# US 2020/0350418 A1 · Gate Stack Structure and Method for Forming the Same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0350418 A1
- Document ID: US20200350418A1
- Status: Published application
- Kind: A1
- Application number: 16/928,423
- Filed: 2020-07-14
- Published: 2020-11-05
- Earliest claimed: 2017-06-30
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Co., Ltd.
- Inventors: Ming-Chi Huang; Ying-Liang Chuang; Ming-Hsi Yeh; Kuo-Bin Huang
- Web page: https://patentgrep.com/patent/US20200350418A1

## CPC

- H10D 30/0243: {using dummy structures having essentially the same shapes as the semiconductor bodies, e.g. to provide stability}
- H10D 30/62: Fin field-effect transistors [FinFET]
- H10D 62/021: {Forming source or drain recesses by etching e.g. recessing by etching and then refilling}
- H10D 62/115: {Dielectric isolations, e.g. air gaps}
- H10D 62/151: {of IGFETs (of IGFETs having LDD or DDD structure H10D30/601; of thin film transistors H10D30/6713)}
- H10D 64/017: {using dummy gates in processes wherein at least parts of the final gates are self-aligned to the dummy gates, i.e. replacement gate processes}
- H10D 64/667: {the conductor comprising a layer of alloy material, compound material or organic material contacting the insulator, e.g. TiN workfunction layers (having lateral variation H10D64/671)}
- H10D 84/0158: {the components including FinFETs}
- H10D 84/0193: {the components including FinFETs}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D 84/853: {comprising FinFETs}
- H10P 14/43: Chemical deposition, e.g. chemical vapour deposition [CVD]
- H10P 14/44: Physical vapour deposition [PVD]
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10P 14/6518: {by introduction of substances into an already-existing insulating layer}
- H10P 14/69396: {the material containing at least one rare earth metal element, e.g. oxides of lanthanides, scandium or yttrium}
- H10P 32/20: Diffusion for doping of insulating layers
- H10P 50/283: {by chemical means}
- H10P 70/20: {Cleaning during device manufacture}
- H10P 70/27: {during, before or after processing of conductive materials, e.g. polysilicon or amorphous silicon layers}
- H10D 62/822: comprising only Group IV materials heterojunctions, e.g. Si/Ge heterojunctions
- H10D 64/691: {comprising metallic compounds, e.g. metal oxides or metal silicates (insulators comprising nitrogen H10D64/693)}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Embodiments of the present disclosure provide a method of cleaning a lanthanum containing substrate without formation of undesired lanthanum compounds during processing. In one embodiment, the cleaning method includes treating the lanthanum containing substrate with an acidic solution prior to cleaning the lanthanum containing substrate with a HF solution. The cleaning method permits using lanthanum doped high-k dielectric layer to modulate effective work function of the gate stack, thus, improving device performance.

## Claims

### Claim 1

A method of forming a semiconductor device, the method comprising:
forming a dielectric layer over a first channel region and a second channel region;
forming a doping layer on the dielectric layer over the first channel region and the second channel region;
removing the doping layer over the second channel region;
annealing to drive dopants from the doping layer into the dielectric layer over the first channel region;
performing a first process to treat remaining portions of the doping layer with an acidic solution; and
after performing the first process, performing a second process to remove the remaining portions of the doping layer, wherein the first process is different than the second process.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first process comprises disposing the acidic solution over a surface of the doping layer and the dielectric layer.

### Claim 3 (depends on 1)

The method of claim 1, wherein the acidic solution comprises carbonic acid (H2CO3), hydrochloric acid (HCl), phosphoric acid (H3PO4), or acetic acid (CH3COOH).

### Claim 4 (depends on 3)

The method of claim 3, wherein performing the first process is performed at a temperature in a range from 20° C. to 80° C.

### Claim 5 (depends on 1)

The method of claim 1, wherein the acidic solution is an aqueous solution of with a ratio of CH3COOH:water in a range from 1:5 to 1:25.

### Claim 6 (depends on 1)

The method of claim 1 further comprising annealing the dielectric layer and the doping layer at a temperature in a range from about 800 to about 850 degrees Celsius.

### Claim 7 (depends on 1)

The method of claim 1, wherein the doping layer is a lanthanum-containing layer.

### Claim 8 (depends on 1)

The method of claim 1, wherein after annealing, the dielectric layer comprises HfO2, HfZrO, HfSiO, SiO, HMO, HMO, TiO, and Ta2O5 doped with lanthanum.

### Claim 9

A method of forming a semiconductor device, the method comprising:
forming a dielectric layer over a first channel region of a p-type transistor and a second channel region of an n-type transistor of a substrate, the dielectric layer being a metal oxide layer;
forming a lanthanum-doping layer on the dielectric layer over the first channel region and the second channel region;
forming one or more capping layers over the lanthanum-doping layer over the first channel region and the second channel region;
removing the one or more capping layers and the lanthanum-doping layer from over the second channel region;
driving lanthanum atoms into the dielectric layer from the lanthanum-doping layer over the first channel region, an unconsumed portion of the lanthanum-doping layer remaining after driving the lanthanum atoms into the dielectric layer;
softening a surface of the unconsumed portion of the lanthanum-doping layer using a first process, the first process comprising exposing the unconsumed portion of the lanthanum-doping layer to a first acidic solution; and
after softening, removing the unconsumed portion of the lanthanum-doping layer using a second process, wherein the first process is different than the second process.

### Claim 10 (depends on 9)

The method of claim 9, wherein the softening is performed at least in part by dispensing the first acidic solution over the substrate while spinning the substrate.

### Claim 11 (depends on 9)

The method of claim 9, wherein removing the unconsumed portion of the lanthanum-doping layer comprises using a second acidic solution.

### Claim 12 (depends on 11)

The method of claim 11, wherein the second acidic solution is stronger than the first acidic solution.

### Claim 13 (depends on 11)

The method of claim 11, wherein the second acidic solution comprises a halogen-containing solution.

### Claim 14 (depends on 11)

The method of claim 11, wherein softening the surface of the unconsumed portion of the lanthanum-doping layer and removing the unconsumed portion of the lanthanum-doping layer are performed in a same spin-rinse dry tool.

### Claim 15 (depends on 11)

The method of claim 11, wherein removing the unconsumed portion of the lanthanum-doping layer comprises applying the second acidic solution while the substrate is spinning.

### Claim 16

A method of forming a semiconductor device, the method comprising:
forming a dielectric layer over a first channel region and a second channel region of a substrate;
forming a doping layer on the dielectric layer over the first channel region and the second channel region, wherein the doping layer comprises lanthanum;
removing the doping layer over the second channel region;
annealing to drive dopants from the doping layer into the dielectric layer over the first channel region, an unconsumed portion of the doping layer remaining after annealing;
exposing the unconsumed portion of the doping layer to an acidic solution while spinning the substrate; and
after exposing, cleaning the substrate to remove the unconsumed portion of the doping layer using a halogen-containing solution.

### Claim 17 (depends on 16)

The method of claim 16, wherein cleaning the substrate comprises applying the halogen-containing solution while the substrate is spinning.

### Claim 18 (depends on 17)

The method of claim 17, wherein the halogen-containing solution comprises a hydrofluoric acid solution.

### Claim 19 (depends on 18)

The method of claim 18, wherein the hydrofluoric acid solution comprises an aqueous HF solution at a concentration of 0.097%.

### Claim 20 (depends on 19)

The method of claim 19, wherein the acidic solution has a PH value in a range from 5.0 to 7.0.