# US 2020/0361777 A1 · Nanometer Niobium Carbide/Carbon Nanotube Reinforced Diamond Composite And A Preparation Method Thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0361777 A1
- Document ID: US20200361777A1
- Status: Published application
- Kind: A1
- Application number: 16/802,613
- Filed: 2020-02-27
- Published: 2020-11-19
- Earliest claimed: 2019-04-04
- Assignees: Jilin University
- Applicants: Jilin University
- Inventors: Baochang Liu; Wenhao DAI; Siqi LI; Zhe HAN; Xinzhe ZHAO; Shujing WANG
- Web page: https://patentgrep.com/patent/US20200361777A1

## CPC

- C01B 32/174: Derivatisation; Solubilisation; Dispersion in solvents
- C01B 32/26: Preparation (by using ultra-high pressure B01J3/06; by crystal growth C30B29/04)
- C01B 32/166: in liquid phase
- C01B 32/25: Diamond
- C01B 32/914: Carbides of single elements
- C01G 33/003: {Preparation involving a liquid-liquid extraction, an adsorption or an ion-exchange}
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- B82Y 40/00: Manufacture or treatment of nanostructures
- C01P 2004/13: Nanotubes
- C01P 2004/64: Nanometer sized, i.e. from 1-100 nanometer
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

A nanometer niobium carbide/carbon nanotube reinforced diamond composite and a preparation method thereof, belonging to the field of materials science. The nanometer niobium carbide/carbon nanotube reinforced diamond composite is composed of nanometer niobium carbide/carbon nanotube composite powders, matrix powders and diamond grains, wherein the nanometer niobium carbide/carbon nanotube composite powders are the composites of nanometer niobium carbide which are evenly distributed in the surface defects and interior of the carbon nanotube, the nanometer niobium carbide/carbon nanotube reinforced diamond composite is prepared by mixing the nanometer niobium carbide/carbon nanotube composite powders, matrix powders and diamond grains uniformly and sintering with a hot pressing technique.

## Claims

### Claim 1

A method for preparing a nanometer niobium carbide/carbon nanotube reinforced diamond composite, comprising the following step:
(1) preparing nanometer niobium carbide/carbon nanotube composite powders; by,
weighing nanometer niobium carbide and carbon nanotube at a mass ratio of (5˜10):1, which are added into distilled water respectively and ultrasonic dispersed for 0.5 h˜1 h, giving an aqueous dispersion of nanometer niobium carbide and an aqueous dispersion of carbon nanotube; thereafter, magnetically stirring the aqueous dispersion of nanometer niobium carbide and slowly adding the aqueous dispersion of carbon nanotube dropwise, and drying in vacuum after 30 min to obtain the composite powders, adding the composite powders into a hard alloy ball-milling tank, into which are additionally added hard alloy grinding balls, wherein the ratio of grinding balls to materials is 40:1, the ball-milling rate is 400 r/min, the time for ball-milling is 3 h˜6 h, and dried in vacuum to obtain nanometer niobium carbide/carbon nanotube composite powders;
(2) preparing of nanometer niobium carbide/carbon nanotube/matrix composite powders; by,
weighing the nanometer niobium carbide/carbon nanotube composite powders obtained in step (1) and the matrix powders at weight percentages of nanometer niobium carbide/carbon nanotube composite powders of 0.5 wt %˜3 wt % and matrix powders of 97 wt%˜99.5 wt %, on which is then conducted the planetary ball milling, wherein the ratio of grinding balls to materials is 6:1, the ball-milling rate is 320 r/min, the time for ball-milling is 3 h˜6 h, and dried in vacuum to obtain nanometer niobium carbide/carbon nanotube/matrix composite powders;
(3) weighing the nanometer niobium carbide/carbon nanotube/matrix composite powders obtained in step (2) and diamond grains at volume percentages of nanometer niobium carbide/carbon nanotube/matrix composite powders of 70 vol %˜80 vol % and diamond grains of 20 vol %˜30 vol %, and then placed into a three-dimensional mixing machine to mix for 1 h˜3 h, giving mixed powders;
(4) charging into graphite moulds the mixed powders obtained in step (3), and sintering in a hot pressing sintering furnace, giving nanometer niobium carbide/carbon nanotube reinforced diamond composites.

### Claim 2 (depends on 1)

The method for preparing a nanometer niobium carbide/carbon nanotube reinforced diamond composite of claim 1, wherein the particle size of nanometer niobium carbide is 10 nm˜30 nm, the length of carbon nanotube is 10 um˜30 um, and the outer diameter is 20 nm˜70 nm.

### Claim 3 (depends on 1)

The method for preparing a nanometer niobium carbide/carbon nanotube reinforced diamond composite of claim 1, wherein the matrix powder in step (2) is composed of WC tungsten carbide powders at a mass fraction of 40%, 35% of 663 bronze powders, 15% of YG6 hard alloy powders, 5% of Ni nickel powders and 5% of Mn manganese powders.

### Claim 4 (depends on 3)

The method for preparing a nanometer niobium carbide/carbon nanotube reinforced diamond composite of claim 3, wherein the matrix powders are prepared as below: WC tungsten carbide powder at a mass fraction of 40%, 35% of 663 bronze powders, 15% of YG6 hard alloy powders, 5% of Ni nickel powders and 5% of Mn manganese powders are added into a hard alloy ball-milling tank, at the same time adding hard alloy grinding balls, wherein the ratio of grinding balls to materials is 6:1, the ball-milling rate is 320 r/min, the time for ball-milling is 1 h˜2 h, and then dried in vacuum to obtain the matrix powder.

### Claim 5 (depends on 3)

The method for preparing a nanometer niobium carbide/carbon nanotube reinforced diamond composite of claim 3, wherein the particle size of WC tungsten carbide powder is −200 meshes, the particle size of 663 bronze powder is −200 meshes, the particle size of YG6 hard alloy powder is −300 meshes, the particle size of Ni nickel powder is −200 meshes, and the particle size of Mn manganese powder is −200 meshes.

### Claim 6 (depends on 1)

The method for preparing a nanometer niobium carbide/carbon nanotube reinforced diamond composite of claim 1, wherein the diamond grains are artificial diamond monocrystals which are 40 meshes˜100 meshes in size.

### Claim 7 (depends on 1)

The method for preparing a nanometer niobium carbide/carbon nanotube reinforced diamond composite of claim 1, wherein the ball-milling medium used during the ball-milling of step (1) is absolute ethanol.

### Claim 8 (depends on 1)

The method for preparing a nanometer niobium carbide/carbon nanotube reinforced diamond composite of claim 1, wherein the sintering process in step (4) is as below: within 300 s, the temperature of mixed powders is increased to 980° C., the pressure is increased from 0 MPa to 18 MPa, keeping the sintering temperature at 980° C. and the pressure at 18 MPa, with a holding time of 300 s; and then within 300 s, the temperature is reduced to 450° C., the pressure is reduced to 6 Mpa; finally withdrawing the pressure and cooling naturally to room temperature.

### Claim 9 (depends on 1)

A nanometer niobium carbide/carbon nanotube reinforced diamond composite prepared with the method of method of claim 1.

### Claim 10 (depends on 2)

A nanometer niobium carbide/carbon nanotube reinforced diamond composite prepared with the method of claim 2.

### Claim 11 (depends on 3)

A nanometer niobium carbide/carbon nanotube reinforced diamond composite prepared with the method of claim 3.

### Claim 12 (depends on 4)

A nanometer niobium carbide/carbon nanotube reinforced diamond composite prepared with the method of claim 4.

### Claim 13 (depends on 5)

A nanometer niobium carbide/carbon nanotube reinforced diamond composite prepared with the method of claim 5.

### Claim 14 (depends on 6)

A nanometer niobium carbide/carbon nanotube reinforced diamond composite prepared with the method of claim 6.

### Claim 15 (depends on 7)

A nanometer niobium carbide/carbon nanotube reinforced diamond composite prepared with the method of claim 7.

### Claim 16 (depends on 8)

A nanometer niobium carbide/carbon nanotube reinforced diamond composite prepared with the method of claim 8.