# US 2020/0376714 A1 · Micro-particle-size thermoplastic micro-airbag polyurethane elastomer material and preparation therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0376714 A1
- Document ID: US20200376714A1
- Status: Published application
- Kind: A1
- Application number: 16/636,629
- Filed: 2018-08-01
- Published: 2020-12-03
- Earliest claimed: 2017-08-04
- Assignees: Nantong De New Material Co., Ltd.
- Applicants: Nantong De New Material Co., Ltd.
- Inventors: Qiaojian CHEN; Yanglong GUO
- Web page: https://patentgrep.com/patent/US20200376714A1

## CPC

- B29B 7/726: {Measuring properties of mixture, e.g. temperature or density (B29B7/724 takes precedence)}
- B29B 9/12: characterised by structure or composition
- B29B 9/065: {under-water, e.g. underwater pelletizers}
- B29C 48/0012: {combined with shaping by internal pressure generated in the material, e.g. foaming}
- B29C 48/022: {characterised by the choice of material}
- B29C 48/297: {at several locations, e.g. using several hoppers or using a separate additive feeding}
- B29C 48/362: {using static mixing devices}
- B29C 48/37: Gear pumps
- C08J 9/0004: {Use of compounding ingredients, the chemical constitution of which is unknown, broadly defined, or irrelevant}
- C08J 9/0061: {characterized by the use of several polymeric components}
- C08J 9/0066: {Use of inorganic compounding ingredients}
- C08J 9/122: {Hydrogen, oxygen, CO2, nitrogen or noble gases}
- C08J 9/141: {Hydrocarbons}
- C08J 9/16: Making expandable particles
- C08L 75/06: from polyesters
- C08L 75/08: from polyethers
- B29B 7/38: rotary (B29B7/52 takes precedence)
- B29B 2009/125: {Micropellets, microgranules, microparticles}
- B29C 44/3465: {by compressing particles in vacuum, followed by expansion in normal pressure}
- B29K 2075/00: Use of {PU, i.e.} polyureas or polyurethanes {or derivatives thereof}, as moulding material
- B29K 2105/041: {Microporous}
- C08J 2201/03: Extrusion of the foamable blend
- C08J 2203/06: CO2, N2 or noble gases
- C08J 2203/14: Saturated hydrocarbons, e.g. butane; Unspecified hydrocarbons
- C08J 2205/044: Micropores, i.e. average diameter being between 0,1 micrometer and 0,1 millimeter
- C08J 2375/04: Polyurethanes
- C08J 2427/18: Homopolymers or copolymers of tetrafluoroethylene
- C08J 2475/04: Polyurethanes
- C08K 2003/265: {Calcium, strontium or barium carbonate}
- C08K 2201/011: Nanostructured additives
- C08L 2203/14: used for foams
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08L 2205/03: containing three or more polymers in a blend
- C08L 2205/24: Crystallisation aids
- C08L 2207/04: Thermoplastic elastomer
- B29B: PREPARATION OR PRETREATMENT OF THE MATERIAL TO BE SHAPED; MAKING GRANULES OR PREFORMS; RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIAL CONTAINING PLASTICS
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

A thermoplastic micro-porous polyurethane elastomer material with a micro particle size and a method for preparing the same are provided. The material comprises, by weight, 1-97% of support frame polymer material, 1-97% of pressure-resistant low-resilience polymer material, 0.01-0.5% of nucleating agent, and 0.1-10% of foaming agent. The method comprises the following steps: (1) is feeding polymer materials and the nucleating agent from the front end of a double-screw extruder, feeding the foaming agent from the middle, hot-melting and fully mixing all the raw materials, then further homogenizing hot melt in a static mixer, and afterwards, controlling the pressure of the hot melt and quantitatively delivering the hot melt by a melt pump. (2) is pelletizing the hot melt entering an underwater pelletizing chamber from the melt pump via a die, separating particles carried out by process water, and screening and drying the particles to obtain a target product.

## Claims

### Claim 1

A thermoplastic micro-porous polyurethane elastomer material with a micro particle size, comprising, by weight, 1-97% of a support frame polymer material, 1-97% of a pressure-resistant low-resilience polymer material, 0.01-0.5% of a nucleating agent, and 0.1-10% of a foaming agent.

### Claim 2 (depends on 1)

The thermoplastic micro-porous polyurethane elastomer material with a micro particle size according to claim 1, wherein the support frame polymer material is a high-molecular weight or high-hardness polymer material, and the pressure-resistant low-resilience polymer material is a low-molecular weight or low-hardness polymer material corresponding to the support frame polymer material.

### Claim 3 (depends on 2)

The thermoplastic micro-porous polyurethane elastomer material with a micro particle size according to claim 2, wherein the support frame polymer material is a high-molecular weight thermoplastic polyurethane, and the pressure-resistant low-resilience polymer material corresponding to the support frame polymer material is a low-molecular weight thermoplastic polyurethane; or
the support frame polymer material is a high-hardness thermoplastic polymer elastomer, and the pressure-resistant low-resilience polymer material corresponding to the support frame polymer material is a low-hardness thermoplastic polymer elastomer.

### Claim 4 (depends on 3)

The thermoplastic micro-porous polyurethane elastomer material with a micro particle size according to claim 3, wherein the high-molecular weight thermoplastic polyurethane has a molecular weight of 8×104-5×105, and the low-molecular weight thermoplastic polyurethane has a molecular weight of 2×104-2.5×105; or
the high-hardness thermoplastic polymer elastomer has a shore hardness of 80 A-75 D, and the low-hardness thermoplastic polymer elastomer has a shore hardness of 30-85 A.

### Claim 5 (depends on 1)

The thermoplastic micro-porous polyurethane elastomer material with a micro particle size according to claim 1, wherein the nucleating agent is at least one selected from carbon nano-tubes, silicon dioxide, talcum powder, modified calcium carbonate, carbon black and tetrafluoroethylene powder; and
the foaming agent is at least one selected from CO2, N2, n-butane, n-pentane and isopentane.

### Claim 6 (depends on 1)

The thermoplastic micro-porous polyurethane elastomer material with a micro particle size according to claim 1, wherein the thermoplastic micro-porous polyurethane elastomer material have a particle size of 0.5-2 mm.

### Claim 7 (depends on 1)

A method for preparing the thermoplastic micro-porous polyurethane elastomer material with a micro particle size according to claim 1, comprising following steps:
(1) feeding the support frame polymer material, the pressure-resistant low-resilience polymer material and the nucleating agent via a feed inlet at a front end of a double-screw extruder, feeding the foaming agent from a middle of the double-screw extruder, hot-melting and fully mixing all raw materials, then further homogenizing a hot melt in a static mixer, and afterwards, controlling a pressure of the hot melt and quantitatively delivering the hot melt by a melt pump; and
(2) pelletizing the hot melt entering an underwater pelletizing chamber from the melt pump via a die, separating particles carried out by process water, and screening and drying the particles to obtain the thermoplastic micro-porous polyurethane elastomer material with a micro particle size.

### Claim 8 (depends on 7)

The method for preparing the thermoplastic micro-porous polyurethane elastomer material with a micro particle size according to claim 7, wherein an inlet pressure of the melt pump is controlled to 100-200 bar, a pressure of the process water in the underwater pelletizing chamber is 6-40 bar, and a rotating speed of a pelletizer in the underwater pelletizing chamber is 3000-8000 rpm.

### Claim 9 (depends on 8)

The method for preparing the thermoplastic micro-porous polyurethane elastomer material with a micro particle size according to claim 8, wherein the particles are carried out by the process water through a multi-stage pressure-relief expanding process water pipe with the pressure decreased gradually; the multi-stage pressure-relief expanding process water pipe is a four-stage process water pipe, wherein a first-stage process water pipe has a water pressure of 6-40 bar, a second-stage process water pipe has a water pressure of 5-35 bar, a third-stage process water pipe has a water pressure of 4-30 bar, and a fourth-stage process water pipe has a water pressure of 3-20 bar.

### Claim 10 (depends on 7)

The method for preparing the thermoplastic micro-porous polyurethane elastomer material with a micro particle size according to claim 7, wherein the die is of a porous plate structure, wherein pores in the porous plate structure have a diameter of 0.1-1.9 mm.

### Claim 11 (depends on 2)

A method for preparing the thermoplastic micro-porous polyurethane elastomer material with a micro particle size according to claim 2, comprising following steps:
(1) feeding the support frame polymer material, the pressure-resistant low-resilience polymer material and the nucleating agent via a feed inlet at a front end of a double-screw extruder, feeding the foaming agent from a middle of the double-screw extruder, hot-melting and fully mixing all raw materials, then further homogenizing a hot melt in a static mixer, and afterwards, controlling a pressure of the hot melt and quantitatively delivering the hot melt by a melt pump; and
(2) pelletizing the hot melt entering an underwater pelletizing chamber from the melt pump via a die, separating particles carried out by process water, and screening and drying the particles to obtain the thermoplastic micro-porous polyurethane elastomer material with a micro particle size.

### Claim 12 (depends on 3)

A method for preparing the thermoplastic micro-porous polyurethane elastomer material with a micro particle size according to claim 3, comprising following steps:
(1) feeding the support frame polymer material, the pressure-resistant low-resilience polymer material and the nucleating agent via a feed inlet at a front end of a double-screw extruder, feeding the foaming agent from a middle of the double-screw extruder, hot-melting and fully mixing all raw materials, then further homogenizing a hot melt in a static mixer, and afterwards, controlling a pressure of the hot melt and quantitatively delivering the hot melt by a melt pump; and
(2) pelletizing the hot melt entering an underwater pelletizing chamber from the melt pump via a die, separating particles carried out by process water, and screening and drying the particles to obtain the thermoplastic micro-porous polyurethane elastomer material with a micro particle size.

### Claim 13 (depends on 4)

A method for preparing the thermoplastic micro-porous polyurethane elastomer material with a micro particle size according to claim 4, comprising following steps:
(1) feeding the support frame polymer material, the pressure-resistant low-resilience polymer material and the nucleating agent via a feed inlet at a front end of a double-screw extruder, feeding the foaming agent from a middle of the double-screw extruder, hot-melting and fully mixing all raw materials, then further homogenizing a hot melt in a static mixer, and afterwards, controlling a pressure of the hot melt and quantitatively delivering the hot melt by a melt pump; and
(2) pelletizing the hot melt entering an underwater pelletizing chamber from the melt pump via a die, separating particles carried out by process water, and screening and drying the particles to obtain the thermoplastic micro-porous polyurethane elastomer material with a micro particle size.

### Claim 14 (depends on 5)

A method for preparing the thermoplastic micro-porous polyurethane elastomer material with a micro particle size according to claim 5, comprising following steps:
(1) feeding the support frame polymer material, the pressure-resistant low-resilience polymer material and the nucleating agent via a feed inlet at a front end of a double-screw extruder, feeding the foaming agent from a middle of the double-screw extruder, hot-melting and fully mixing all raw materials, then further homogenizing a hot melt in a static mixer, and afterwards, controlling a pressure of the hot melt and quantitatively delivering the hot melt by a melt pump; and
(2) pelletizing the hot melt entering an underwater pelletizing chamber from the melt pump via a die, separating particles carried out by process water, and screening and drying the particles to obtain the thermoplastic micro-porous polyurethane elastomer material with a micro particle size.

### Claim 15 (depends on 6)

A method for preparing the thermoplastic micro-porous polyurethane elastomer material with a micro particle size according to claim 6, comprising following steps:
(1) feeding the support frame polymer material, the pressure-resistant low-resilience polymer material and the nucleating agent via a feed inlet at a front end of a double-screw extruder, feeding the foaming agent from a middle of the double-screw extruder, hot-melting and fully mixing all raw materials, then further homogenizing a hot melt in a static mixer, and afterwards, controlling a pressure of the hot melt and quantitatively delivering the hot melt by a melt pump; and
(2) pelletizing the hot melt entering an underwater pelletizing chamber from the melt pump via a die, separating particles carried out by process water, and screening and drying the particles to obtain the thermoplastic micro-porous polyurethane elastomer material with a micro particle size.