# US 2020/0350095 A1 · Power cable

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0350095 A1
- Document ID: US20200350095A1
- Status: Published application
- Kind: A1
- Application number: 16/963,085
- Filed: 2019-01-24
- Published: 2020-11-05
- Earliest claimed: 2018-01-25
- Assignees: Ls Cable & System Ltd.
- Applicants: Ls Cable & System Ltd.
- Inventors: Young Eun CHO; Gi Joon NAM; Min Sang CHO; Sue Jin SON
- Web page: https://patentgrep.com/patent/US20200350095A1

## CPC

- H01B 7/04: Flexible cables, conductors, or cords, e.g. trailing cables
- C08L 23/10: Homopolymers or copolymers of propene
- H01B 3/28: natural or synthetic rubbers
- H01B 3/441: {from alkenes}
- C08L 2203/202: use in electrical wires or wirecoating
- H01B 7/02: Disposition of insulation
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

Provided is a power cable, and particularly, to an ultra-high-voltage power cable of 45 kV to 600 kV. Specifically, the present invention relates to a power cable which is eco-friendly and includes an insulating layer formed of an insulating material having not only high heat resistance and mechanical strength but also high flexibility, bendability, impact resistance, cold resistance, installability, workability, etc., which are in trade-off with heat resistance and mechanical strength, and of which the lifespan, flexibility and installability can be additionally improved through precise control of a thickness of the insulating layer according to characteristics of the insulating material, thereby enhancing workability.

## Claims

### Claim 1

A power cable comprising a conductor and an insulating layer covering the conductor, wherein the insulating layer is formed of an insulating composition containing heterophasic polypropylene resin,
a flexural modulus of an insulating sample formed of the insulating composition at room temperature is in a range of 50 to 1,200 MPa, when measured according to the standard ASTM D790, and xylene insolubility thereof is 10% or less according to the following Equation 1:
xylene insolubility=(mass of insulating sample after eluted with xylene solvent/mass of insulating sample before eluted with xylene solvent)×100,
wherein the mass of insulating sample after eluted with xylene solvent represents mass of an insulating sample, measured when 0.3 grams of the insulating sample was immersed into a xylene solvent, heated at 150° C. or higher for six hours, cooled to room temperature, taken out of the xylene solvent and dried in an oven at 150° C. until the xylene solvent was dried, and
a thickness of the insulating layer of the power cable is 5.5 to 84.0 times train expressed in the following Equation 2:
tmin=2.5 Uo/breakdown electric field for insulating sample,
wherein Uo represents a reference voltage in a voltage test according to the standard IEC 60840, and
the breakdown electric field for insulating sample represents an electric field (kV/mm) according to a voltage applied when a probability of dielectric breakdown occurring in a plurality of insulating samples was 63.2% when electrodes were brought into contact with both ends of each of the plurality of insulating samples to apply a voltage thereto.

### Claim 2 (depends on 1)

The power cable of claim 1, wherein the heterophasic polypropylene resin comprises rubbery propylene copolymer dispersed in a crystalline polypropylene matrix.

### Claim 3 (depends on 2)

The power cable of claim 2, wherein the crystalline polypropylene matrix comprises a propylene homopolymer, a propylene copolymer, or both of them.

### Claim 4 (depends on 2)

The power cable of claim 2, wherein the rubbery propylene copolymer comprises at least one comonomer selected from the group consisting of ethylene and C4-12 alpha-olefins such as 1-butene, 1-pentene, 4-methyl-1-pentene, 1-hexene, 1-heptene, 1-octene, and the like.