# US 2020/0370199 A1 · Method for making mnbi2te4 single crystal

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0370199 A1
- Document ID: US20200370199A1
- Status: Published application
- Kind: A1
- Application number: 16/525,930
- Filed: 2019-07-30
- Published: 2020-11-26
- Earliest claimed: 2019-05-22
- Assignees: Tsinghua University; Hon Hai Precision Industry Co., Ltd.
- Applicants: Tsinghua University; Hon Hai Precision Industry Co., Ltd.
- Inventors: HAO LI; YANG WU; YUE-GANG ZHANG; SHOU-SHAN FAN
- Web page: https://patentgrep.com/patent/US20200370199A1

## CPC

- C30B 1/02: by thermal treatment, e.g. strain annealing (C30B1/12 takes precedence)
- C30B 29/46: Sulfur-, selenium- or tellurium-containing compounds
- C01B 19/002: {Compounds containing, besides selenium or tellurium, more than one other element, with -O- and -OH not being considered as anions}
- C01G 29/006: {Compounds containing bismuth, with or without oxygen or hydrogen, and containing two or more other elements}
- C30B 33/02: Heat treatment (C30B33/04, C30B33/06 take precedence)
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2002/82: by IR- or Raman-data
- C01P 2002/85: by XPS, EDX or EDAX data
- C01P 2004/02: obtained by optical microscopy
- C01P 2004/03: obtained by SEM
- C01P 2006/42: Magnetic properties
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

A method for making MnBi2Te4 single crystal is provided. The method includes: providing a mixture of polycrystalline MnTe and polycrystalline Bi2Te3 in Molar ratio of 1.1:1˜1:1.1; heating the mixture in a vacuum reaction chamber to 700° C.˜900° C., cooling the mixture to 570° C.˜600° C. slowly with a speed less than or equal to 1° C./hour, and annealing the mixture at 570° C.˜600° C. for a time above 10 days to obtain an intermediate product; and air quenching the intermediate product from 570° C.˜600° C. to room temperature. The method for making MnBi2Te4 single crystal is simple and has low cost.

## Claims

### Claim 1

A method for making MnBi2Te4 single crystal, the method comprising:
providing a mixture of polycrystalline MnTe and polycrystalline Bi2Te3 in Molar ratio of 1.1:1˜1:1.1;
heating the mixture in a vacuum reaction chamber to 700° C.˜900° C., cooling the mixture to 570° C.˜600° C. at a speed less than or equal to 1° C./hour, and annealing the mixture at 570° C.˜600° C. for at least 10 days to obtain an intermediate product; and
air quenching the intermediate product from 570° C.˜600° C. to room temperature.

### Claim 2 (depends on 1)

The method of claim 1, wherein the providing the mixture of polycrystalline MnTe and polycrystalline Bi2Te3 comprises: making the polycrystalline MnTe and polycrystalline Bi2Te3 first respectively; and mixing the polycrystalline MnTe and polycrystalline Bi2Te3.

### Claim 3 (depends on 2)

The method of claim 2, wherein the polycrystalline MnTe is made by following steps: mixing elemental Mn and Te in Molar ratio of 1:1 to obtain a Mn/Te mixture;
sintering the Mn/Te mixture in a vacuum room at 700° C.˜1000° C. for approximately 3˜5 days to obtain a reaction product; and natural cooling the reaction product.

### Claim 4 (depends on 2)

The method of claim 2, wherein the polycrystalline Bi2Te3 is made by following steps: mixing elemental Bi and Te in Molar ratio of 2:3 to obtain a Bi/Te mixture; sintering the Bi/Te mixture in a vacuum room at 700° C.˜1000° C. for approximately 24˜40 hours; cooling the vacuum room to 560° C.˜580° C. by a speed of 0.1° C./minute to obtain a reaction product; and air quenching the reaction product from 560° C.˜580° C. to room temperature.

### Claim 5 (depends on 1)

The method of claim 1, wherein the Molar ratio of the polycrystalline MnTe and the polycrystalline Bi2Te3 is 1:1.

### Claim 6 (depends on 1)

The method of claim 1, wherein the mixture is cooled to 570° C.˜600° C. at the speed less than or equal to 0.6° C./hour.

### Claim 7 (depends on 1)

The method of claim 1, wherein the mixture is annealed at 591° C.

### Claim 8 (depends on 1)

The method of claim 1, wherein the mixture is annealed for at least 14 days.

### Claim 9 (depends on 1)

The method of claim 1, wherein a pressure of the vacuum reaction chamber is less than 10 Pa.

### Claim 10 (depends on 1)

The method of claim 1, wherein the intermediate product is removed from the reaction chamber directly and cooled in air in the process of air quenching.

### Claim 11

A method for making MnBi2Te4 single crystal, the method comprising:
mixing elemental Mn, Bi and Te in Molar ratio of 1:2:4 to obtain a Mn/Bi/Te mixture;
sintering the Mn/Bi/Te mixture in a vacuum reaction chamber at 700° C.˜900° C. for approximately 3˜5 days to obtain a mixture of polycrystalline MnTe and polycrystalline Bi2Te3;
cooling the mixture to 570° C.˜600° C. at a speed less than or equal to 1° C./hour;
annealing the mixture at 570° C.˜600° C. for at least 10 days to obtain an intermediate product; and
air quenching the intermediate product from 570° C.˜600° C. to room temperature.

### Claim 12 (depends on 11)

The method of claim 11, wherein the mixture is cooled to 570° C.˜600° C. at the speed less than or equal to 0.6° C./hour.

### Claim 13 (depends on 11)

The method of claim 11, wherein the mixture is annealed at 591° C.

### Claim 14 (depends on 11)

The method of claim 11, wherein the mixture is annealed for at least 14 days.

### Claim 15 (depends on 11)

The method of claim 11, wherein a pressure of the vacuum reaction chamber is less than 10 Pa.

### Claim 16 (depends on 11)