# US 2020/0370167 A1 · Tungsten Sputtering Target And Method For Producing Same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0370167 A1
- Document ID: US20200370167A1
- Status: Published application
- Kind: A1
- Application number: 16/758,589
- Filed: 2018-09-07
- Published: 2020-11-26
- Earliest claimed: 2017-11-10
- Assignees: JX Metals Corporation
- Applicants: JX Nippon Mining & Metals Corporation
- Inventors: Shinji Sogawa; Takafumi Dasai; Seiji Nakasumi
- Web page: https://patentgrep.com/patent/US20200370167A1

## CPC

- C23C 14/3414: {Metallurgical or chemical aspects of target preparation, e.g. casting, powder metallurgy}
- B22F 3/15: Hot isostatic pressing
- B22F 3/18: by using pressure rollers
- C22C 27/04: Alloys based on tungsten or molybdenum
- C23C 14/165: {by cathodic sputtering}
- B22F 2998/10: Processes characterised by the sequence of their steps
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

According to one of various aspects of the present invention, a tungsten sputtering target has a purity of tungsten is 5 N (99.999% by weight) or more, and an impurity of carbon and an impurity of oxygen contained in tungsten are 50 ppm by weight or less, respectively, and an average grain size of tungsten crystal is more than 100 μm.

## Claims

### Claim 1

A tungsten sputtering target, wherein a purity of tungsten is 5 N (99.999% by weight) or more, and an impurity of carbon and an impurity of oxygen contained in tungsten are 50 ppm by weight or less, respectively, and an average grain size of tungsten crystal is more than 100 μm, and a relative density is 99.3% or more.

### Claim 2

(canceled)

### Claim 3 (depends on 1)

The sputtering target according to claim 1, wherein the carbon and the oxygen are 10 ppm by weight or less, respectively.

### Claim 4 (depends on 1)

A method for manufacturing a tungsten sputtering target according to claim 1, in which tungsten powder is formed by a hot pressing (HP) method and then densified by a hot isostatic pressing (HIP) method, wherein
a temperature in the hot isostatic pressing method is 1800° C. or more and a sintering time is 5.5 hours or more.

### Claim 5

A method for manufacturing a tungsten sputtering target in which tungsten powder is formed by a hot pressing (HP) method and then densified by a rolling method, wherein
a temperature in the rolling method is 1200° C. or more and 1700° C. or less, and a total rolling reduction is 15% or more and 25% or less.

### Claim 6 (depends on 5)

The method for manufacturing a tungsten sputtering target according to claim 5, wherein in the rolling method, a rolling reduction per rolling is 3 to 12%.

### Claim 7 (depends on 3)

A method for manufacturing a tungsten sputtering target according to claim 3, in which tungsten powder is formed by a hot pressing (HP) method and then densified by a hot isostatic pressing (HIP) method, wherein
a temperature in the hot isostatic pressing method is 1800° C. or more and a sintering time is 5.5 hours or more.