

### Claim 9 (depends on 1)

The process of claim 1, wherein the thermal process results in some sintering of the particles, the process further comprising mechanically agitating the particles to separate sintered particles.

### Claim 10 (depends on 1)

The process of claim 1, wherein the metal is titanium, the oxygen-containing atmosphere is ambient atmosphere, and the process temperature is not greater than 530° C.

### Claim 11 (depends on 10)

The process of claim 10, wherein the process duration is about 20 hours.

### Claim 12 (depends on 10)

The process of claim 10, wherein the process temperature is about 430° C. up to 530° C. and the process duration is about 20 to about 24 hours.

### Claim 13 (depends on 1)

The process of claim 1, wherein the surface hardness of the particles is increased to a case depth of about 2 to 3 μm.

### Claim 14 (depends on 1)

The process of claim 1, wherein the particles have diameters of about 50 to about 100 μm.

### Claim 15 (depends on 1)

The process of claim 1, wherein the surfaces of the particles have oxide islands.

### Claim 16 (depends on 1)

The process of claim 1, wherein the particles are entirely formed of the metal.

### Claim 17 (depends on 1)

Shot peening media comprising particles produced by the thermal process of claim 1.

### Claim 18 (depends on 1)

A process comprising peening a surface of an article with particles produced by the thermal process of claim 1, wherein the article is formed of a base metal that is the same as the metal of the particles.

### Claim 19 (depends on 18)

The process of claim 18, wherein the article is formed of titanium or an alloy thereof, and the metal of the particles is titanium or an alloy thereof.

### Claim 20 (depends on 15)

The process of claim 15, wherein the article is an aerospace, automotive, or biomedical component.