# US 2020/0368873 A1 · Polishing pad with improved crosslinking density and process for preparing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0368873 A1
- Document ID: US20200368873A1
- Status: Published application
- Kind: A1
- Application number: 16/791,881
- Filed: 2020-02-14
- Published: 2020-11-26
- Earliest claimed: 2019-05-21
- Assignees: Skc Co., Ltd.
- Applicants: Skc Co., Ltd.
- Inventors: Jong Wook YUN; Eun Sun JOENG; Hye Young HEO; Jang Won SEO
- Web page: https://patentgrep.com/patent/US20200368873A1

## CPC

- B24B 37/24: characterised by the composition or properties of the pad materials
- B24B 7/228: {for grinding thin, brittle parts, e.g. semiconductors, wafers (grinding edges of thin, brittle parts B24B9/065)}
- B24D 11/00: Constructional features of flexible abrasive materials; Special features in the manufacture of such materials
- C08G 18/12: using two or more compounds having active hydrogen in the first polymerisation step
- C08G 18/3206: {aliphatic}
- C08G 18/3243: {containing two or more aromatic rings}
- C08G 18/4854: {Polyethers containing oxyalkylene groups having four carbon atoms in the alkylene group}
- C08G 18/6529: {Compounds of group C08G18/3225 or polyamines of C08G18/38}
- C08G 18/6685: {with compounds of group C08G18/3225 or polyamines of C08G18/38}
- C08G 18/724: {Combination of aromatic polyisocyanates with (cyclo)aliphatic polyisocyanates}
- C08G 18/758: {containing two or more cycloaliphatic rings}
- C08G 18/7621: {being toluene diisocyanate including isomer mixtures}
- C08J 9/12: by a physical blowing agent
- H10P 52/402: {of semiconductor materials}
- C08J 9/122: {Hydrogen, oxygen, CO2, nitrogen or noble gases}
- C08J 9/146: {only fluorine as halogen atoms}
- C08J 9/32: from compositions containing microballoons, e.g. syntactic foams
- C08J 2201/026: Crosslinking before of after foaming
- C08J 2203/06: CO2, N2 or noble gases
- C08J 2203/22: Expandable microspheres, e.g. Expancel®
- C08J 2375/04: Polyurethanes
- H10P 95/062: {involving a dielectric removal step}
- B24B: MACHINES, DEVICES, OR PROCESSES FOR GRINDING OR POLISHING (grinding of gear teeth B23F, of screw-threads B23G1/36; by electro-erosion B23H; abrasive or related blasting B24C; tools for grinding, buffing or sharpening B24D; polishing compositions C09G1/00; abrasives C09K3/14; electrolytic etching or polishing C25F3/00; grinding arrangements for use on assembled railway tracks E01B31/17); DRESSING OR CONDITIONING OF ABRADING SURFACES; FEEDING OF GRINDING, POLISHING, OR LAPPING AGENTS
- B24D: TOOLS FOR GRINDING, BUFFING OR SHARPENING (abrading-bodies specially designed for tumbling apparatus, e.g. abrading-balls B24B31/14; honing tools B24B33/08; lapping tools B24B37/11)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

The present invention provides a polishing pad whose crosslinking density is adjusted to enhance the performance of the CMP process such as polishing rate and cut pad rate, in addition, in the process for preparing a polishing pad according to the embodiment, it is possible to implement such a crosslinking density by a simple method of controlling the preheating temperature of the mold for curing, Thus, the polishing pad may be applied to a process of preparing a semiconductor device, which comprises a CMP process, to provide a semiconductor device such as a wafer of excellent quality.

## Claims

### Claim 1

A polishing pad, which comprises a polishing layer comprising a porous polyurethane-based resin, wherein the polishing layer has a swelling ratio of 100% to 350% in dimethylformamide (DMF) based on the volume or weight of the polishing layer.

### Claim 2 (depends on 1)

The polishing pad of claim 1, wherein the polishing layer has a swelling ratio of 150% to 300% in DMF based on the volume of the polishing layer and a swelling ratio of 200% to 350% in DMF based on the weight of the polishing layer.

### Claim 3 (depends on 1)

The polishing pad of claim 1, wherein the polishing layer has a swelling ratio of 150% to 450% in N-methyl-2-pyrrolidone (NMP) based on the volume or weight of the polishing layer.

### Claim 4 (depends on 3)

The polishing pad of claim 3, wherein the polishing layer has a swelling ratio of 200% to 350% in NMP based on the volume of the polishing layer and a swelling ratio of 300% to 450% in NMP based on the weight of the polishing layer.

### Claim 5 (depends on 1)

The polishing pad of claim 1, wherein the porous polyurethane-based resin comprises a first crosslinking unit in which two urethane groups are crosslinked by a diisocyanate.

### Claim 6 (depends on 5)

The polishing pad of claim 5, wherein the first crosslinking unit comprises a structure of Formula 1:

### Claim 7 (depends on 1)

The polishing pad of claim 1, wherein the porous polyurethane-based resin comprises a second crosslinking unit in which two urea groups are crosslinked by a diisocyanate.

### Claim 8 (depends on 7)

The polishing pad of claim 7, wherein the second crosslinking unit comprises a structure of Formula 2:

### Claim 9 (depends on 1)

The polishing pad of claim 1, wherein the polishing layer has an elongation of 100% to 120% and a modulus of 30 kgf/cm2 to 100 kgf/cm2.

### Claim 10 (depends on 1)

The polishing pad of claim 1, wherein the polishing layer has a polishing rate (or removal rate) of 3,000 Å/min to 4,000 Å/min against a silicon oxide layer.

### Claim 11

A process for preparing a polishing pad, which comprises:
preparing a first raw material composition comprising a urethane-based prepolymer, a second raw material composition comprising a curing agent, and a third raw material composition comprising a foaming agent;
sequentially or simultaneously mixing the first raw material composition with the second raw material composition and the third raw material composition to prepare a raw material mixture; and
injecting the raw material mixture into a mold preheated to a temperature of 50° C. or higher and curing it to obtain a polishing layer,
wherein the polishing layer has a swelling ratio of 100% to 350% in dimethylformamide (DMF) based on the volume or weight of the polishing layer.

### Claim 12 (depends on 11)

The process for preparing a polishing pad of claim 11, wherein the preheating temperature of the mold is 50° C. to 150° C.

### Claim 13 (depends on 11)

The process for preparing a polishing pad of claim 11, wherein the urethane-based prepolymer and the curing agent are employed at a molar equivalent ratio of 1:0.8 to 1:1.2 based on the number of moles of the reactive groups in each molecule.

### Claim 14 (depends on 11)

The process for preparing a polishing pad of claim 11, wherein the urethane-based prepolymer is prepared by a prepolymerization reaction of at least one diisocyanate monomer and at least one polyol, and the at least one diisocyanate monomer and the at least one polyol are employed at a molar equivalent ratio of 1:0.8 to 1:1.2 based on the number of moles of the reactive groups in each molecule.

### Claim 15

A process for preparing a semiconductor device, which comprises polishing the surface of a semiconductor substrate using a polishing pad, wherein the polishing pad comprises a polishing layer comprising a porous polyurethane-based resin, and the polishing layer has a swelling ratio of 100% to 350% in dimethylformamide (DMF) based on the volume or weight of the polishing layer.