# US 2020/0368725 A1 · Heterogeneous catalysts

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0368725 A1
- Document ID: US20200368725A1
- Status: Published application
- Kind: A1
- Application number: 16/986,065
- Filed: 2020-08-05
- Published: 2020-11-26
- Earliest claimed: 2014-05-02
- Assignees: Lummus Technology Inc.
- Applicants: Lummus Technology LLC
- Inventors: Wayne P. Schammel; Anja Rumplecker; Fabio R. Zurcher; Erik C. Scher; Joel M. Cizeron; Joel Gamoras
- Web page: https://patentgrep.com/patent/US20200368725A1

## CPC

- B01J 23/10: of rare earths
- B01J 35/19: {Catalysts containing parts with different compositions}
- B01J 35/45: Nanoparticles
- B01J 35/58: Fabrics or filaments
- B01J 37/03: Precipitation; Co-precipitation
- C07C 2/84: catalytic
- B01J 23/002: {Mixed oxides other than spinels, e.g. perovskite}
- C07C 2521/02: Boron or aluminium; Oxides or hydroxides thereof
- C07C 2521/10: Magnesium; Oxides or hydroxides thereof
- C07C 2523/02: of the alkali- or alkaline earth metals or beryllium
- C07C 2523/04: Alkali metals
- C07C 2523/10: of rare earths
- C07C 2529/83: Aluminophosphates (APO compounds)
- Y02P 20/52: using catalysts, e.g. selective catalysts
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Heterogeneous catalysts with optional dopants are provided. The catalysts are useful in a variety of catalytic reactions, for example, the oxidative coupling of methane to C2+ hydrocarbons. Related methods for use and manufacture of the same are also disclosed.

## Claims

### Claim 1

A method for conversion of methane to C2+ hydrocarbons, the method comprising contacting a catalyst with a gas comprising methane, the catalyst comprising:
a base material comprising an oxide of two or more lanthanide elements; and
a dopant combination selected from the group consisting of Sr/Sm, Sr/Gd, Sr/Dy, Sr/Er, Sr/Lu, Sr/Ba/B, Ba/Sr, Sr/K, Sr/Ga/Mg, Sr/Y, Sr/B/Y, Sr/Al, Sr/Ba/W, Sr/W/B and Sr/Ba/W/B,
provided that one of the lanthanide elements is not lanthanum when another lanthanide element is neodymium.

### Claim 2 (depends on 1)

The method of claim 1, wherein the methane is converted to C2+ hydrocarbons by an oxidative coupling of methane (OCM) reaction.

### Claim 3 (depends on 1)

The method of claim 1, wherein the gas further comprises an oxidant source.

### Claim 4 (depends on 3)

The method of claim 3, wherein the oxidant source is a gas enriched for oxygen.

### Claim 5 (depends on 3)

The method of claim 3, wherein the oxidant source is air.

### Claim 6 (depends on 1)

The method of claim 1, wherein the method is performed in the presence of ethane.

### Claim 7 (depends on 1)

The method of claim 1, wherein the oxide has the following formula (III):
Ln1a Ln2b Ln3d Ln4e Ln5fOc (III)
wherein:
Ln1, Ln2, Ln3, Ln4 and Ln5 are independently different lanthanide elements;
O is oxygen;
a and c are each independently numbers greater than 0; and
b, d, e, and f are independently 0 or a number greater than 0.

### Claim 8 (depends on 1)

The method of claim 1, wherein the catalyst comprises a C2+ selectivity of greater than 50% and a methane conversion of greater than 20% when the catalyst is contacted with the gas at a temperature of 750° C. or less.

### Claim 9 (depends on 8)

The method of claim 8, wherein the catalyst further comprises a C2+ yield greater than 10% when the catalyst is contacted with the gas at a temperature of 750° C. or less.

### Claim 10 (depends on 9)

The method of claim 9, wherein the methane conversion, C2+ selectivity, or C2+ yield, or combinations thereof, are measured in a 4 millimeter inner diameter tube with a methane to oxygen ratio of 5.5:1 using air as an oxidant, wherein the temperature is 650° C.

### Claim 11

A method for conversion of methane to C2+ hydrocarbons, the method comprising contacting a catalyst with a gas comprising methane, the catalyst comprising a Group 4 or lanthanide oxide in combination with an alkaline earth metal dopant selected from the group consisting of Ba/W, Ba/B, Ba/Sr, Ba/Ce, Ba/Hf, Y/Ba, Ca/B, Sr/Ba/W, Ba/W/B, Sr/Ba/B and Sr/Ba/W/B.

### Claim 12 (depends on 11)

The method of claim 11, wherein the methane is converted to C2+ hydrocarbons by an oxidative coupling of methane (OCM) reaction.

### Claim 13 (depends on 11)

The method of claim 11, wherein the gas further comprises an oxidant source.

### Claim 14 (depends on 13)

The method of claim 13, wherein the oxidant source is a gas enriched for oxygen.

### Claim 15 (depends on 13)

The method of claim 13, wherein the oxidant source is air.

### Claim 16 (depends on 11)

The method of claim 11, wherein the method is performed in the presence of ethane.

### Claim 17 (depends on 11)

The method of claim 11, wherein the dopant is Ba/W, Sr/Ba/W or Sr/Ba/W/B.

### Claim 18 (depends on 11)

The method of claim 11, wherein the catalyst comprises one of the following compositions: Ba/W/Nd2O3 or Ba/W/Er2O3.

### Claim 19 (depends on 11)

The method of claim 11, wherein the catalyst comprises a C2+ selectivity of greater than 50% and a methane conversion of greater than 20% when the catalyst is contacted with the gas at a temperature of 750° C. or less.

### Claim 20 (depends on 19)

The method of claim 19, wherein the catalyst further comprises a C2+ yield greater than 10% when the catalyst is contacted with the gas at a temperature of 750° C. or less.

### Claim 21 (depends on 20)

The method of claim 20, wherein the methane conversion, C2+ selectivity, or C2+ yield, or combinations thereof, are measured in a 4 millimeter inner diameter tube with a methane to oxygen ratio of 5.5:1 using air as an oxidant, wherein the temperature is 650° C.

### Claim 22

A method for conversion of methane to C2+ hydrocarbons, the method comprising contacting a catalyst with a gas comprising methane, the catalyst comprising a mixed oxide base material and a dopant combination, the mixed oxide comprising erbium (Er) and at least one further lanthanide element, the dopant combination selected from the group consisting of Sr/Sm, Sr/Gd, Sr/Dy, Sr/Er, Sr/Lu, Sr/Ba/B, Ba/B, Ba/Sr, Er/W, Sr/K, Ba/Ce, Ba/Hf, Ga/Mg, Mg/Er, Y/Ba, Sr/Ga/Mg, Sr/Y, Sr/B/Y, Ca/B, Sr/Al, Ba/W, B/W, Sr/Ba/W, Sr/W/B, Ba/W/B and Sr/Ba/W/B.

### Claim 23 (depends on 22)

The method of claim 22, wherein the methane is converted to C2+ hydrocarbons by an oxidative coupling of methane (OCM) reaction.

### Claim 24 (depends on 22)

The method of claim 22, wherein the gas further comprises an oxidant source.

### Claim 25 (depends on 24)

The method of claim 24, wherein the oxidant source is a gas enriched for oxygen.

### Claim 26 (depends on 24)

The method of claim 24, wherein the oxidant source is air.

### Claim 27 (depends on 22)

The method of claim 22, wherein the method is performed in the presence of ethane.

### Claim 28 (depends on 22)

The method of claim 22, wherein the mixed oxide comprises a physical blend of Er, or an oxidized form thereof, and the further lanthanide element, or an oxidized form thereof.

### Claim 29 (depends on 28)

The method of claim 28, wherein the mixed oxide has the following formula (I):
LnxEryOz (I)
wherein:
Ln is the lanthanide element;
Er is erbium;
O is oxygen; and
x, y and z are each independently numbers greater than 0, wherein x, y and z are selected such that the overall charge of the catalyst is about 0.

### Claim 30 (depends on 29)

The method of claim 29, wherein x, y and z are selected such that z is from 150% to 200% of the sum of x and y.

### Claim 31 (depends on 29)

The method of claim 29, wherein the mixed oxide is LnErO3 or Ln3ErO6.

### Claim 32 (depends on 22)

The method of claim 22, wherein the catalyst comprises a C2+ selectivity of greater than 50% and a methane conversion of greater than 20% when the catalyst is contacted with the gas at a temperature of 750° C. or less.

### Claim 33 (depends on 32)

The method of claim 32, wherein the catalyst further comprises a C2+ yield greater than 10% when the catalyst is contacted with the gas at a temperature of 750° C. or less.

### Claim 34 (depends on 33)

The method of claim 33, wherein the methane conversion, C2+ selectivity, or C2+ yield, or combinations thereof, are measured in a 4 millimeter inner diameter tube with a methane to oxygen ratio of 5.5:1 using air as an oxidant, wherein the temperature is 650° C.