# US 2020/0391183 A1 · Catalyst Support Comprising Homogeneously Distributed Titanium Dioxide and Method for Production

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0391183 A1
- Document ID: US20200391183A1
- Status: Published application
- Kind: A1
- Application number: 16/956,936
- Filed: 2019-01-21
- Published: 2020-12-17
- Earliest claimed: 2018-01-22
- Assignees: Sasol Germany GmbH
- Applicants: Sasol Germany GmbH
- Inventors: Dierk Niemeyer; Hans-Jorg Wolk; Katharina Goroll; Marcos Schoneborn; Martin Kuhn
- Web page: https://patentgrep.com/patent/US20200391183A1

## CPC

- B01J 21/063: {Titanium; Oxides or hydroxides thereof}
- B01J 21/04: Alumina
- B01J 23/34: Manganese
- B01J 37/0203: {the impregnation liquid containing organic compounds}
- B01J 37/0207: {Pretreatment of the support}
- B01J 37/0236: {Drying, e.g. preparing a suspension, adding a soluble salt and drying}
- B01J 37/086: {Decomposition of an organometallic compound, a metal complex or a metal salt of a carboxylic acid}
- B01J 2235/00: Indexing scheme associated with group B01J35/00, related to the analysis techniques used to determine the catalysts form or properties
- B01J 2235/30: Scanning electron microscopy; Transmission electron microscopy
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS

## Abstract

The present invention relates a method of making a catalyst support comprising at least homogeneously distributed titanium dioxide and alumina and to a catalyst support obtained according to this method.

## Claims

### Claim 1

A method of preparing a catalyst support, the method comprising the following steps:
i) preparing an alumina suspension, the alumina suspension having a pH of between 6 and 8, wherein the alumina suspension comprises an alumina selected from the group consisting of transition alumina, boehmite and mixtures thereof;
ii) preparing a titanium compound solution;
iii) adding an acid to the alumina suspension until the pH of the alumina suspension is between 4 and 5 to form an acid modified alumina suspension; and
iv) adding the titanium compound solution to the acid modified alumina suspension to form an alumina/titanium compound suspension.

### Claim 2 (depends on 1)

The method according to claim 1 comprising the further step of adding an acid to the alumina/titanium compound suspension to form an acid modified alumina/titanium compound suspension.

### Claim 3 (depends on 2)

The method according to claim 2 comprising the further step of heating the alumina/titanium compound suspension or the acid modified alumina/titanium compound suspension to form a heated alumina/titanium compound suspension or a heated acid modified alumina/titanium compound suspension.

### Claim 4 (depends on 1)

The method according to claim 1 comprising the further step of drying the acid modified alumina suspension before adding the titanium compound solution to form a dried alumina acid modified mixture.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the acid added to the alumina suspension is formic acid, lactic acid, citric acid, or mixtures thereof.

### Claim 6 (depends on 1)

The method of claim 1, wherein the alumina/titanium compound suspension comprises 99 to 95 wt. % alumina, calculated as Al2O3, and 1 to 5 wt. % titanium compounds, calculated as TiO2, relative to sum of alumina, calculated as Al2O3, and titanium compounds, calculated as TiO2.

### Claim 7 (depends on 4)

The method according to claim 4, wherein the acid added is a carboxylic acid selected from the group consisting of formic acid, lactic acid, citric acid, and mixtures thereof.

### Claim 8 (depends on 1)

The method of claim 1, wherein the percentage of acid added to the alumina suspension is between 5 to 30 wt % of the acid modified alumina suspension.

### Claim 9 (depends on 3)

The method of claim 3 comprising the step of drying a) the alumina/titanium compound suspension or the heated alumina/titanium compound suspension to form a dried alumina/titanium compound mixture or b) the acid modified alumina/titanium compound suspension or heated acid modified alumina/titanium compound suspension to form a dried acid modified alumina/titanium compound mixture.

### Claim 10 (depends on 9)

The method of claim 9 comprising the step of calcining the dried alumina/titanium compound mixture or the dried acid modified alumina/titanium compound mixture.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the transition alumina is γ-alumina, β-alumina, θ-alumina or mixtures thereof.

### Claim 12 (depends on 1)

The method according to claim 1, wherein the titanium compound solution is made by dissolving a titanium precursor in at least water.

### Claim 13 (depends on 12)

The method according to claim 12, wherein the titanium precursor is a water-soluble titanium precursor is selected from the group consisting of potassium titanium oxalates, ammonium titanium oxalates, ammonium titanium lactates, and mixtures thereof.

### Claim 14 (depends on 1)

A catalyst support prepared according to claim 1.

### Claim 15

A calcined catalyst support comprising an alumina support coated with between 1 and 5 wt. % TiO2 in relation to the alumina support (Al2O3), the TiO2 being homogeneously dispersed on the alumina support.

### Claim 16 (depends on 1)

A method of preparing a promoted catalyst support, the method comprising:
i) preparing a catalyst support according to claim 1, and
ii) introducing a promoter onto and/or into the catalyst support thereby to obtain a promoted catalyst support.