# US 2020/0391190 A1 · Photocatalyst nanocomposite

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0391190 A1
- Document ID: US20200391190A1
- Status: Published application
- Kind: A1
- Application number: 16/437,614
- Filed: 2019-06-11
- Published: 2020-12-17
- Earliest claimed: 2019-06-11
- Assignees: Imam Abdulrahman Bin Faisal University
- Applicants: Imam Abdulrahman Bin Faisal University
- Inventors: Nuhad Abdullah ALOMAIR; Hanan Hussein Amin Mohamed
- Web page: https://patentgrep.com/patent/US20200391190A1

## CPC

- B01J 23/8953: {with zinc, cadmium or mercury}
- B01J 21/18: Carbon
- B01J 23/38: of noble metals
- B01J 23/60: with zinc, cadmium or mercury
- B01J 35/39: Photocatalytic properties
- B01J 35/45: Nanoparticles
- B01J 35/647: {2-50 nm}
- B01J 37/031: {Precipitation}
- B01J 37/038: {to form slurries or suspensions, e.g. a washcoat}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- C02F 1/30: by irradiation
- C02F 1/725: {by catalytic oxidation}
- B01J 2235/00: Indexing scheme associated with group B01J35/00, related to the analysis techniques used to determine the catalysts form or properties
- B01J 2235/10: Infrared [IR]
- B01J 2235/15: X-ray diffraction
- B01J 2235/30: Scanning electron microscopy; Transmission electron microscopy
- C02F 2101/308: {Dyes; Colorants; Fluorescent agents}
- C02F 2305/08: Nanoparticles or nanotubes
- C02F 2305/10: Photocatalysts
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C02F: TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE (separation in general B01D; special arrangements on waterborne vessels of installations for treating water, waste water or sewage, e.g. for producing fresh water, B63J; adding materials to water to prevent corrosion C23F; treating radioactively-contaminated liquids G21F9/04; regeneration of reactants for recirculation into processes, see the relevant places for the processes)

## Abstract

An efficient photocatalyst nanocomposite comprising reduced graphene oxide, noble metal, and a metal oxide prepared by a one-step method that utilizes date seed extract as a reducing and nanoparticle determining size agent. The photocatalyst of the invention is a more effective sunlight photocatalyst than that prepared by traditional method in the photo decomposition of organic compounds in contaminated water.

## Claims

### Claim 1

A photocatalyst nanocomposite, comprising:
noble metal nanoparticles, metal oxide nanoparticles, and reduced graphene oxide (rGO),
wherein the photocatalyst nanocomposite comprises rGO in an amount in the range of 40 wt. % to 60 wt. % of the total weight of the photocatalyst nanocomposite,
wherein the noble metal nanoparticles have a diameter in the range of 5 nm to 50 nm and are dispersed on the metal oxide nanoparticles which are present on the rGO; the metal oxide nanoparticles have a diameter in the range of 20 nm to 80 nm; and the noble metal nanoparticles are present in an amount in the range of 2 mol. % to 10 mol. % based on the molar amount of the metal oxide nanoparticles; and
wherein the metal oxide nanoparticles comprise a metal oxide of at least one metal selected from the group consisting of Sc, Ti, V, Cr, Mn, Fe, Co, Ni, Zn, Y, Zr, Nb, and Mo.

### Claim 2 (depends on 1)

The photocatalyst nanocomposite of claim 1, wherein the photocatalyst composite comprises rGO in an amount in the range of 48 wt. % to 52 wt. % of the total weight of the nanocomposite.

### Claim 3 (depends on 1)

The photocatalyst nanocomposite of claim 1, wherein the noble metal nanoparticles have a diameter in the range of 10-30 nm.

### Claim 4 (depends on 1)

The photocatalyst nanocomposite of claim 1, wherein the noble metal nanoparticles are selected from the group consisting of ruthenium, rhodium, palladium, silver, osmium, iridium, platinum, and gold.

### Claim 5 (depends on 1)

The photocatalyst nanocomposite of claim 1, wherein the noble metal nanoparticles are gold.

### Claim 6 (depends on 1)

The photocatalyst nanocomposite of claim 1, wherein the metal oxide is an oxide of a metal selected from the group consisting of Ti, V, Mn, and Zn.

### Claim 7 (depends on 1)

The photocatalyst nanocomposite of claim 1, wherein the metal oxide is hexagonal wurtzite ZnO.

### Claim 8 (depends on 1)

The photocatalyst nanocomposite of claim 1, wherein the metal oxide nanoparticles have diameter in the range of 25-50 nm.

### Claim 9 (depends on 1)

The photocatalyst nanocomposite of claim 1, wherein the photocatalyst nanocomposite comprises 5 mol. % of Au based on the molar amount of the ZnO.

### Claim 10

A photocatalyst nanocomposite, comprising:
gold nanoparticles,
ZnO nanoparticles, and
reduced graphene oxide (rGO),
wherein the photocatalyst nanocomposite comprises the rGO in an amount in the range of 45 wt. % to 55 wt. % of the total weight of the photocatalyst nanocomposite;
wherein the gold nanoparticles have a diameter in the range of 10 nm to 30 nm;
wherein the gold nanoparticles are dispersed on hexagonal wurtzite ZnO nanoparticles having diameter in the range of 20 nm to 60 nm; and
wherein the gold nanoparticles are present in an amount in the range of 2 mol. % to 10 mol. % based on the molar amount of the zinc oxide nanoparticles.

### Claim 11 (depends on 10)

The photocatalyst nanocomposite of claim 10, comprising gold nanoparticles in an amount of about 49 wt. %,
ZnO nanoparticles in an amount of about 45.5 wt. %, and
reduced graphene oxide in an amount of about 5.5 wt. %, of the total weight of the photocatalyst nanocomposite.

### Claim 12 (depends on 1)

A method of making the photocatalyst nanocomposite of claim 1, comprising:
preparing an aqueous suspension of a metal salt, a noble metal precursor, and graphene oxide,
mixing the aqueous suspension with date seed extract to form a mixture, and
heating the mixture at temperature in the range of 100-200° C. for a time in the range of 10 to 20 hours;
wherein the date seed extract is prepared by grinding date seed and heating the ground date seed in water at a temperature in the range of 60 to 100° C. for a time in the range of 1 to 5 hours and separating solids to form the date seed extract in the form of a liquid.

### Claim 13 (depends on 12)

The method of claim 12, wherein the molar amount of the noble metal precursor is in the range of 1 mol. % to 10 mol. % of the molar amount of the metal salt.

### Claim 14 (depends on 12)

The method of claim 12, wherein the metal salt is zinc acetate and the noble metal precursor is chloroauric acid (HAuCl4).

### Claim 15 (depends on 14)

The method of claim 14, wherein the amount of graphene oxide in the suspension is the range of 40 wt. % to 60 wt. % of the total weight of the total amount of graphene oxide, metal salt, and noble metal precursor.

### Claim 16 (depends on 14)

The method of claim 14, wherein the molar amount of the noble metal precursor is in the range of 1 mol. % to 10 mol. % of the molar amount of the metal salt.

### Claim 17

A method of preparing a composition comprising noble metal nanoparticles, comprising:
preparing an aqueous solution or suspension comprising a noble metal precursor,
mixing the aqueous suspension with date seed extract to form a mixture, and
heating the mixture at temperature in the range of 100-200° C. for a time in the range of 10 to 20 hours;
wherein the date seed extract is prepared by grinding date seed and heating the ground date seed in water at a temperature in the range of 60 to 100° C. for a time in the range of 1 to 5 hours, and separating solids to form the date seed extract in the form of a liquid, and the noble metal nanoparticles have a diameter in the range of 5 nm to 30 nm.

### Claim 18 (depends on 1)

A method of photodecomposing of an organic compound, comprising:
contacting the photocatalyst nanocomposite of claim 1 with an aqueous solution of an organic compound to form a mixture, and
irradiating the mixture with sunlight.

### Claim 19 (depends on 11)

A process of purifying water contaminated with an organic material, comprising:
contacting the contaminated water with the photocatalyst nanocomposite of claim 11, and
irradiating the mixture with sunlight.