# US 2020/0369865 A1 · Thermoplastic resin composition for wire-coating and heat resistant wire

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0369865 A1
- Document ID: US20200369865A1
- Status: Published application
- Kind: A1
- Application number: 16/636,935
- Filed: 2017-08-08
- Published: 2020-11-26
- Earliest claimed: 2017-08-08
- Assignees: Riken Technos Corporation
- Applicants: Riken Technos Corporation
- Inventors: Kaoru IWASA; Shinichi KISHIMOTO
- Web page: https://patentgrep.com/patent/US20200369865A1

## CPC

- C08L 25/18: Homopolymers or copolymers of aromatic monomers containing elements other than carbon and hydrogen
- H01B 3/441: {from alkenes}
- C08K 3/12: Hydrides
- C08K 3/22: of metals
- C08K 5/01: Hydrocarbons {(C08K5/0091 takes precedence)}
- C08K 5/13: Phenols; Phenolates
- C08K 5/14: Peroxides
- C08K 5/36: Sulfur-, selenium-, or tellurium-containing compounds {(C08K5/0091 takes precedence)}
- C08K 5/372: Sulfides {, e.g. R-(S)x-R'}
- C08K 5/5425: containing at least one C=C bond
- C08L 9/06: Copolymers with styrene
- C08L 23/0815: {with aliphatic 1-olefins containing one carbon-to-carbon double bond}
- C08L 23/10: Homopolymers or copolymers of propene
- C08L 23/26: modified by chemical after-treatment (saponified copolymers C08L23/0861; unsaturated acid salts C08L23/0876)
- C08L 53/025: {modified}
- H01B 3/442: {from aromatic vinyl compounds}
- H01B 7/295: using material resistant to flame
- C08K 2003/2224: {Magnesium hydroxide}
- C08L 2201/02: Flame or fire retardant/resistant
- C08L 2201/08: Stabilised against heat, light or radiation or oxydation
- C08L 2203/202: use in electrical wires or wirecoating
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

The invention provides a thermoplastic resin composition having (A) a thermoplastic polymer comprising (a1) 5 mass % to less than 50 mass % of a propylene polymer having a melting point of 150° C. or higher, (a2) 10 mass % to less than 60 mass % of an ethylene polymer, (a3) 5 mass % to less than 50 mass % of, for example, a hydrogenated product of a block copolymer of an aromatic vinyl compound and a conjugated diene compound, and (a4) 1 mass % to less than 30 mass % of, for example, an unsaturated carboxylic acid-modified olefin polymer; (B) a softener for nonaromatic rubbers; (C) a metal hydrate; (D) an organic peroxide; (E) an antioxidant; and (F) a coupling agent.

## Claims

### Claim 1

A thermoplastic resin composition comprising, (A) a thermoplastic polymer, (B) a softener for nonaromatic rubbers, (C) a metal hydrate, (D) an organic peroxide, (E) an antioxidant, and (F) a coupling agent,
wherein said component (A) comprises:
(a1) 5 mass % to less than 50 mass % of a propylene polymer having a melting point of 150° C. or higher;
(a2) 10 mass % to less than 60 mass % of an ethylene polymer;
(a3) 5 mass % to less than 50 mass % of one or more selected from the group consisting of a block copolymer of an aromatic vinyl compound and a conjugated diene compound, a block copolymer of an aromatic vinyl compound and isobutylene, and a hydrogenated product of a block copolymer of an aromatic vinyl compound and a conjugated diene compound; and
(a4) 1 mass % to less than 30 mass % of one or more selected from the group consisting of an unsaturated carboxylic acid-modified olefin polymer, an unsaturated carboxylic acid-modified aromatic vinyl compound elastomer, and an epoxy group-containing olefin polymer;
wherein the total of said components (a1), (a2), (a3) and (a4) is 100 mass %; and
said component (E) is comprised in an amount of more than 1 part by mass and 15 parts by mass or less with respect to the total of 100 parts by mass of said component (A) and said component (B).

### Claim 2 (depends on 1)

The thermoplastic resin composition according to claim 1, comprising:
70 to 95% by mass of said component (A); and
30 to 5% by mass of said component (B), with the total of said component (A) and said component (B) being 100 mass %, and based on the total of 100 parts by mass of said component (A) and said component (B),
30 to 150 parts by mass of said component (C);
0.01 to 1.0 part by mass of said component (D);
1 to 15 parts by mass of said component (E); and
0.1 to 8 parts by mass of said component (F).

### Claim 3 (depends on 1)

The thermoplastic resin composition according to claim 1, wherein said component (a2) comprises one or more selected from the group consisting of:
(a2-1) a copolymer of ethylene and an a-olefin having 4 to 10 carbon atoms, having a density of 860 to 935 Kg/m3; and
(a2-2) a polar ethylene copolymer.

### Claim 4 (depends on 1)

The thermoplastic resin composition according to claim 1, wherein said component (E) comprises:
(E-1) a hindered phenol antioxidant; and
(E-2) a thioether antioxidant.

### Claim 5 (depends on 1)

A wire comprising the thermoplastic resin composition according to claim 1.

### Claim 6 (depends on 5)

The wire according to claim 5 for vehicles.

### Claim 7 (depends on 5)

A method for producing the wire according to claim 5, comprising:
(1) a step of melt-kneading (A) a thermoplastic polymer, (B) a softener for nonaromatic rubbers, (C) a metal hydrate, (D) an organic peroxide, (E) an antioxidant, (F) a coupling agent, and optional components to be used as desired at a temperature higher than or equal to the 1 minute half-life temperature of said component (D) for 30 seconds or longer to obtain the thermoplastic resin composition; and
(2) a step of forming a wire using the thermoplastic resin composition obtained in said step (1), without
(3) a step of post-crosslinking treatment.

### Claim 8 (depends on 1)

A method for producing a thermoplastic resin composition according to claim 1, comprising at least any one of the steps selected from the group consisting of:
a step of introducing all of (A) a thermoplastic polymer, (B) a softener for nonaromatic rubbers, (C) a metal hydrate, (D) an organic peroxide, (E) an antioxidant, (F) a coupling agent, and optional components to be used as desired into a melt kneader and melt kneading the mixture for 30 seconds or longer at a temperature higher than or equal to the 1 minute half-life temperature of said component (D) to obtain a thermoplastic resin composition;
a step of introducing all of said components (A) to (D), (F) and the optional components to be used as desired into a melt kneader and after the melt kneading temperature has reached a temperature higher than or equal to the 1 minute half-life temperature of said component (D), introducing said component (E) into the melt kneader to obtain a thermoplastic resin composition;
a step of firstly introducing all of said components (A) to (D), (F), and the optional components to be used as desired, and a part of said component (E) into a melt kneader and after the melt kneading temperature has reached a temperature higher than or equal to the 1 minute half-life temperature of said component (D), introducing the remainder of said component (E) into the melt kneader to obtain a thermoplastic resin composition; and
a step of firstly introducing all of said component (D), and at least a part of said components (A) to (C), (F), and the optional components to be used as desired into a melt kneader, and after the melt kneading temperature has reached a temperature higher than or equal to the 1 minute half-life temperature of said component (D), introducing the remainder of said components (A) to (C), (F), and the optional components to be used as desired, and said component (E) into the melt kneader to obtain a thermoplastic resin composition.

### Claim 9 (depends on 8)

A method for producing a wire, comprising:
(1) a step of obtaining a thermoplastic resin composition by the method according to claim 8;
(2) a step of forming a wire using the thermoplastic resin composition obtained in said step (1); without
(3) a step of post-crosslinking treatment.

### Claim 10 (depends on 2)

The thermoplastic resin composition according to claim 2, wherein said component (a2) comprises one or more selected from the group consisting of:
(a2-1) a copolymer of ethylene and an a-olefin having 4 to 10 carbon atoms, having a density of 860 to 935 Kg/m3; and
(a2-2) a polar ethylene copolymer.

### Claim 11 (depends on 2)

The thermoplastic resin composition according to claim 2 wherein said component (E) comprises:
(E-1) a hindered phenol antioxidant; and
(E-2) a thioether antioxidant.

### Claim 12 (depends on 3)

The thermoplastic resin composition according to claim 3 wherein said component (E) comprises:
(E-1) a hindered phenol antioxidant; and
(E-2) a thioether antioxidant.

### Claim 13 (depends on 2)

A wire comprising the thermoplastic resin composition according claim 2.

### Claim 14 (depends on 3)

A wire comprising the thermoplastic resin composition according claim 3.

### Claim 15 (depends on 4)

A wire comprising the thermoplastic resin composition according claim 4.

### Claim 16 (depends on 6)

A method for producing the wire according to claim 6, comprising:
(1) a step of melt-kneading (A) a thermoplastic polymer, (B) a softener for nonaromatic rubbers, (C) a metal hydrate, (D) an organic peroxide, (E) an antioxidant, (F) a coupling agent, and optional components to be used as desired at a temperature higher than or equal to the 1 minute half-life temperature of said component (D) for 30 seconds or longer to obtain the thermoplastic resin composition; and
(2) a step of forming a wire using the thermoplastic resin composition obtained in said step (1), without
(3) a step of post-crosslinking treatment.

### Claim 17 (depends on 2)

A method for producing a thermoplastic resin composition according to claim 2, comprising at least any one of the steps selected from the group consisting of:
a step of introducing all of (A) a thermoplastic polymer, (B) a softener for nonaromatic rubbers, (C) a metal hydrate, (D) an organic peroxide, (E) an antioxidant, (F) a coupling agent, and optional components to be used as desired into a melt kneader and melt kneading the mixture for 30 seconds or longer at a temperature higher than or equal to the 1 minute half-life temperature of said component (D) to obtain a thermoplastic resin composition;
a step of introducing all of said components (A) to (D), (F) and the optional components to be used as desired into a melt kneader and after the melt kneading temperature has reached a temperature higher than or equal to the 1 minute half-life temperature of said component (D), introducing said component (E) into the melt kneader to obtain a thermoplastic resin composition;
a step of firstly introducing all of said components (A) to (D), (F), and the optional components to be used as desired, and a part of said component (E) into a melt kneader and after the melt kneading temperature has reached a temperature higher than or equal to the 1 minute half-life temperature of said component (D), introducing the remainder of said component (E) into the melt kneader to obtain a thermoplastic resin composition; and
a step of firstly introducing all of said component (D), and at least a part of said components (A) to (C), (F), and the optional components to be used as desired into a melt kneader, and after the melt kneading temperature has reached a temperature higher than or equal to the 1 minute half-life temperature of said component (D), introducing the remainder of said components (A) to (C), (F), and the optional components to be used as desired, and said component (E) into the melt kneader to obtain a thermoplastic resin composition.

### Claim 18 (depends on 3)

A method for producing a thermoplastic resin composition according to claim 3, comprising at least any one of the steps selected from the group consisting of:
a step of introducing all of (A) a thermoplastic polymer, (B) a softener for nonaromatic rubbers, (C) a metal hydrate, (D) an organic peroxide, (E) an antioxidant, (F) a coupling agent, and optional components to be used as desired into a melt kneader and melt kneading the mixture for 30 seconds or longer at a temperature higher than or equal to the 1 minute half-life temperature of said component (D) to obtain a thermoplastic resin composition;
a step of introducing all of said components (A) to (D), (F) and the optional components to be used as desired into a melt kneader and after the melt kneading temperature has reached a temperature higher than or equal to the 1 minute half-life temperature of said component (D), introducing said component (E) into the melt kneader to obtain a thermoplastic resin composition;
a step of firstly introducing all of said components (A) to (D), (F), and the optional components to be used as desired, and a part of said component (E) into a melt kneader and after the melt kneading temperature has reached a temperature higher than or equal to the 1 minute half-life temperature of said component (D), introducing the remainder of said component (E) into the melt kneader to obtain a thermoplastic resin composition; and
a step of firstly introducing all of said component (D), and at least a part of said components (A) to (C), (F), and the optional components to be used as desired into a melt kneader, and after the melt kneading temperature has reached a temperature higher than or equal to the 1 minute half-life temperature of said component (D), introducing the remainder of said components (A) to (C), (F), and the optional components to be used as desired, and said component (E) into the melt kneader to obtain a thermoplastic resin composition.

### Claim 19 (depends on 4)

A method for producing a thermoplastic resin composition according to claim 4, comprising at least any one of the steps selected from the group consisting of:
a step of introducing all of (A) a thermoplastic polymer, (B) a softener for nonaromatic rubbers, (C) a metal hydrate, (D) an organic peroxide, (E) an antioxidant, (F) a coupling agent, and optional components to be used as desired into a melt kneader and melt kneading the mixture for 30 seconds or longer at a temperature higher than or equal to the 1 minute half-life temperature of said component (D) to obtain a thermoplastic resin composition;
a step of introducing all of said components (A) to (D), (F) and the optional components to be used as desired into a melt kneader and after the melt kneading temperature has reached a temperature higher than or equal to the 1 minute half-life temperature of said component (D), introducing said component (E) into the melt kneader to obtain a thermoplastic resin composition;
a step of firstly introducing all of said components (A) to (D), (F), and the optional components to be used as desired, and a part of said component (E) into a melt kneader and after the melt kneading temperature has reached a temperature higher than or equal to the 1 minute half-life temperature of said component (D), introducing the remainder of said component (E) into the melt kneader to obtain a thermoplastic resin composition; and
a step of firstly introducing all of said component (D), and at least a part of said components (A) to (C), (F), and the optional components to be used as desired into a melt kneader, and after the melt kneading temperature has reached a temperature higher than or equal to the 1 minute half-life temperature of said component (D), introducing the remainder of said components (A) to (C), (F), and the optional components to be used as desired, and said component (E) into the melt kneader to obtain a thermoplastic resin composition.