# US 2020/0369859 A1 · Elastomeric Article

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0369859 A1
- Document ID: US20200369859A1
- Status: Published application
- Kind: A1
- Application number: 16/857,024
- Filed: 2020-04-23
- Published: 2020-11-26
- Earliest claimed: 2019-05-23
- Assignees: Top Glove International Sdn. Bhd.
- Applicants: Top Glove International Sdn., Bhd.
- Inventors: Chong Ban Wong; Keuw Wei Lim; Siew Szen Ling; Siti Ayuni Hamka
- Web page: https://patentgrep.com/patent/US20200369859A1

## CPC

- C08L 7/00: Compositions of natural rubber
- C08L 11/00: Compositions of homopolymers or copolymers of chloroprene
- A41D 19/0006: {made of several layers of material}
- C08L 9/02: Copolymers with acrylonitrile
- A41D 19/0055: {Plastic or rubber gloves}
- C08K 3/013: Fillers, pigments or reinforcing additives
- C08K 3/06: Sulfur
- C08K 5/005: {Stabilisers against oxidation, heat, light, ozone}
- C08K 5/01: Hydrocarbons {(C08K5/0091 takes precedence)}
- C08K 5/18: with aromatically bound amino groups
- C08K 5/42: Sulfonic acids; Derivatives thereof
- C08K 5/435: Sulfonamides
- C08K 2003/2241: {Titanium dioxide}
- C08K 2003/2296: {of zinc}
- C08K 2201/019: the composition being defined by the absence of a certain additive
- C08L 2201/08: Stabilised against heat, light or radiation or oxydation
- C08L 2205/03: containing three or more polymers in a blend
- C08L 2207/04: Thermoplastic elastomer
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- A41D: OUTERWEAR; PROTECTIVE GARMENTS; ACCESSORIES
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

An accelerator-free elastomeric formulation comprising base polymers, crosslinkers, stabilizers, an activator, an antioxidant, a pigment, a wax, an antifoam and a pH adjuster. A method of preparing an accelerator-free elastomeric formulation, comprising the steps of mixing Base polymer A with Crosslinker A to produce mixture A, adding while stirring Stabilizer A, Crosslinker B, an activator, an antioxidant, a pigment, a wax and an antifoam one after another with no particular order and followed by a pH adjuster into the mixture A to produce mixture B, adding Base polymer B and Stabilizer B one after another with no particular order into the mixture B to produce an accelerator-free elastomeric formulation and allowing the accelerator-free elastomeric formulation to mature.

## Claims

### Claim 1

An accelerator-free elastomeric formulation, comprising:
(a) base polymers, wherein the base polymers are a mixture of Base polymer A and Base polymer B, wherein the Base polymer A is used in an amount ranging between 30 phr to 50 phr and wherein the Base polymer B is used in an amount ranging between 50 phr to 70 phr;
(b) crosslinkers, wherein the crosslinkers are a mixture of Crosslinker A and Crosslinker B, wherein the Crosslinker A is used in an amount ranging between 0.40 phr to 1.00 phr based on total dry weight of the base polymers and wherein the Crosslinker B is used in an amount ranging between 0.10 phr to 0.40 phr based on total dry weight of the base polymers;
(c) stabilizers, wherein the stabilizers are base polymer specific, wherein the stabilizer used with Base polymer A is Stabilizer A and the stabilizer used with Base polymer B is Stabilizer B, wherein the Stabilizer A is used in an amount ranging between 0.15 phr to 1.00 phr based on total dry weight of the base polymers and wherein the Stabilizer B is used in an amount ranging between 0.50 phr to 2.50 phr based on total dry weight of the base polymers;
(d) an activator, wherein the activator is used in an amount ranging between 0.40 phr to 1.00 phr based on total dry weight of the base polymers;
(e) an antioxidant, wherein the antioxidant is used in an amount ranging between 0.50 phr to 2.00 phr based on total dry weight of the base polymers;
(f) a pigment, wherein the pigment is used in an amount ranging between 0.80 phr to 1.50 phr based on total dry weight of the base polymers;
(g) a wax, wherein the wax is used in an amount ranging between 0.30 phr to 0.80 phr based on total dry weight of the base polymers;
(h) a antifoam, wherein the antifoam is used in an amount ranging between 0.01 phr to 0.15 phr based on total dry weight of the base polymers; and
(i) a pH adjuster, wherein the pH adjuster in an amount ranging between

### Claim at position 2

70 phr to 2.00 phr based on total dry weight of the base polymers.

### Claim 2 (depends on 1)

The accelerator-free elastomeric formulation as claimed in claim 1, wherein the Base polymer A is any one selected from the group consisting of acrylonitrile butadiene rubber and polyisoprene rubber and wherein the Base polymer B is polychloroprene rubber.

### Claim 3 (depends on 1)

The accelerator-free elastomeric formulation as claimed in claim 1, wherein the Crosslinker A is any one selected from the group consisting of sodium aluminate, aluminium oxide, aluminium sulphate, aluminium chloride, aluminium hydroxide, aluminium phosphate or mixtures therefrom and wherein the Crosslinker B is any one selected from the group consisting of sulphur, benzothiazole sulfonamide or mixtures therefrom.

### Claim 4 (depends on 1)

The accelerator-free elastomeric formulation as claimed in claim 1, wherein the Stabilizer A is any one selected from the group consisting of SDBS, alkyldiphenyloxide disulphonate, dioctyl sulphosuccinates, alkyl benzene sulphonate or mixtures therefrom and wherein the Stabilizer B is any one selected from either sulphated methyl oleate or sodium alkyl sulphates or mixtures therefrom.

### Claim 5 (depends on 1)

The accelerator-free elastomeric formulation as claimed in claim 1, wherein the activator is any one selected from the group consisting of zinc oxide, magnesium oxide, copper oxide, aluminium oxide or mixtures therefrom.

### Claim 6 (depends on 1)

The accelerator-free elastomeric formulation as claimed in claim 1, wherein the antioxidant is any one selected from the group consisting of poly(dicyclopentadiene-co-P-cresol), alkylated diphenylamines or mixtures therefrom.

### Claim 7 (depends on 1)

The accelerator-free elastomeric formulation as claimed in claim 1, wherein the pigment is titanium dioxide and wherein the titanium dioxide may be used alone or used in combination with clays and calcium carbonate.

### Claim 8 (depends on 1)

The accelerator-free elastomeric formulation as claimed in claim 1, wherein the wax is any one selected from the group consisting of paraffin wax emulsion, microcrystalline wax or mixtures therefrom.

### Claim 9 (depends on 1)

The accelerator-free elastomeric formulation as claimed in claim 1, wherein the antifoam is any one selected from either polydimethylsiloxane or emulsion of modified silicone.

### Claim 10 (depends on 1)

The accelerator-free elastomeric formulation as claimed in claim 1, wherein the pH adjuster is any one selected from the group consisting of ammonia, sodium hydroxide, potassium hydroxide, ammonium chloride or mixtures therefrom.

### Claim 11

A method of preparing an accelerator-free elastomeric formulation, comprising the steps of:
i. mixing Base polymer A with Crosslinker A to produce mixture A and stirring the mixture A for a duration between 10 minutes to 40 minutes, wherein the Crosslinker A is used in an amount ranging between 0.40 phr to 1.00 phr based on total dry weight of the base polymers;
ii. adding while stirring Stabilizer A, Crosslinker B, an activator, an antioxidant, a pigment, a wax and an antifoam one after another with no particular order and followed by a pH adjuster into the mixture A to produce mixture B, wherein the mixture B comprises:
the Stabilizer A in an amount ranging between 0.15 phr to 1.00 phr based on total dry weight of the base polymers,
the Crosslinker B in an amount ranging between 0.10 phr to 0.40 phr based on total dry weight of the base polymers,
the activator in an amount ranging between 0.40 phr to 1.00 phr based on total dry weight of the base polymers,
the antioxidant in an amount ranging between 0.50 phr to 2.00 phr based on total dry weight of the base polymers,
the pigment in an amount ranging between 0.80 phr to 1.50 phr based on total dry weight of the base polymers,
the wax in an amount ranging between 0.30 phr to 0.80 phr based on total dry weight of the base polymers,
the antifoam in an amount ranging between 0.01 phr to 0.15 phr based on total dry weight of the base polymers,
the pH adjuster in an amount ranging between 0.70 phr to 2.00 phr based on total dry weight of the base polymers, wherein the mixture B is continuously stirred for a duration of 3 hours to 6 hours and wherein pH range of the mixture B is adjusted to be between 10.70 to 12.00;
iii. adding Base polymer B and Stabilizer B one after another with no particular order into the mixture B to produce accelerator-free elastomeric formulation and allowing the accelerator-free elastomeric formulation to mature for a duration between 1 day to 3 days, wherein the Stabilizer B is used in an amount ranging between 0.50 phr to 2.50 phr based on total dry weight of the base polymers,
wherein the Base polymer A is used in an amount ranging between 30 phr to 50 phr and wherein the Base polymer B is used in an amount ranging between 50 phr to 70 phr to make up to the total dry weight of the base polymers.

### Claim 12 (depends on 11)

The method of preparing an accelerator-free elastomeric formulation as claimed in claim 11, wherein the Base polymer A is any one selected from the group consisting of acrylonitrile butadiene rubber and polyisoprene rubber and wherein the Base polymer B is polychloroprene rubber.

### Claim 13 (depends on 11)

The method of preparing an accelerator-free elastomeric formulation as claimed in claim 11, wherein the Crosslinker A is any one selected from the group consisting of sodium aluminate, aluminium oxide, aluminium sulphate, aluminium chloride, aluminium hydroxide and aluminium phosphate or mixtures therefrom and wherein the Crosslinker B is any one selected from the group consisting of sulphur, benzothiazole sulfonamide or mixtures therefrom.

### Claim 14 (depends on 11)

The method of preparing an accelerator-free elastomeric formulation as claimed in claim 11, wherein the Stabilizer A is any one selected from the group consisting of SDBS, alkyldiphenyloxide disulphonate, dioctyl sulphosuccinates and alkyl benzene sulphonate or mixtures therefrom and wherein the Stabilizer B is any one selected from either sulphated methyl oleate or sodium alkyl sulphates or mixtures therefrom.

### Claim 15 (depends on 11)

The method of preparing an accelerator-free elastomeric formulation as claimed in claim 11, wherein the activator is any one selected from the group consisting of zinc oxide, magnesium oxide, copper oxide, aluminium oxide or mixtures therefrom.

### Claim 16 (depends on 11)

The method of preparing an accelerator-free elastomeric formulation as claimed in claim 11, wherein the antioxidant is any one selected from the group consisting of poly(dicyclopentadiene-co-P-cresol), alkylated diphenylamines or mixtures therefrom.

### Claim 17 (depends on 11)

The method of preparing an accelerator-free elastomeric formulation as claimed in claim 11, wherein the pigment is titanium dioxide and wherein the titanium dioxide may be used alone or used in combination with clays and calcium carbonate.

### Claim 18 (depends on 11)

The method of preparing an accelerator-free elastomeric formulation as claimed in claim 11, wherein the wax is any one selected from the group consisting of paraffin wax emulsion, microcrystalline wax or mixtures therefrom.

### Claim 19 (depends on 11)

The method of preparing an accelerator-free elastomeric formulation as claimed in claim 11, wherein the antifoam is any one selected from either polydimethylsiloxane or emulsion of modified silicone.

### Claim 20 (depends on 11)

The method of preparing an accelerator-free elastomeric formulation as claimed in claim 11, wherein the pH adjuster is any one selected from the group consisting of ammonia, sodium hydroxide, potassium hydroxide, ammonium chloride or mixtures therefrom.

### Claim 21 (depends on 1)

An accelerator-free elastomeric glove produced using the accelerator-free elastomeric formulation as claimed in claim 1.

### Claim 22 (depends on 11)

An accelerator-free elastomeric glove produced from an accelerator-free elastomeric formulation, wherein the accelerator-free elastomeric formulation is prepared using the method as claimed in claim 11.