# US 2020/0347512 A1 · Spincoating epitaxial films

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0347512 A1
- Document ID: US20200347512A1
- Status: Published application
- Kind: A1
- Application number: 16/398,430
- Filed: 2019-04-30
- Published: 2020-11-05
- Earliest claimed: 2019-04-30
- Assignees: The Curators of the University of Missouri
- Applicants: The Curators of the University of Missouri
- Inventors: Jay A. Switzer
- Web page: https://patentgrep.com/patent/US20200347512A1

## CPC

- C30B 19/12: characterised by the substrate
- C30B 7/06: using non-aqueous solvents
- C30B 19/08: Heating of the reaction chamber or the substrate
- C30B 29/12: Halides
- C30B 29/16: Oxides
- C30B 29/50: Cadmium sulfide
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

A process for forming an epitaxial film comprising spinning a substrate having an ordered crystal structure; heating the substrate during spinning to a temperature between 70° C. and 150° C.; dripping epitaxial film precursor solution onto the spinning substrate, where the precursor solution comprises inorganic film precursor material in a solvent; and continuing the heating and spinning to remove the solvent and epitaxially grow the epitaxial film on the substrate.

## Claims

### Claim 1

A process for forming an epitaxial film comprising:
spinning a substrate having an ordered crystal structure;
heating the substrate during spinning to a temperature between 70° C. and 150° C.;
dripping epitaxial film precursor solution onto the spinning substrate, where the precursor solution comprises inorganic film precursor material in a solvent; and
continuing the heating and spinning to remove the solvent and epitaxially grow the epitaxial film on the substrate.

### Claim 2 (depends on 1)

The process of claim 1 wherein the precursor material comprises a material selected from the group consisting of Pbl2, CsPbBr3, NaCl, and Zn(II).

### Claim 3 (depends on 1)

The process of claim 1 wherein the epitaxial film precursor solution comprises PbBr2 and CsBr and the epitaxial film comprises CsPbBr3.

### Claim 4 (depends on 1)

The process of claim 1 wherein the epitaxial film precursor solution comprises PbBr2 and CsBr dissolved in dimethyl sulfoxide solution and the epitaxial film comprises CsPbBr3.

### Claim 5 (depends on 1)

The process of claim 1 wherein the epitaxial film precursor solution comprises Pbl2 and the epitaxial film comprises Pbl2.

### Claim 6 (depends on 1)

The process of claim 1 wherein the epitaxial film precursor solution comprises Pbl2 dissolved in dimethylformamide solution and the epitaxial film comprises Pbl2.

### Claim 7 (depends on 1)

The process of claim 1 wherein the epitaxial film precursor solution comprises Zn ions and the epitaxial film comprises ZnO.

### Claim 8 (depends on 1)

The process of claim 1 wherein the epitaxial film precursor solution comprises Zn ions in ammonium hydroxide and the epitaxial film comprises ZnO.

### Claim 9 (depends on 1)

The process of claim 1 wherein the epitaxial film precursor solution comprises NaCl dissolved in water and the epitaxial film comprises NaCl.

### Claim 10 (depends on 1)

The process of claim 1 wherein the epitaxial film precursor solution comprises Cd ions or Pb ions and the epitaxial film comprises CdS or PbS.

### Claim 11 (depends on 1)

The process of claim 1 wherein the heating the substrate is to a temperature in the range of 70 to 130° C.

### Claim 12 (depends on 1)

The process of claim 1 wherein the heating the substrate is to a temperature in the range of 70 to 90° C.

### Claim 13 (depends on 1)

The process of claim 1 wherein the heating the substrate is to a temperature in the range of 90 to 130° C.

### Claim 14 (depends on 1)

The process of claim 1 further comprising preheating the epitaxial film precursor solution to a temperature in the range of 70 to 150° prior to said dripping so that it is at said temperature during said dripping.

### Claim 15 (depends on 1)

The process of claim 1 wherein:
the spinning the substrate comprises spinning a substrate based on SrTiO3(100), Mica(001), Au/Si(111), or Au/Si(100) at a rotation rate between 400 and 3000 rpm;
the dripping epitaxial film precursor solution onto the spinning substrate comprises dripping a CsPbBr3 solution;
the continuing the heating and spinning to remove the solvent and epitaxially grow the epitaxial film on the substrate is performed for between 25 and 180 seconds; and
the epitaxial film comprises CsPbBr3.

### Claim 16 (depends on 1)

The process of claim 1 wherein:
the spinning the substrate comprises spinning a substrate based on Au/Si(111) at a rotation rate between 400 and 3000 rpm;
the dripping epitaxial film precursor solution onto the spinning substrate comprises dripping a Pbl2 solution;
the continuing the heating and spinning to remove the solvent and epitaxially grow the epitaxial film on the substrate is performed for between 25 and 180 seconds; and
the epitaxial film comprises Pbl2.

### Claim 17 (depends on 1)

The process of claim 1 wherein:
the spinning the substrate comprises spinning a substrate based on Ag(100) deposited on a Au(100) film on a Si(100) substrate at a rotation rate between 400 and 3000 rpm;
the dripping epitaxial film precursor solution onto the spinning substrate comprises dripping a NaCl solution;
the continuing the heating and spinning to remove the solvent and epitaxially grow the epitaxial film on the substrate is performed for between 25 and 180 seconds; and
the epitaxial film comprises NaCl.

### Claim 18 (depends on 1)

The process of claim 1 wherein:
the spinning the substrate comprises spinning a substrate based on Au(111) at a rotation rate between 400 and 3000 rpm;
the dripping epitaxial film precursor solution onto the spinning substrate comprises dripping a Zn ion solution; and
the continuing the heating and spinning to remove the solvent and epitaxially grow the epitaxial film on the substrate is performed for between 25 and 180 seconds; and
the epitaxial film comprises ZnO.