# US 2020/0369932 A1 · Deicer composition and method of making

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0369932 A1
- Document ID: US20200369932A1
- Status: Published application
- Kind: A1
- Application number: 16/874,956
- Filed: 2020-05-15
- Published: 2020-11-26
- Earliest claimed: 2019-05-20
- Assignees: NW Straw Pulp, LLC
- Applicants: NW Straw Pulp, LLC
- Inventors: Keith C. Kuykendall; David W. Wilkening
- Web page: https://patentgrep.com/patent/US20200369932A1

## CPC

- D21C 11/0042: {Fractionating or concentration of spent liquors by special methods (concentration by evaporation D21C11/10)}
- C09K 3/185: {Thawing materials}
- D21C 11/0007: {Recovery of by-products, i.e. compounds other than those necessary for pulping, for multiple uses or not otherwise provided for (volatile compounds obtained by decomposition of spent liquors in order to regenerate them D21C11/125; compounds obtained by fractionating the liquors in order to regenerate them D21C11/0042)}
- D21C 11/10: Concentrating spent liquor by evaporation (evaporators B01D)
- D21C: PRODUCTION OF CELLULOSE BY REMOVING NON-CELLULOSE SUBSTANCES FROM CELLULOSE-CONTAINING MATERIALS; REGENERATION OF PULPING LIQUORS; APPARATUS THEREFOR
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE

## Abstract

A deicer composition is disclosed. The deicer composition may comprise water, a metal chloride salt, and a biopolymer composition derived from wheat straw, alfalfa, or other cereal grain straws. The biopolymer composition may include inorganic material and a copolymer comprised of lignin and polysaccharides. The biopolymer composition may have an average molecular weight of between 3500 and 5500 Daltons. The metal chloride salt may be selected from magnesium chloride, calcium chloride, and sodium chloride.

## Claims

### Claim 1

A deicer composition, comprising:
water;
a metal chloride salt; and
a biopolymer composition derived from wheat straw, alfalfa, or other cereal grain straws, the biopolymer composition including inorganic material and a copolymer comprised of lignin and polysaccharides, the lignins being polydisperse and having an average molecular weight between 3500 and 5500 Daltons.

### Claim 2 (depends on 1)

The deicer composition of claim 1, wherein the deicer comprises:
65-75% by weight water;
25-35% by weight metal chloride salt; and
1-10% by weight of the biopolymer composition.

### Claim 3 (depends on 1)

The deicer composition of claim 1, wherein the metal chloride salt is selected from the group consisting of magnesium chloride, calcium chloride, and sodium chloride.

### Claim 4 (depends on 1)

The deicer composition of claim 1, wherein the biopolymer composition is a sulfonated biopolymer composition.

### Claim 5 (depends on 4)

The deicer composition of claim 4, wherein the sulfonated biopolymer composition is produced by reacting the biopolymer composition with ammonium persulfate, sodium sulfite, and formaldehyde.

### Claim 6 (depends on 1)

The deicer composition of claim 1, wherein the biopolymer composition comprises about 25-50% by weight water, about 5-20% by weight of the lignin, about 5-20% by weight of the polysaccharides, and about 15-30% by weight of the inorganic material.

### Claim 7 (depends on 1)

The deicer composition of claim 1, wherein the polysaccharides include hemicellulose polymers.

### Claim 8 (depends on 6)

The deicer composition of claim 6, wherein the polysaccharides include sugar units of xylose, arabinose, glucose, galactose, galacturonic acid, gluconuronic acid, rhamnose, fucose, 4-methyl glucouronic acid, mannose, and related saccarinic acids derived from the sugars when treated under alkaline conditions.

### Claim 9

A deicer composition, comprising:
water;
a metal chloride salt; and
a sulfonated biopolymer composition obtained as a lignin/hemicellulose co-product from pulp processing of wheat straw, alfalfa, or other cereal grain straws, the biopolymer including inorganic material and a copolymer comprised of lignin and polysaccharides.

### Claim 10 (depends on 9)

The deicer composition of claim 9, wherein the deicer composition comprises:
65-75% by weight water;
25-35% by weight metal chloride salt; and
1-10% by weight of the sulfonated biopolymer composition.

### Claim 11 (depends on 9)

The deicer composition of claim 9, wherein the metal chloride salt is selected from the group consisting of magnesium chloride, calcium chloride, and sodium chloride.

### Claim 12 (depends on 9)

The deicer composition of claim 9, wherein the sulfonated biopolymer composition is produced by reacting a biopolymer composition with ammonium persulfate, sodium sulfite, and formaldehyde.

### Claim 13 (depends on 9)

The deicer composition of claim 9, wherein the sulfonated biopolymer composition comprises about 25-50% by weight water, about 5-20% by weight of the lignin, about 5-20% by weight of the polysaccharides, and about 15-30% by weight of the inorganic material.

### Claim 14 (depends on 13)

The deicer composition of claim 13, wherein the wherein the polysaccharides include hemicellulose polymers.

### Claim 15

A method of making a deicer composition, comprising:
obtaining a dilute lignin pulp liquor composition derived from wheat straw, alfalfa, or other cereal grain straws;
filtering the dilute liquor to remove undissolved fiber related solids;
concentrating the dilute liquor to provide a biopolymer composition comprising about 25-55% by weight of total solids; and
blending the biopolymer composition with a metal chloride salt to produce a deicer composition.

### Claim 16 (depends on 15)

The method of claim 15, wherein the metal chloride salt is selected from the group consisting of magnesium chloride, calcium chloride, and sodium chloride.

### Claim 17 (depends on 15)

The method of claim 15, wherein the deicer composition comprises:
65-75% by weight water;
25-35% by weight metal chloride salt; and
1-10% by weight of the biopolymer composition.

### Claim 18 (depends on 15)

The method of claim 15, wherein the biopolymer composition is a sulfonated biopolymer composition and the method further comprises modifying the biopolymer composition to produce a sulfonated biopolymer composition, prior to blending with the metal chloride salt.

### Claim 19 (depends on 18)

The method of claim 18, wherein modifying the biopolymer composition to produce a sulfonated biopolymer composition further comprises:
heating the biopolymer composition to between 35 and 65 degrees Celsius;
mixing the biopolymer composition with ammonium persulfate to produce an oxidized biopolymer composition;
heating the oxidized biopolymer composition to between 50 and 90 degrees Celsius;
mixing the oxidized biopolymer composition with sodium sulfite; and
combining the mixture of oxidized biopolymer composition and sodium sulfite with formaldehyde to produce a sulfonated biopolymer composition.

### Claim 20 (depends on 19)

The method of claim 19, further comprising holding the sulfonated biopolymer composition between 50 and 90 degrees for between 30 to 90 minutes.