# US 2020/0385631 A1 · Preparation Method of Supercritical Carbon Dioxide Thickener for Tight Oil and Gas Reservoir

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0385631 A1
- Document ID: US20200385631A1
- Status: Published application
- Kind: A1
- Application number: 16/928,567
- Filed: 2020-07-14
- Published: 2020-12-10
- Earliest claimed: 2019-08-11
- Assignees: Southwest Petroleum University
- Applicants: Southwest Petroleum University
- Inventors: Ming Zhou; Hongjun Tu; Xiao Guo; Jinfeng Zhang; Juncheng Bu; Peng'ao Peng; Hongchang Han; Linkai Li; Mao Liao; Yinhua Gu; Rongjun Yi; Yongqiang Shi; Liangliang Xia
- Web page: https://patentgrep.com/patent/US20200385631A1

## CPC

- C09K 8/62: Compositions for forming crevices or fractures
- C09K 8/70: characterised by their form or by the form of their components, e.g. foams
- C07C 269/06: by reactions not involving the formation of carbamate groups
- C07C 273/1836: {from derivatives of carbamic acid}
- C07C 303/28: by reaction of hydroxy compounds with sulfonic acids or derivatives thereof
- Y02P 20/54: using solvents, e.g. supercritical solvents or ionic liquids
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present invention disclosed a method for prparing a thickener for tight oil and gas reservoir, which relieves damages. The technical solution includes the following steps: putting a three-flask in ice; adding perfluoroalkyl alcohol, P-toluenesulfonyl chloride and pyridine; reacting for 3 h at 0-20° C.; adding filter paper; ultrasonic dispersing for 1 h; removing the filter paper; washing the solution for 3-5 times by adding dilute hydrochloric acid to collect the intermediate product (I); adding 1,3-dihydroxy-propane-2-tert-butyl carbamate and the intermediate product (I) in another three-flask; adding potassium carbonate and N,N-dimethylformamide; reacting for 4h at 40° C. to collect the intermediate product (II); adding trifluoroacetic acid and methylene chloride into the intermediate product (II); reacting at 45° C. for 2 h; extracting and vacuum drying; and adding 1,6-hexamethylene diisocyanate; reacting for 2 h to collect the final product (III).

## Claims

### Claim 1

A method for preparing a supercritical carbon dioxide thickener for a tight oil and gas reservoir, comprising following steps:
(1) preparing P-toluene perfluoroalkyl ethylenesulfonates (TFES), which further comprises following sub-steps: after adding a perfluoroalkyl alcohol and a P-toluenesulfonyl chloride in a three-neck flask, wherein a molar ratio of the perfluoroalkyl alcohol and the P-toluenesulfonyl chloride is 1:1.1-1.2, and adding a pyridine; forming a system; wherein the system has reacted for 3 h under stirring thoroughly; maintaining a temperature at 0-20° C.; adding filter paper and carrying out ultrasonic dispersion for 1 h after a reaction is over; after removing unreacted residue P-toluenesulfonyl chloride and the filter paper; forming a system; washing the system with 15% dilute hydrochloric acid many times to remove the pyridine and collect a white solid; washing the white solid with distilled water for multiple times, drying the white solid by a vacuum drying oven at 40° C. for 3 h to prepare an intermediate product (I) TFES;
(2) preparing intermediate product (II) (1,3-bis(perfluoroalkyl ethoxy) isopropyl-2-tertbutyl carbamate) (PFEIT), which further comprises the following sub-steps: adding a 1,3-dihydroxy-propane-2-tert-butyl carbamate and the intermediate product (I) TFES in a three-neck flask, wherein a molar ratio of the 1,3-dihydroxy-propane-2-tert-butyl carbamate and the TFES is 2.1-2.2:1; then adding potassium carbonate and N,N-dimethylformamide; forming a system; wherein the system has been reacted for 4 h under stirring thoroughly at 40° C.; washing a reaction liquid with distilled water repeatedly after a reaction process is over; then carrying out vacuum drying to collect an intermediate product (II) PFEIT; and
(3) preparing a final product (III) 1,6-bis[1,3-bis(perfluoroalkyl ethoxy) isopropyl-2-urea] hexane (PFEIUH), which further comprises the following sub-steps: adding a mixture of methylene chloride and trifluoroacetic acid in a three-neck flask; wherein a volume ratio of the methylene chloride and the three trifluoroacetic acid is 2:1; adding the intermediate product (III) PFEIT to the mixture; maintaining a temperature at 45° C.; reacting for 2 h; adding the methylene chloride for extracting for 3 times to form an organic layer; drying the organic layer with a Na2SO4; adding 1,6-hexamethylene diisocyanate (HMDI), wherein a molar ratio of the HMDI and the PFEIT is 1:2.05-2.10, reacting under a temperature of 50° C. for 2 h, washing a crude product with a mixture of ethyl acetate and benzene for multiple times; filtering and carrying out vacuum drying to collect a final product (III) PFEIUH, wherein a perfluoro alkyl is one from these groups C5F11, C6F13, C7F15, C8F17, C9F19, C10F21.

### Claim 2

A method for mixing a supercritical carbon dioxide thickener PFEIUH with a supercritical carbon dioxide and a testing method thereof, comprising steps of: adding the supercritical carbon dioxide thickener PFEIUH with a mass fraction of 0.5 wt %, 1.0 wt %, 1.5 wt %, 2.0 wt %, 2.5 wt %, 3.0 wt % in a high temperature and high pressure closed system assembled with supporting equipment, respectively; injecting the corresponding supercritical carbon dioxide into the closed system through a sampling valve; rotating a rotor and adjusting a system pressure and a system temperature; stirring a mixture of the thickener PFEIUH and the corresponding supercritical carbon dioxide thoroughly to fully dissolve the supercritical carbon dioxide thickener: completing a mixing of two compounds and formatting a thickening supercritical carbon dioxide gel; setting a pressure at 28 MPa and a temperature at 60° C.; turning on a rheometer and maintaining a shear rate at 100 s−1 during the experiment; calculating a result and finding out a value of a viscosity of the supercritical carbon dioxide with the supercritical carbon dioxide thickener is 38.8-131.0 times of the supercritical carbon dioxide without the supercritical carbon dioxide thickener PFEIUH; evaluating the damage of the thickening supercritical carbon dioxide gel to a permeability of a tight matrix core and a fracturing core by core flooding experiment, wherein a permeability damage rate of the tight matrix core and the fracturing core are lower than the supercritical carbon dioxide without the supercritical carbon dioxide thickener PFEIUH.