# US 2020/0365300 A1 · Thick film resistors having customizable resistances and methods of manufacture

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0365300 A1
- Document ID: US20200365300A1
- Status: Published application
- Kind: A1
- Application number: 16/901,429
- Filed: 2020-06-15
- Published: 2020-11-19
- Earliest claimed: 2019-05-17
- Assignees: Raytheon Company; University of Massachusetts
- Applicants: Raytheon Company; University of Massachusetts
- Inventors: Erika C. Klek; Mary K. Herndon; Thomas V. Sikina; James E. Benedict; Andrew R. Southworth; Kevin M. Wilder; Oshadha K. Ranasingha; Alkim Akyurtlu
- Web page: https://patentgrep.com/patent/US20200365300A1

## CPC

- H01C 7/003: {Thick film resistors}
- H01B 3/10: metallic oxides (ceramics H01B3/12)
- H01C 17/0652: {containing carbon or carbides}
- H01C 17/06533: {composed of oxides}
- H01C 17/06553: {composed of a combination of metals and oxides}
- H01C 17/2416: {by chemical etching}
- H01C 17/30: adapted for baking
- H05K 1/167: {incorporating printed resistors}
- H01C 1/14: Terminals or tapping points specially adapted for resistors; Arrangements of terminals or tapping points on resistors
- H01C 17/28: adapted for applying terminals
- H01C 17/281: {by thick film techniques}
- H05K 2201/0323: Carbon
- H01C: RESISTORS
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS

## Abstract

A method includes blending a dielectric material including a titanate with a carbon-based ink to form a modified carbon-based ink. The method also includes printing the modified carbon-based ink onto a structure. The method further includes curing the printed modified carbon-based ink on the structure at a temperature that does not exceed about 250° C. In addition, the method includes processing the cured printed modified carbon-based ink to form a thick film resistor. Blending the dielectric material with the carbon-based ink causes the modified carbon-based ink to have a resistivity that is at least double a resistivity of the carbon-based ink.

## Claims

### Claim 1

A method comprising:
blending a dielectric material comprising a titanate with a carbon-based ink to form a modified carbon-based ink;
printing the modified carbon-based ink onto a structure;
curing the printed modified carbon-based ink on the structure at a temperature that does not exceed about 250° C.; and
processing the cured printed modified carbon-based ink to form a thick film resistor;
wherein blending the dielectric material with the carbon-based ink causes the modified carbon-based ink to have a resistivity that is at least double a resistivity of the carbon-based ink.

### Claim 2 (depends on 1)

The method of claim 1, wherein the dielectric material comprises a titanate.

### Claim 3 (depends on 1)

The method of claim 1, wherein printing the modified carbon-based ink onto the structure comprises printing the modified carbon-based ink onto the structure such that the printed modified carbon-based ink connects multiple conductive traces.

### Claim 4 (depends on 1)

The method of claim 1, wherein the printed modified carbon-based ink is cured at a temperature that does not exceed about 160° C.

### Claim 5 (depends on 1)

The method of claim 1, wherein processing the cured printed modified carbon-based ink to form the thick film resistor comprises etching the cured printed modified carbon-based ink to obtain a desired resistance value.

### Claim 6 (depends on 1)

The method of claim 1, wherein processing the cured printed modified carbon-based ink to form the thick film resistor comprises applying about 0.25 W to about 0.5 W of power to the thick film resistor.

### Claim 7 (depends on 1)

The method of claim 1, wherein the thick film resistor is configured to at least one of:
handle up to about 200 mA of current without fusing; and
handle up to about 1.0 W of power without fusing.

### Claim 8

A method comprising:
obtaining a modified carbon-based thick film material that comprises a carbon-based thick film material blended with a dielectric material;
depositing the modified carbon-based thick film material onto a structure;
curing the deposited modified carbon-based thick film material on the structure at a temperature that does not exceed about 250° C.; and
processing the cured deposited modified carbon-based thick film material to form a thick film resistor;
wherein the dielectric material blended with the carbon-based thick film material causes the modified carbon-based thick film material to have a resistivity that is at least double a resistivity of the carbon-based thick film material.

### Claim 9 (depends on 8)

The method of claim 8, wherein an amount of the dielectric material blended with the carbon-based thick film material does not exceed about 5% to about 15% by weight of the modified carbon-based thick film material.

### Claim 10 (depends on 8)

The method of claim 8, wherein the dielectric material comprises at least one of: barium titanate, strontium titanate, and barium strontium titanate.

### Claim 11 (depends on 8)

The method of claim 8, wherein depositing the modified carbon-based thick film material onto the structure comprises depositing the modified carbon-based thick film material onto the structure such that the deposited modified carbon-based thick film material connects multiple conductive traces.

### Claim 12 (depends on 8)

The method of claim 8, wherein the deposited modified carbon-based thick film material is cured on the structure at a temperature that does not exceed about 160° C.

### Claim 13 (depends on 8)

The method of claim 8, wherein processing the cured deposited modified carbon-based thick film material to form the thick film resistor comprises etching the cured deposited modified carbon-based thick film material to obtain a desired resistance value.

### Claim 14 (depends on 8)

The method of claim 8, wherein processing the cured deposited modified carbon-based thick film material to form the thick film resistor comprises applying about 0.25 W to about 0.5 W of power to the thick film resistor.

### Claim 15 (depends on 8)

The method of claim 8, wherein the thick film resistor is configured to at least one of:
handle up to about 200 mA of current without fusing; and
handle up to about 1.0 W of power without fusing.

### Claim 16

An apparatus comprising:
a thick film resistor fabricated by:
printing a modified carbon-based ink onto a structure, wherein the modified carbon-based ink comprises a dielectric material comprising a titanate blended with a carbon-based ink;
curing the printed modified carbon-based ink on the structure at a temperature that does not exceed about 250° C.; and
processing the cured printed modified carbon-based ink to form the thick film resistor;
wherein the dielectric material blended with the carbon-based ink causes the modified carbon-based ink to have a resistivity that is at least double a resistivity of the carbon-based ink.

### Claim 17 (depends on 16)

The apparatus of claim 16, wherein the dielectric material comprises a titanate.

### Claim 18 (depends on 16)

The apparatus of claim 16, wherein the thick film resistor electrically connects multiple conductive traces of the structure.

### Claim 19 (depends on 16)

The apparatus of claim 16, wherein the thick film resistor is configured to handle up to about 200 mA of current without fusing.

### Claim 20 (depends on 16)

The apparatus of claim 16, wherein the thick film resistor is configured to handle up to about 1.0 W of power without fusing.