# US 2020/0368728 A1 · Method of coupling methane dry-reforming and composite catalyst regeneration

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0368728 A1
- Document ID: US20200368728A1
- Status: Published application
- Kind: A1
- Application number: 16/344,020
- Filed: 2018-05-15
- Published: 2020-11-26
- Earliest claimed: 2018-03-28
- Assignees: Zhejiang University
- Applicants: Zhejiang University
- Inventors: Sufang WU; Jiayan XU; Hao LIU; Qirui LIN; Hui XIAO
- Web page: https://patentgrep.com/patent/US20200368728A1

## CPC

- B01J 23/94: of catalysts comprising metals, oxides or hydroxides of the iron group metals or copper
- B01J 21/04: Alumina
- B01J 23/78: with alkali- or alkaline earth metals
- B01J 27/232: Carbonates
- B01J 37/0203: {the impregnation liquid containing organic compounds}
- B01J 37/0213: {Preparation of the impregnating solution}
- B01J 37/088: {Decomposition of a metal salt}
- B01J 37/343: {of ultrasonic wave energy}
- B01J 38/02: Heat treatment
- B01J 38/04: Gas or vapour treating; Treating by using liquids vaporisable upon contacting spent catalyst
- C01B 3/344: {using non-catalytic solid particles}
- C01B 3/40: characterised by the catalyst
- B01J 2523/00: Constitutive chemical elements of heterogeneous catalysts
- C01B 2203/0238: the reforming step being a carbon dioxide reforming step
- C01B 2203/0425: In-situ adsorption process during hydrogen production
- C01B 2203/0475: the impurity being carbon dioxide
- C01B 2203/1058: Nickel catalysts
- C01B 2203/1082: Composition of support materials
- Y02P 20/52: using catalysts, e.g. selective catalysts
- Y02P 20/584: Recycling of catalysts
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present invention is related to a method of coupling methane dry-reforming and composite catalyst regeneration. A composite catalyst is filled into a reactor, and methane or a methane mixture gas is introduced therein. CaCO3 in the composite catalyst is decomposed under 600-850° C. CO2 obtained by the decomposition reacts with methane to perform methane dry-reforming reaction and produce synthesis gas containing CO and hydrogen. The composite catalyst contains CaCO3 , active nickel and alumina support. This method couples the CaCO3 decomposition reaction in calcium looping and methane dry-reforming reaction to solve the technical problem of limiting CaCO3 decomposition by high-temperature equilibrium. The decomposition of CaCO3 is enhanced, and the CO2 produced by decomposing CaCO3 is dry-reformed to produce synthesis gas to be utilized.

## Claims

### Claim at position 1

1-10. (canceled)

### Claim 11

A method of coupling methane dry-reforming and composite catalyst regeneration, comprising:
filling a first composite catalyst into a reactor, wherein the first composite catalyst comprises CaCO3 and an active nickel containing NiO supported on a support containing alumina (Al2O3);
introducing a methane-containing gas into the reactor;
decomposing the CaCO3 in the first composite catalyst at 600-850° C. to obtain CO2 and CaO; and
performing methane dry reforming reaction by reacting the obtained CO2 with methane in the methane-containing gas to form synthesis gas containing CO and H2.

### Claim 12 (depends on 11)

The method of claim 11, wherein a mass ratio of CaO, NiO and Al2O3 in the first composite catalyst is 2-7:1:1.0-3.5.

### Claim 13 (depends on 11)

The method of claim 11, wherein the methane-containing gas is methane, or a mixture of methane and at least one of water vapor, CO2 and nitrogen.

### Claim 14 (depends on 11)

The method of claim 11, wherein a volume ratio of the methane in the methane-containing gas is at least 10%.

### Claim 15 (depends on 11)

The method of claim 11, wherein the decomposing step is performed under a pressure of 0.1-3.0 MPa, and a gas space velocity is 100-1000 h−1.

### Claim 16 (depends on 11)

The method of claim 11, wherein the alumina of the support reacts with the CaO obtained in the decomposing step to form calcium aluminate.

### Claim 17 (depends on 11)

The method of claim 11, wherein the reactor comprises a fixed bed reactor, a fluidized bed reactor, a moving bed reactor or a bubbling bed reactor.

### Claim 18 (depends on 11)

The method of claim 11, wherein the first composite catalyst is prepared by a second composite catalyst adsorbing CO2 from methane steam reforming reaction, and the second composite catalyst comprises alumina-supported CaO and NiO.

### Claim 19 (depends on 1, 18)

The method of claim 18, further comprising performing the steps of filling the first composite catalyst into the reactor, introducing the methane-containing gas into the reactor, decomposing the CaCO3 in the first composite catalyst, and performing the methane dry reforming reaction in claim 1.

### Claim 20 (depends on 11)

The method of claim 11, wherein the first composite catalyst is prepared by a second composite catalyst adsorbing CO2 from flue gas decarburization process, and the second composite catalyst comprises alumina-supported CaO and NiO.

### Claim 21 (depends on 1, 20)

The method of claim 20, further comprising performing the steps of filling the first composite catalyst into the reactor, introducing the methane-containing gas into the reactor, decomposing the CaCO3 in the first composite catalyst, and performing the methane dry reforming reaction in claim 1.