# US 2020/0391189 A1 · Catalyst for selective hydrodesulphurization of cracked naphtha streams, method of preparation thereof, and process for selective hydrodesulphurization of cracked naphtha

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0391189 A1
- Document ID: US20200391189A1
- Status: Published application
- Kind: A1
- Application number: 16/753,985
- Filed: 2018-10-04
- Published: 2020-12-17
- Earliest claimed: 2017-10-06
- Assignees: Petroleo Brasileiro S.A. - Petrobras
- Applicants: PetróLeo Brasileiro S.A. - Petrobras
- Inventors: Sandra Shirley Ximeno CHIARO; Jose Luiz ZOTIN; Dayse Lovatte FONSECA; Anilza de ALMEIDA LYRA CORREA
- Web page: https://patentgrep.com/patent/US20200391189A1

## CPC

- B01J 23/002: {Mixed oxides other than spinels, e.g. perovskite}
- B01J 35/396: {Distribution of the active metal ingredient}
- B01J 23/007: {Mixed salts}
- B01J 23/882: and cobalt
- B01J 23/8872: {Alkali or alkaline earth metals}
- B01J 27/0515: {with iron group metals or platinum group metals}
- B01J 35/392: {Metal surface area}
- B01J 35/397: {Egg shell like}
- B01J 35/399: {homogeneously throughout the support particle}
- B01J 35/615: {100-500 m2/g}
- B01J 35/633: {less than 0.5 ml/g}
- B01J 35/635: {0.5-1.0 ml/g}
- B01J 35/647: {2-50 nm}
- B01J 37/0201: {Impregnation}
- B01J 37/0236: {Drying, e.g. preparing a suspension, adding a soluble salt and drying}
- B01J 37/088: {Decomposition of a metal salt}
- C10G 45/08: in combination with chromium, molybdenum, or tungsten metals, or compounds thereof
- B01J 2235/00: Indexing scheme associated with group B01J35/00, related to the analysis techniques used to determine the catalysts form or properties
- B01J 2235/15: X-ray diffraction
- B01J 2235/30: Scanning electron microscopy; Transmission electron microscopy
- C10G 2300/104: Light gasoline having a boiling range of about 20 - 100 °C
- C10G 2300/1044: Heavy gasoline or naphtha having a boiling range of about 100 - 180 °C
- C10G 2300/202: Heteroatoms content, i.e. S, N, O, P
- C10G 2300/308: Gravity, density, e.g. API
- C10G 2300/4006: Temperature
- C10G 2300/4012: Pressure
- C10G 2300/4018: Spatial velocity, e.g. LHSV, WHSV
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C10G: CRACKING HYDROCARBON OILS; PRODUCTION OF LIQUID HYDROCARBON MIXTURES, e.g. BY DESTRUCTIVE HYDROGENATION, OLIGOMERISATION, POLYMERISATION (cracking to hydrogen or synthesis gas C01B; cracking or pyrolysis of hydrocarbon gases to individual hydrocarbons or mixtures thereof of definite or specified constitution C07C; cracking to cokes C10B); RECOVERY OF HYDROCARBON OILS FROM OIL-SHALE, OIL-SAND, OR GASES; REFINING MIXTURES MAINLY CONSISTING OF HYDROCARBONS; REFORMING OF NAPHTHA; MINERAL WAXES

## Abstract

The present invention relates to a catalyst for selective hydrodesulphurization of cracked naphtha streams in the form of an extrudate, which comprises a support based on an inorganic oxide and an outer layer bound to the support, wherein the outer layer comprises desulphurization metals dispersed therein forming a crown, the desulphurization metals being cobalt and molybdenum. The present invention also relates to the preparation of said catalyst by the incipient wetness impregnation method and to the process for selective hydrodesulphurization of cracked naphtha employing same.

## Claims

### Claim 1

Catalyst for selective hydrodesulphurization of cracked naphtha streams, wherein it is in the form of an extrudate and comprises:
(i) a support based on hydrotalcite; and
(ii) an outer layer bound to said support, which comprises desulphurization metals dispersed therein forming a crown, wherein the desulphurization metals that form the active phase of the extrudate are cobalt and molybdenum, wherein molybdenum is distributed almost uniformly throughout the extrudate and cobalt is absent from the interior of the extrudate and shows a maximum in the inner portion of the crown.

### Claim 2 (depends on 1)

Catalyst according to claim 1, wherein the support based on hydrotalcite additionally comprises one or more M+2 elements selected from manganese, zinc, copper, cobalt or nickel, more preferably manganese, zinc, copper or cobalt, and an M+3 element selected from aluminium or lanthanum.

### Claim 3 (depends on 1)

Catalyst according to claim 1, wherein the support based on hydrotalcite comprises magnesium, aluminium, lanthanum, manganese, copper and/or zinc, preferably magnesium and aluminium, or magnesium, aluminium and zinc.

### Claim 4 (depends on 1)

Catalyst according to claim 1, wherein the content of the active phase in the catalyst is from 3 to 20 wt %, preferably between 8 and 12%, of MoO3 and cobalt, expressed as CoO, based upon the weight of the catalyst, and maintains a ratio of the metals CoO/(CoO+MoO3) between 0.1 and 0.7, preferably 0.2.

### Claim 5 (depends on 1)

Catalyst according to claim 1, wherein the thickness of the outer layer comprising the active phase is up to 500 μm.

### Claim 6 (depends on 1)

Catalyst according to claim 1, wherein the support comprises a value of specific surface area measured by N2 adsorption between 100 and 300 m2/g, preferably 220 m2/g, a pore volume between 0.2 and 1 cm3/g, an average pore diameter between 4 and 12 nm and size of crystallites between 25 and 55 nm.

### Claim 7 (depends on 1)

Method for preparing a catalyst, as defined in claim 1, wherein it is incipient wetness impregnation and comprises the following steps:
a) obtaining an extrudate of hydrotalcite;
b) impregnating said extrudate at the wet point with a solution of molybdenum;
c) impregnating said extrudate obtained in step b) at the wet point with a solution of cobalt;
d) adjusting the pH of the impregnation solution with acid to a value from 1 to 10, preferably from 1 to 5, more preferably 3;
e) drying the catalyst obtained in step d) for 1 to 6 hours, preferably for 2 hours, and
f) calcining the catalyst obtained in step e) at a temperature between 350 and 600° C., preferably at 450° C., for at least 1 hour.

### Claim 8 (depends on 7)

Method according to claim 7, wherein the temperature of the impregnation solution is maintained between room temperature and up to 100° C., preferably 60° C., for a period of 5 minutes to 1 hour, preferably for 10 minutes.

### Claim 9 (depends on 7)

Method according to claim 7, wherein the incipient wetness impregnations in steps b) and c) are carried out simultaneously.

### Claim 10 (depends on 1)

Process for selective hydrodesulphurization of a cracked naphtha stream containing olefins without excessive saturation of olefins, wherein it comprises:
(a) reacting a cracked naphtha stream containing olefin in a hydrodesulphurization zone containing the hydrodesulphurization catalyst defined in claim 1; and
(b) recovering the naphtha stream having a reduced sulphur concentration.

### Claim 11 (depends on 2)

Catalyst according to claim 2, wherein the support based on hydrotalcite comprises magnesium, aluminium, lanthanum, manganese, copper and/or zinc, preferably magnesium and aluminium, or magnesium, aluminium and zinc.

### Claim 12 (depends on 2)

Catalyst according to claim 2, wherein the content of the active phase in the catalyst is from 3 to 20 wt %, preferably between 8 and 12%, of MoO3 and cobalt, expressed as CoO, based upon the weight of the catalyst, and maintains a ratio of the metals CoO/(CoO+MoO3) between 0.1 and 0.7, preferably 0.2.

### Claim 13 (depends on 3)

Catalyst according to claim 3, wherein the content of the active phase in the catalyst is from 3 to 20 wt %, preferably between 8 and 12%, of MoO3 and cobalt, expressed as CoO, based upon the weight of the catalyst, and maintains a ratio of the metals CoO/(CoO+MoO3) between 0.1 and 0.7, preferably 0.2.

### Claim 14 (depends on 2)

Catalyst according to claim 2, wherein the thickness of the outer layer comprising the active phase is up to 500 μm.

### Claim 15 (depends on 3)

Catalyst according to claim 3, wherein the thickness of the outer layer comprising the active phase is up to 500 μm.

### Claim 16 (depends on 4)

Catalyst according to claim 4, wherein the thickness of the outer layer comprising the active phase is up to 500 μm.

### Claim 17 (depends on 2)

Catalyst according to claim 2, wherein the support comprises a value of specific surface area measured by N2 adsorption between 100 and 300 m2/g, preferably 220 m2/g, a pore volume between 0.2 and 1 cm3/g, an average pore diameter between 4 and 12 nm and size of crystallites between 25 and 55 nm.

### Claim 18 (depends on 3)

Catalyst according to claim 3, wherein the support comprises a value of specific surface area measured by N2 adsorption between 100 and 300 m2/g, preferably 220 m2/g, a pore volume between 0.2 and 1 cm3/g, an average pore diameter between 4 and 12 nm and size of crystallites between 25 and 55 nm.

### Claim 19 (depends on 4)

Catalyst according to claim 4, wherein the support comprises a value of specific surface area measured by N2 adsorption between 100 and 300 m2/g, preferably 220 m2/g, a pore volume between 0.2 and 1 cm3/g, an average pore diameter between 4 and 12 nm and size of crystallites between 25 and 55 nm.

### Claim 20 (depends on 5)

Catalyst according to claim 5, wherein the support comprises a value of specific surface area measured by N2 adsorption between 100 and 300 m2/g, preferably 220 m2/g, a pore volume between 0.2 and 1 cm3/g, an average pore diameter between 4 and 12 nm and size of crystallites between 25 and 55 nm.