# US 2020/0391185 A1 · Highly active metal oxide supported atomically dispersed platinum group metal catalysts

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0391185 A1
- Document ID: US20200391185A1
- Status: Published application
- Kind: A1
- Application number: 16/898,173
- Filed: 2020-06-10
- Published: 2020-12-17
- Earliest claimed: 2019-06-11
- Assignees: Arizona Board of Regents on behalf of Arizona State University
- Inventors: Yang Lou; Jingyue Liu
- Web page: https://patentgrep.com/patent/US20200391185A1

## CPC

- B01J 23/42: Platinum
- B01J 21/04: Alumina
- B01J 23/10: of rare earths
- B01J 23/63: with rare earths or actinides
- B01J 23/745: Iron
- B01J 23/83: with rare earths or actinides
- B01J 23/8906: {Iron and noble metals}
- B01J 35/45: Nanoparticles
- B01J 37/0221: {of particles}
- B01J 37/06: Washing {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/088: {Decomposition of a metal salt}
- C01B 32/50: Carbon dioxide
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}

## Abstract

A nanocatalyst including single atoms of platinum dispersed on a nanoscale metal oxide, and the nanocatalyst comprises 0.01 wt % to 1 wt % platinum. Preparing the nanocatalyst includes combining a solution comprising a nanoscale metal oxide and a compound containing a Group 10 metal to yield a mixture, aging the mixture for a length of time, filtering the mixture to yield a solid, washing the solid to eliminate water soluble anions, and calcining the solid to yield a nanocatalyst including single atoms or clusters of atoms of the Group 10 metal on the nanoscale metal oxide.

## Claims

### Claim 1

A method of preparing a nanocatalyst, the method comprising:
combining a solution comprising a nanoscale metal oxide and a compound containing a Group 10 metal to yield a mixture;
aging the mixture for a length of time;
filtering the mixture to yield a solid;
washing the solid to eliminate water soluble anions; and
calcining the solid to yield a nanocatalyst comprising single atoms of the Group 10 metal or atom clusters of the Group 10 metal on the nanoscale metal oxide.

### Claim 2 (depends on 1)

The method of claim 1, wherein the Group 10 metal is platinum.

### Claim 3 (depends on 2)

The method of claim 2, wherein the compound containing the Group 10 metal is a Group 10 metal salt comprising an anion.

### Claim 4 (depends on 3)

The method of claim 3, wherein the anion comprises chloride, nitrate, or acetate.

### Claim 5 (depends on 3)

The method of claim 3, wherein the compound containing the Group 10 metal salt comprises H2PtCl4, H2PtCl6, Pt(NH3)2Cl4, Pt(NH3)2Cl2, H2Pt(OH)6, or Pt(NH3)4(NO3)2.

### Claim 6 (depends on 2)

The method of claim 2, wherein a concentration of the platinum is in a range of 0.001 wt % to 5 wt % or 0.01 wt % to 0.5 wt % of the metal oxide.

### Claim 7 (depends on 1)

The method of claim 1, wherein the nanoscale metal oxide comprises one or more of Fe2O3, FeOx, CeO2, CeOx, TiO2, TiOx, CoOx, Co3O4, NiO, Cu2O, CuO, CuOx, ZrOx, NbOx, MnOx, and VOx.

### Claim 8 (depends on 1)

The method of claim 1, wherein a pH of the solution is in a range of 0.5 to 7.

### Claim 9 (depends on 8)

The method of claim 8, wherein the compound containing the Group 10 metal is H2PtCl4 or H2PtCl6, and the pH is in a range of 2 to 5.

### Claim 10 (depends on 8)

The method of claim 8, wherein the nanoscale metal oxide is Fe2O3 and a pH of the solution is in a range of 1 to 6 or 3 to 5.

### Claim 11 (depends on 8)

The method of claim 8, wherein the nanoscale metal oxide is CeO2, the compound containing the Group 10 metal is H2PtCl4 or H2PtCl6 and a pH of the solution is in a range of 1 to 5.

### Claim 12 (depends on 1)

The method of claim 1, wherein the nanoscale metal oxide is Fe2O3, the compound containing the Group 10 metal is Pt(NH3)4(NO3)2, and a pH of the solution is greater than 10.

### Claim 13 (depends on 1)

The method of claim 1, wherein the nanoscale metal oxide is CeO2, the compound containing the Group 10 metal is Pt(NH3)4(NO3)2, and a pH of the solution is greater than 10.

### Claim 14 (depends on 1)

The method of claim 1, wherein aging comprises aging the mixture at a temperature between room temperature and 60° C.

### Claim 15 (depends on 1)

The method of claim 1, further comprising drying the solid at a temperature less than 120° C. before calcining the solid.

### Claim 16 (depends on 1)

The method of claim 1, wherein the nanocatalyst comprises 0.001 wt % to 5 wt % of the Group 10 metal, or 0.005 wt % to 1 wt % of the Group 10 metal, or 0.01 wt % to 0.5 wt % Group 10 metal.

### Claim 17 (depends on 1)

The method of claim 1, wherein the nanoscale metal oxide is in powder form.

### Claim 18 (depends on 1)

The method of claim 1, wherein the nanoscale metal oxide is in the form of nanocrystallites.

### Claim 19 (depends on 1)

The method of claim 1, wherein each atom cluster of the Group 10 metal comprises two to about 10 atoms of the Group 10 metal.

### Claim 20 (depends on 19)

The method of claim 19, wherein each atom cluster has a largest dimension of less than 1 nm.

### Claim 21

A nanocatalyst comprising:
single atoms of platinum dispersed on a nanoscale metal oxide,
wherein the nanocatalyst comprises 0.01 wt % to 1 wt % platinum.

### Claim 22 (depends on 21)

The nanocatalyst of claim 21, wherein the nanoscale metal oxide comprises one or more of Fe2O3, FeOx, CeO2, CeOx, TiO2, TiOx, CoOx, Co3O4, NiO, Cu2O, CuO, CuOx, ZrOx, NbOx, MnOx, and VOx.

### Claim 23 (depends on 21)

The nanocatalyst of claim 21, wherein the nanoscale metal oxide is supported on a refractory oxide comprising one or both of Al2O3 and SiO2, mixtures of Al2O3 and SiO2, cordierites, or mullites.

### Claim 24 (depends on 21)

The nanocatalyst of claim 21, wherein the nanoscale metal oxide is Fe2O3 or FeOx and a turnover frequency for CO oxidation at 350° C. exceeds 500/s or 1500/s.

### Claim 25 (depends on 21)

The nanocatalyst of claim 21, wherein the nanoscale metal oxide is CeO2 or CeOx and a turnover frequency for CO oxidation at 350° C. exceeds 400/s or 1300/s.